# US 2004/0018690 A1 · Method of forming semiconductor device and semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0018690 A1
- Document ID: US20040018690A1
- Status: Published application
- Kind: A1
- Application number: 10/401,967
- Filed: 2003-03-31
- Published: 2004-01-29
- Earliest claimed: 2002-03-29
- Assignees: Kabushi Kaisha Toshiba
- Inventors: Kouichi Muraoka
- Web page: https://patentgrep.com/patent/US20040018690A1

## CPC

- H10D 64/685: {being perpendicular to the channel plane}
- H10D 64/01336: {on single crystalline silicon, e.g. chemical oxidation using a liquid}
- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/01342: {by deposition, e.g. evaporation, ALD or laser deposition (H10D64/01344 takes precedence)}
- H10D 64/01346: {in a gaseous ambient using an oxygen or a water vapour, e.g. oxidation through a layer (H10D64/01344 takes precedence)}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/6328: {Deposition from the gas or vapour phase}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 14/69395: {the material containing zirconium, e.g. ZrO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a semiconductor device having an improved silicon oxide film as a gate insulation film of a Metal Insulator Semiconductor structure and a method of making the same.

## Claims

### Claim 1

A method of forming a semiconductor device, comprising:
forming a silicon oxide film on a silicon surface at a temperature in an oxidation ambient, wherein the temperature is 650° C. or more and wherein the oxidation ambient comprises oxygen, water vapor, and either helium or neon, and the sum of the oxygen and water vapor partial pressures in the ambient is not less than 133×1011.703-18114/T Pa, wherein T is expressed in Kelvin; and
forming a high dielectric insulation film on the silicon oxide film, wherein the high dielectric insulation film has a dielectric constant greater than that of silicon oxide, and the high dielectric insulation film and the silicon oxide film form a gate insulation layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silicon oxide film has a thickness of not more than 1 nm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the high dielectric insulation film comprises SiONx or SiN.

### Claim 4 (depends on 1)

The method of claim 1, wherein the high dielectric insulation film comprises Al, Zr or Hf.

### Claim 5 (depends on 1)

The method of claim 1, wherein the high dielectric insulation film comprises BeO, MgO, CaO, Sro, BaO, Y2O3, CeO2, Pr,Oy, Nd2O3, ThO2, RuO2, IrO2, or In2O3.

### Claim 6 (depends on 1)

The method of claim 1, wherein the high dielectric insulation film comprises AlSiOx, ZrSiOx, or HfSiOx.

### Claim 7

A method of forming a semiconductor device, comprising:
dipping a silicon surface of a silicon substrate in a solution and forming a silicon oxide film on the silicon substrate;
annealing the silicon oxide film at a temperature in an oxidation ambient, wherein the temperature is 650° C. or more and wherein the oxidation ambient comprises oxygen, water vapor, and either helium or neon, and the sum of the oxygen and water vapor partial pressures in the ambient is not more than 133×1011.703-18114/T Pa, wherein T is expressed in Kelvin ; and
forming a high dielectric insulation film on the silicon oxide film, wherein the high dielectric insulation film has a dielectric constant greater than that of the silicon oxide film, and the high dielectric insulation film and the silicon oxide film form a gate insulation layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein said solution is a hydrochloric acid-ozone water solution.

### Claim 9 (depends on 7)

The method of claim 7, wherein the silicon oxide film has a thickness of not more than 1 nm.

### Claim 10 (depends on 7)

The method of claim 7, wherein the high dielectric insulation film comprises SiONx or SiN.

### Claim 11 (depends on 7)

The method of claim 7, wherein the high dielectric insulation film comprises Al, Zr or Hf.

### Claim 12 (depends on 7)

The method of claim 7, wherein said annealing comprises a reduction reaction.

### Claim 13 (depends on 7)

The method of claim 7, wherein said annealing reduces the silicon oxide film thickness.

### Claim 14 (depends on 7)

The method of claim 7, wherein the high dielectric insulation film comprises AlSiOx, ZrSiOx, or HfSiOx.

### Claim 15

A semiconductor device, comprising:
a semiconductor substrate;
a silicon oxide film on the semiconductor substrate comprising helium and neon;
a high dielectric insulation film, wherein the dielectric constant of the high dielectric insulation film is greater than that of the silicon oxide film;
a gate electrode formed on the high dielectric insulation film; and
a pair of source/drain regions formed two sides of the high dielectric insulation film.

### Claim 16 (depends on 15)

The semiconductor device of claim 15, wherein the silicon oxide film has a thickness of not more than 1 nm.

### Claim 17 (depends on 15)

The semiconductor device of claim 15, wherein the high dielectric insulation film comprises SiONx or SiN.

### Claim 18 (depends on 15)

The semiconductor device of claim 15, wherein the high dielectric insulation film comprises Al, Zr or Hf.

### Claim 19 (depends on 15)

The semiconductor device of claim 15, wherein the high dielectric insulation film comprises BeO, MgO, CaO, SrO, BaO, Y2O3, CeO2, PrxOy, Nd2O3, ThO2, RuO2, IrO2, or In2O3.

### Claim 20 (depends on 15)

A semiconductor device of claim 15, wherein the high dielectric insulation film comprises AlSiOx, ZrSiOx, or HfSiOx.

### Claim 21

A method of forming a semiconductor device, comprising:
forming a silicon oxynitride film on a silicon substrate; and
annealing the silicon oxynitride film at a temperature in an oxidation ambient, wherein the temperature is 650° C. or more and wherein the oxidation ambient comprises oxygen, water vapor, and either helium or neon, and the sum of the oxygen and water vapor partial pressures in the ambient is not more than 133×1011.703-18114/T Pa, wherein T is expressed in Kelvin, and the silicon oxynitride film forms a gate insulation layer.

### Claim 22 (depends on 21)

The method of forming a semiconductor device of claim 21, further comprising step of forming a high dielectric insulation film on the silicon oxynitride film, wherein the high dielectric insulation film has a dielectric constant greater than that of the silicon oxynitride film, and the high dielectric insulation film and the silicon oxynitride film form a gate insulation layer.