# US 2004/0016557 A1 · Coarse carbide substrate cutting elements and method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0016557 A1
- Document ID: US20040016557A1
- Status: Published application
- Kind: A1
- Application number: 10/437,750
- Filed: 2003-05-14
- Published: 2004-01-29
- Earliest claimed: 2002-07-24
- Assignees: Smith International, Inc.
- Inventors: Madapusi K. Keshavan; Anthony Griffo; David Truax; Dah-Ben Liang
- Web page: https://patentgrep.com/patent/US20040016557A1

## CPC

- E21B 10/567: with preformed cutting elements mounted on a distinct support, e.g. polycrystalline inserts
- C22C 29/08: based on tungsten carbide
- C23C 30/005: {on hard metal substrates}
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Cutting elements having coarse grain substrates and ultra hard material layers are provided. The substrates are formed from coarse grain size particles of tungsten carbide. A method of forming such cutting elements and a drag bit incorporating such cutting elements are also provided.

## Claims

### Claim 1

A cutting element comprising:
a substrate having an end surface, wherein the substrate is formed by the consolidation of a composition comprising tungsten carbide and a binder material, the substrate after consolidation having at least one substrate property selected from the group consisting of a median particle size of at least 6 μm, a Rockwell A hardness less than 86, and an impurity content of the tungsten carbide being not greater than about 0.1% by weight; and
an ultra hard material layer over the end surface of the substrate.

### Claim 2 (depends on 1)

The cutting element as recited in claim 1 further comprising at least one intermediate layer between the substrate and the ultra hard material layer.

### Claim 3 (depends on 1)

The cutting element as recited in claim 1 wherein the substrate has a median particle size of at least about 9 μm.

### Claim 4 (depends on 1)

The cutting element as recited in claim 1 wherein the substrate has a fracture toughness after consolidation of at least about 18 ksi(in)0.5.

### Claim 5 (depends on 1)

The cutting element as recited in claim 1 wherein the substrate has a hardness after consolidation in the range from about 83 to about 85 Rockwell A.

### Claim 6 (depends on 1)

The cutting element as recited in claim 1 wherein the substrate end surface is non-planar.

### Claim 7 (depends on 1)

The cutting element as recited in claim 1 further wherein the ultra hard material layer comprises an ultra hard material selected from the group consisting of diamond, cubic boron nitride and a mixture thereof.

### Claim 8 (depends on 1)

The cutting element as recited in claim 1 wherein after consolidation the substrate has a fracture toughness of at least about 18 ksi(in)0.5 and a hardness in the range from about 83 to about 85 Rockwell A.

### Claim 9 (depends on 1)

The cutting element as recited in claim 1 wherein the ultra hard material comprises ultra hard material particles, wherein the median particle size of the ultra hard particles is approximately the same as the median particle size of the substrate.

### Claim 10 (depends on 1)

The cutting element as recited in claim 1 wherein the substrate comprises at least a 6% concentration of particles having a grain size of at least 7 μm or more.

### Claim 11 (depends on 1)

The cutting element as recited in claim 1 wherein the substrate comprises cobalt and wherein the impurity content of the tungsten carbide is controlled to provide a thermal conductivity after consolidation not less than a value Kmin as determined by the following equation:
Kmin=0.38−0.00426X,
where X in the substrate cobalt content in weight %.

### Claim 12 (depends on 1)

The cutting element as recited in claim 1 wherein the substrate comprises cobalt and wherein the substrate composition has a minimal Rockwell A scale hardness Hmin after consolidation defined by the equation:
Hmin=91.1−0.63X,
where X is the substrate cobalt content in weight %.

### Claim 13 (depends on 1)

The cutting element as recited in claim 1 wherein the substrate comprises cobalt, wherein the impurity content of the tungsten carbide is controlled to provide a thermal conductivity not less than a value Kmin as determined by the following equation:
Kmin=0.00102X2−0.03076X+0.5464,
where X is the substrate cobalt content in weight %, and Kmin is in the units of cal/cm·s·K.

### Claim 14 (depends on 1)

The cutting element as recited in claim 1 further comprising a transition layer between the substrate and the ultra hard material layer.

### Claim 15

A cutting element comprising:
a substrate having an end surface, wherein the substrate has a median particle size of at least 6 μm; and
an ultra hard material layer over the end surface of the substrate.

### Claim 16 (depends on 15)

The cutting element as recited in claim 15 wherein the substrate has a Rockwell A hardness not greater than 87.

### Claim 17 (depends on 15)

The cutting element as recited in claim 15 wherein the substrate has a Rockwell A hardness not greater than 85.

### Claim 18 (depends on 15)

The cutting element as recited in claim 15 wherein the substrate is formed with tungsten carbide having an impurity content not greater than about 0.1% by weight.

### Claim 19 (depends on 15)

The cutting element as recited in claim 15 wherein the substrate has fracture toughness of at least about 18 ksi (in)0.5.

### Claim 20 (depends on 15)

The cutting element as recited in claim 15 wherein the substrate has a wear number of at least about 1.5.

### Claim 21 (depends on 15)

The cutting element as recited in claim 15 further comprising a transition layer between the substrate and the ultra hard material layer.

### Claim 22

A method of manufacturing a cutting element comprising:
providing a substrate having an endsurface, wherein the substrate is formed from a composition including tungsten carbide having a median particle size of at least 6 μm and a binder material;
placing a layer ultra hard material layer over the substrate end surface; and
processing the resulting assembly of substrate and ultra hard material layer at a sufficient temperature and pressure for metallurgical joining of the substrate and ultra hard material.

### Claim 23 (depends on 22)

The method as recited in claim 22 wherein providing a substrate comprises:
providing the tungsten carbide in powder form having a median particle size of at least 6 μm; and
providing the binder.

### Claim 24 (depends on 23)

The method as recited in claim 23 further comprising heating the powder and binder to at least partly cement the tungsten carbide particles.

### Claim 25 (depends on 23)

The method as recited in claim 23 wherein providing the tungsten carbide in powder form comprises providing the tungsten carbide in powder form having a median particle size of at least about 9 μm.

### Claim 26 (depends on 23)

The method as recited in claim 23 wherein providing the tungsten carbide in powder form comprises providing the tungsten carbide in powder form having a 6% concentration of particles having a grain size of at least 7 μm.

### Claim 27 (depends on 23)

The method as recited in claim 23 wherein the binder comprises cobalt, the method further comprising controlling the impurity content of the tungsten carbide powder to provide a thermal conductivity not less than a value Kmin as determined by the following equation:
Kmin=0.38−0.00426X,
where X in the substrate cobalt content in weight %.

### Claim 28 (depends on 23)

The method as recited in claim 23 wherein the binder comprises cobalt, the method further comprising controlling the impurity content of the tungsten carbide to provide a thermal conductivity not less than a value Kmin as determined by the following equation:
Kmin=0.00102X2−0.03076X+0.5464,
where X is cobalt content in weight %, and Kmin is in the units of cal/cm·s·K.

### Claim 29 (depends on 22)

The method as recited in claim 22 wherein providing the tungsten carbide in powder form comprises providing the tungsten carbide in powder form having an impurity content of not greater than about 0.1% by weight.

### Claim 30 (depends on 22)

The method as recited in claim 22 wherein the ultra hard material comprises an ultra hard material median particle size and wherein placing a layer of ultra hard material comprises placing a layer of ultra hard material having a median ultra hard material particle size that is approximately the same as the median particle size of the tungsten carbide powder.

### Claim 31

A drag bit comprising:
a drag bit body; and
a shear cutter mounted on the body, the shear cutter comprising,
a substrate, formed by the consolidation of a composition comprising tungsten carbide and a binder material, wherein the substrate has a property selected from the group of properties consisting of a median particle size of at least 6 μm; and
an ultra hard material layer over the end surface of the substrate.

### Claim 32 (depends on 31)

The drag bit as recited in claim 31 wherein the substrate comprises a Rockwell A hardness not greater than 87.

### Claim 33 (depends on 31)

The drag bit as recited in claim 31 wherein the substrate comprises an impurity content of the tungsten carbide being not greater than about 0.1%.

### Claim 34 (depends on 31)

The drag bit as recited in claim 31 wherein the substrate comprises a fracture toughness of at least about 18 ksi (in)0.5.

### Claim 35 (depends on 31)

The drag bit as recited in claim 31 wherein the substrate comprises a wear number of at least 1.5.

### Claim 36 (depends on 31)

The drag bit as recited in claim 31 wherein the shear cutter further comprises a transition layer between the substrate and the ultra hard material layer.

### Claim 37

A cutting element comprising:
a substrate comprising tungsten carbide particles and a cobalt binder disposed around the particles, wherein a grain size of the tungsten carbide particles and a content of the cobalt binder are selected to provide a fracture toughness of at least about 18 ksi (in)0.5 and a wear number of at least about 2; and
a polycrystalline ultra hard material layer disposed over said substrate.

### Claim 38 (depends on 37)

The cutting element as recited in claim 37 wherein the substrate has a hardness in a range of about 85 to 87 Rockwell A.

### Claim 39

A cutting element comprising:
a substrate comprising tungsten carbide particles and a cobalt binder disposed around the particles, wherein a grain size of the tungsten carbide particles and a content of the cobalt binder are selected to provide a fracture toughness of at least about 20 ksi (in)0.5 and a wear number of at least about 1.5; and
an ultra hard material layer disposed over said substrate.

### Claim 40 (depends on 39)

The cutting element as recited in claim 39 wherein the substrate has a hardness in a range of about 83 to 85 Rockwell A.