# US 2004/0018684 A1 · Method of etching a dielectric material in the presence of polysilicon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0018684 A1
- Document ID: US20040018684A1
- Status: Published application
- Kind: A1
- Application number: 10/202,992
- Filed: 2002-07-25
- Published: 2004-01-29
- Earliest claimed: 2002-07-25
- Assignees: Mosel Vitelic, Inc.
- Inventors: Hua Ji
- Web page: https://patentgrep.com/patent/US20040018684A1

## CPC

- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D 64/01326: {Aspects related to lithography, isolation or planarisation of the conductor}
- H10D 84/0188: {Manufacturing their isolation regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 50/283: {by chemical means}
- H10W 10/0143: {comprising concurrently refilling multiple trenches having different shapes or dimensions}
- H10W 10/0148: {comprising introducing impurities in side walls or bottom walls of trenches, e.g. for forming channel stoppers}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method is provided for advantageously etching dielectric material between highly integrated polysilicon devices with high dielectric-to-polysilicon selectivity to expose polysilicon with minimal polysilicon loss and without photoresist lift. A wet etch solution comprising surfactant and between about 0% and about 10% NH4F is used to wet etch the dielectric material and reduce polysilicon loss thickness, polysilicon resistance ratios, and polysilicon etch rates, while increasing dielectric-to-polysilicon selectivity. Advantageously, the present invention may penetrate into increasingly small geometries of highly integrated devices and may also be used for general wet etches of dielectric material in conjunction with photoresist.

## Claims

### Claim 1

A method of etching a dielectric layer in the presence of polysilicon, comprising:
forming two gate structures over a semiconductor substrate, each of said gate structures comprising a polysilicon layer;
forming a trench between said gate structures;
depositing a dielectric layer between said two gate structures; and
etching portions of said dielectric layer with a wet etch solution to expose polysilicon portions of said gate structures, said wet etch solution comprising surfactant and between about 0% and 10% by weight NH4F.

### Claim 2 (depends on 1)

The method of claim 1, wherein each of said gate structures further comprise an insulator layer underneath said polysilicon layer, and a silicon nitride layer over said polysilicon layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein said dielectric layer comprises silicon oxide.

### Claim 4 (depends on 1)

The method of claim 1, wherein said wet etch solution further comprises between about 0.05% and about 8.5% by weight HF.

### Claim 5 (depends on 4)

The method of claim 4, wherein said wet etch solution further comprises between about 81.5% and about 99.9% by weight deionized water.

### Claim 6 (depends on 5)

The method of claim 5, wherein said wet etch solution comprises between about 25 ppm and about 2,000 ppm surfactant.

### Claim 7 (depends on 1)

The method of claim 1, further comprising forming a photoresist layer over a region of said substrate prior to said etching.

### Claim 8

A method of etching a dielectric layer in the presence of polysilicon, comprising:
forming two gate structures over a semiconductor substrate, each of said gate structures comprising a polysilicon layer;
forming a trench between said two gate structures;
depositing a dielectric layer between said two gate structures; and
etching portions of said dielectric layer with a wet etch solution to expose polysilicon portions of said gate structures, said wet etch solution comprising surfactant and between about 0% and 10% by weight NH4F, and said etching occurring with a dielectric-to-polysilicon selectivity above about 15.

### Claim 9 (depends on 8)

The method of claim 8, wherein each of said gate structures further comprise an insulator layer underneath said polysilicon layer, and a silicon nitride layer over said polysilicon layer.

### Claim 10 (depends on 8)

The method of claim 8, wherein said dielectric layer comprises silicon oxide.

### Claim 11 (depends on 8)

The method of claim 8, wherein said wet etch solution further comprises between about 0.05% and about 8.5% by weight HF.

### Claim 12 (depends on 11)

The method of claim 11, wherein said wet etch solution further comprises between about 81.5% and about 99.9% by weight deionized water.

### Claim 13 (depends on 12)

The method of claim 12, wherein said wet etch solution further comprises between about 25 ppm and about 2,000 ppm surfactant.

### Claim 14 (depends on 8)

The method of claim 8, wherein said etching occurs with a polysilicon etch rate from about 1 Å/min to about 10 Å/min.

### Claim 15 (depends on 8)

The method of claim 8, further comprising forming a photoresist layer over a region of said substrate prior to said etching.

### Claim 16

A method of manufacturing a semiconductor device, comprising:
forming a first region over a semiconductor substrate, said first region having at least two gate structures, and each of said at least two gate structures comprising a polysilicon layer;
forming a second region over said semiconductor substrate;
forming a trench between said at least two gate structures;
depositing a dielectric layer between said at least two gate structures;
forming a photoresist layer over said second region; and
etching portions of said dielectric layer only in said first region with a wet etch solution to expose polysilicon portions of said at least two gate structures, said wet etch solution comprising between about 0% and 10% by weight NH4F.

### Claim 17 (depends on 16)

The method of claim 16, wherein said first region is a memory array region of a flash memory device.

### Claim 18 (depends on 16)

The method of claim 16, wherein said second region is a periphery region of a flash memory device.

### Claim 19 (depends on 16)

The method of claim 16, wherein said dielectric layer comprises silicon oxide.

### Claim 20 (depends on 16)

The method of claim 16, wherein said wet etch solution further comprises between about 0.05% and about 8.5% by weight HF.

### Claim 21 (depends on 20)

The method of claim 20, wherein said wet etch solution further comprises between about 81.5% and about 99.9% by weight deionized water.

### Claim 22 (depends on 21)