# US 2004/0016647 A1 · Anolyte for copper plating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0016647 A1
- Document ID: US20040016647A1
- Status: Published application
- Kind: A1
- Application number: 10/616,044
- Filed: 2003-07-08
- Published: 2004-01-29
- Earliest claimed: 2002-07-24
- Assignees: Applied Materials, Inc.
- Inventors: Michael X. Yang; Nicolay Y. Kovarsky
- Web page: https://patentgrep.com/patent/US20040016647A1

## CPC

- C25D 17/002: {Cell separation, e.g. membranes, diaphragms}
- A23D 7/00: Edible oil or fat compositions containing an aqueous phase, e.g. margarines (preservation of edible oil compositions containing aqueous phase A23B20/10)
- A23D 7/005: characterised by ingredients other than fatty acid triglycerides
- A23D 7/01: Other fatty acid esters, e.g. phosphatides
- A23J 7/00: Phosphatide compositions for foodstuffs, e.g. lecithin
- C07F 9/103: {Extraction or purification by physical or chemical treatment of natural phosphatides; Preparation of compositions containing phosphatides of unknown structure}
- C25D 7/123: {Semiconductors first coated with a seed layer or a conductive layer}
- C25D 17/001: {Apparatus specially adapted for electrolytic coating of wafers, e.g. semiconductors or solar cells}
- C25D 21/22: by ion-exchange
- H10P 14/47: Electrolytic deposition, i.e. electroplating; Electroless plating
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- A23D: EDIBLE OILS OR FATS, e.g. MARGARINES, SHORTENINGS OR COOKING OILS (preservation thereof A23B20/00; production, refinement or preservation of animal or vegetable fats or oils C11B, C11C)
- A23J: PROTEIN COMPOSITIONS FOR FOODSTUFFS; WORKING-UP PROTEINS FOR FOODSTUFFS; PHOSPHATIDE COMPOSITIONS FOR FOODSTUFFS
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments of the invention provide a method for plating copper into features formed on a semiconductor substrate. The method includes positioning the substrate in a plating cell, wherein the plating cell includes a catholyte volume containing a catholyte solution, an anolyte volume containing an anolyte solution, an ionic membrane positioned to separate the anolyte volume from the catholyte volume, and an anode positioned in the anolyte volume. The method further includes applying a plating bias between the anode and the substrate, plating copper ions onto the substrate from the catholyte solution, and replenishing the copper ions plated onto the substrate from the catholyte solution with copper ions transported from the anolyte solution via the ionic membrane, wherein the catholyte solution has a copper concentration of greater than about 51 g/L.

## Claims

### Claim 1

A method for plating metal onto a substrate, comprising:
positioning the substrate in a catholyte solution contained in a catholyte chamber of a plating cell, the catholyte solution comprising:
an acid source at a concentration of between about 5 g/L and about 15 g/L;
a copper source at a concentration of between about 0.8M and about 0.9M; and
chlorine ions at a concentration of between about 25 ppm and about and about 75 ppm; and
applying a plating bias between the substrate and an anode positioned in an anolyte chamber of the plating cell, the anolyte chamber being separated from the catholyte chamber by an ionic membrane and being supplied with an anolyte solution comprising a copper source having a concentration of greater than about 51 g/L.

### Claim 2 (depends on 1)

The method of claim 1, wherein the catholyte solution further comprises:
a leveler at a concentration of between about 2 mL/L and about 3 mL/L;
a suppressor at a concentration of between about 2 mL/L and about 3 mL/L; and
an accelerator at a concentration of between about 5.5 mL/L and about 8 mL/L.

### Claim 3 (depends on 2)

The method of claim 2, wherein the suppressor comprises at least one of ethylene oxide and propylene oxide.

### Claim 4 (depends on 2)

The method of claim 2, wherein the accelerator comprises sulfo propyldisulfide.

### Claim 5 (depends on 1)

The method of claim 1, wherein the anolyte has a pH of between about 2 and about 4.8.

### Claim 6 (depends on 5)

The method of claim 5, wherein the anolyte comprises a copper 11 salt having a concentration of copper ions of between about 0.1M and about 2M.

### Claim 7 (depends on 6)

The method of claim 6, wherein the copper II salt comprises at least one of copper sulfate, copper sulfonate, copper chloride, copper nitrate, and blends thereof.

### Claim 8 (depends on 5)

The method of claim 5, wherein the anolyte provides a copper transport of copper ions through the ionic membrane of between about 90% and about 100%.

### Claim 9 (depends on 1)

The method of claim 1, wherein the anode comprises at least one of a copper anode and a platinum anode.

### Claim 10

A method for plating copper into features formed on a semiconductor substrate, comprising:
positioning the substrate in a plating cell, wherein the plating cell comprises:
a catholyte volume containing a catholyte solution;
an anolyte volume containing an anolyte solution;
an ionic membrane positioned to separate the anolyte volume from the catholyte volume; and
an anode positioned in the anolyte volume;
applying a plating bias between the anode and the substrate;
plating copper ions onto the substrate from the catholyte solution; and
replenishing the copper ions plated onto the substrate from the catholyte solution with copper ions transported from the anolyte solution via the ionic membrane, wherein the anolyte solution has a copper concentration of greater than about 51 g/L.

### Claim 11 (depends on 10)

The method of claim 10, wherein the copper concentration is supplied by copper sulfate pentahydrate having a molarity of between about 0.8M and about 0.9M.

### Claim 12 (depends on 11)

The method of claim 11, wherein the anolyte has a pH of between about 2 and 4.8.

### Claim 13 (depends on 10)

The method of claim 10, wherein the plating cell further comprises a diffusion member positioned between an upper surface of the ionic membrane and the substrate.

### Claim 14 (depends on 13)

The method of claim 13, wherein the diffusion member comprises a porous ceramic disk.

### Claim 15 (depends on 10)

The method of claim 10, wherein the ionic membrane comprises a membrane having a fluorized polymer matrix.

### Claim 16 (depends on 10)

The method of claim 10, wherein the ionic membrane comprises a membrane having a polydivinilbenzol matrix.

### Claim 17 (depends on 12)

The method of claim 12, wherein the catholyte solution comprises:
acid at a concentration of between about 5 g/L and about 15 g/L;
copper at a concentration of between about 0.8M and about 0.9M; and
chlorine ions at a concentration of between about 25 ppm and about and about 75 ppm.

### Claim 18 (depends on 17)

The method of claim 17, wherein the catholyte further comprises:
a leveler at a concentration of between about 2 mL/L and about 3 mL/L;
a suppressor at a concentration of between about 2 mL/L and about 3 mL/L; and
an accelerator at a concentration of between about 5 mL/L and about 8 mL/L.

### Claim 19

A method for electrochemically plating copper onto features of a semiconductor substrate, comprising:
positioning the substrate in a plating cell having a catholyte solution volume, an anolyte solution volume, and an ionic membrane separating catholyte solution volume from the anolyte solution volume;
contacting the substrate with a catholyte solution;
applying an electrical bias between the substrate and an anode positioned in the anolyte volume, the electrical bias being sufficient to plate copper ions from the catholyte solution onto the substrate; and
replenishing copper ions plated from the catholyte solution via transfer of copper ions from the anolyte solution through the ionic membrane to the catholyte solution, the anolyte solution having a pH of between about 2 and about 4.8 and a copper ion concentration of between about 0.1M and about 2M.

### Claim 20 (depends on 19)

The method of claim 19, wherein the copper ion concentration in the anolyte comprises between about 51 g/L and about 60 g/L of copper metal to the anolyte.

### Claim 21 (depends on 19)

The method of claim 19, wherein the anolyte provides a copper transport of copper ions through the ionic membrane of between about 90% and about 100%.

### Claim 22 (depends on 19)

The method of claim 19, wherein the catholyte solution volume comprises:
an acid source at a concentration of between about 5 g/L and about 15 g/L;
a copper source at a concentration of between about 0.8M and about 0.9M; and
chlorine ions at a concentration of between about 25 ppm and about and about 75 ppm.

### Claim 23 (depends on 22)

The method of claim 22, wherein the catholyte further comprises:
a leveler at a concentration of between about 2 mL/L and about 4 mL/L;
a suppressor at a concentration of between about 1.5 mL/L and about 3 mL/L; and
an accelerator at a concentration of between about 5.5 mL/L and about 8 mL/L.

### Claim 24 (depends on 23)

The method of claim 23, wherein the anode comprises at least one of a copper anode and a platinum anode.

### Claim 25

A method for plating copper onto a substrate, comprising:
positioning the substrate in a catholyte plating solution contained in a catholyte chamber of a plating cell, the catholyte plating solution comprising:
an acid source at a concentration of between about 5 g/L and about 15 g/L;
a copper source at a concentration of between about 0.5M and about 1.0M; and
chlorine ions at a concentration of between about 25 ppm and about and about 75 ppm; and
applying a plating bias between the substrate and an anode positioned in an anolyte chamber of the plating cell, the anolyte chamber being separated from the catholyte chamber by an ionic membrane.

### Claim 26 (depends on 25)

The method of claim 25, wherein the anolyte comprises a copper source having a concentration of greater than about 51 g/L.

### Claim 27 (depends on 26)

The method of claim 26, wherein the anolyte has a pH of between about 2 and about 4.8.

### Claim 28 (depends on 26)

The method of claim 26, wherein the ionic membrane comprises a membrane having a polydivinilbenzol matrix.
