# US 2004/0011441 A1 · Cold-rolled aluminum killed steel sheet and method of manufacturing packaging from said sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0011441 A1
- Document ID: US20040011441A1
- Status: Published application
- Kind: A1
- Application number: 10/391,529
- Filed: 2003-03-19
- Published: 2004-01-22
- Earliest claimed: 2002-03-21
- Assignees: Usinor
- Inventors: Mohamed Bouzekri
- Web page: https://patentgrep.com/patent/US20040011441A1

## CPC

- C22C 38/04: containing manganese
- C22C 38/001: {containing N}
- C22C 38/06: containing aluminium
- C21D 8/0421: {characterised by the working steps}
- C21D 8/0447: {characterised by the heat treatment}
- C21D 9/48: deep-drawing sheets
- Y10T 428/24248: One piece
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention concerns a cold-rolled aluminum killed steel sheet, which includes by weight between 0.003 and 0.130% of carbon, between 0.10 and 1% of manganese, between 0.010 and 0.100% of aluminum, between 0.0015 and 0.0140% nitrogen, the remainder being of iron and impurities resulting from the manufacturing, and which has a content of carbon in solid solution (Css) of at least 50 ppm, as well as a method of manufacturing packaging from said sheet.

## Claims

### Claim 1

Cold-rolled aluminum killed sheet steel, characterized in that it has by weight between 0.003 and 0.130% carbon, between 0.10 and 1% manganese, between 0.010 and 0.100% aluminum, between 0.0015 and 0.0140% nitrogen, the remainder being iron and impurities resulting from production, and in that it has a content of carbon in solid solution (Css) of at least 50 ppm.

### Claim 2 (depends on 1)

Sheet according to the claim 1, characterized in that it has between 0.010 and 0.080% by weight of carbon, between 0.15 and 0.50% of manganese, between 0.0020 and 0.0060% nitrogen, and between 0.010 and 0.100% aluminum.

### Claim 3 (depends on 1)

Sheet according to the claim 1, characterized in that it has between 0.060 and 0.080% by weight of carbon, between 0.35 and 0.50% of manganese, between 0.0035 and 0.0060% nitrogen, and between 0.010 and 0.100% aluminum.

### Claim 4 (depends on 1, 2, 3)

Sheet according to any of the claims 1 to 3, characterized in that it has a rate of elongation of between 3 and 8%,

### Claim 5 (depends on 1, 2, 3, 4)

Sheet according to any of the claims 1 to 4, characterized in that it has a limit of elasticity greater than 660 MPa.

### Claim 6 (depends on 5)

Sheet according to claim 5, characterized in that it has a limit of elasticity greater than 700 MPa.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

Method of manufacturing packaging from aluminum killed steel, characterized in that it is composed of the step of forming a cold-rolled sheet of aluminum killed steel, according to any of the claims 1 to 8, and that it possibly includes a heat treatment of said formed sheet.

### Claim 8 (depends on 7)

Method according to the claim 7, characterized in that said forming is a drawing operation.

### Claim 9 (depends on 7)

Method according to claim 7, characterized in that said forming is a drawing operation followed by finishing.