# US 2004/0001995 A1 · Lanthanum gallate-based sintered body, manufacturing method thereof, and solid oxide fuel cell using the same as solid electrolyte

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0001995 A1
- Document ID: US20040001995A1
- Status: Published application
- Kind: A1
- Application number: 10/464,457
- Filed: 2003-06-19
- Published: 2004-01-01
- Earliest claimed: 2002-06-28
- Assignees: Nissan Motor Co., Ltd.
- Inventors: Kenji Furuya; Masaharu Hatano; Kazunori Fujii
- Web page: https://patentgrep.com/patent/US20040001995A1

## CPC

- C04B 35/01: based on oxide ceramics
- C04B 35/6262: {of calcined, sintered clinker or ceramics}
- H01M 8/1246: the electrolyte consisting of oxides
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3213: Strontium oxides or oxide-forming salts thereof
- C04B 2235/3215: Barium oxides or oxide-forming salts thereof
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3227: Lanthanum oxide or oxide-forming salts thereof
- C04B 2235/3284: Zinc oxides, zincates, cadmium oxides, cadmiates, mercury oxides, mercurates or oxide forming salts thereof
- C04B 2235/3286: Gallium oxides, gallates, indium oxides, indates, thallium oxides, thallates or oxide forming salts thereof, e.g. zinc gallate
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/6567: Treatment time
- C04B 2235/768: Perovskite structure ABO3
- C04B 2235/78: Grain sizes and shapes, product microstructures, e.g. acicular grains, equiaxed grains, platelet-structures
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/786: Micrometer sized grains, i.e. from 1 to 100 micron
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A lanthanum gallate-based sintered body comprises a base material formed of lanthanum gallate-based oxide, and grains having a K2NiF4 structure and/or grains having a layered perovskite structure are dispersed into the base material. Consequently, the lanthanum gallate-based sintered body has a high mechanical strength and is excellent in thermal resistance. Further, a SOFC having excellent properties can be obtained by using the lanthanum gallate-based sintered body as the solid electrolyte.

## Claims

### Claim 1

A lanthanum gallate-based sintered body, comprising:
a base material formed of lanthanum gallate-based oxide,
wherein grains having a K2NiF4 structure and/or grains having a layered perovskite structure are dispersed into the base material.

### Claim 2 (depends on 1)

A lanthanum gallate-based sintered body according to claim 1,
wherein the lanthanum gallate-based oxide is a compound represented by the following general formula (I):
(La1-xAx)(Ga1-yBy)O3-δ (I)
where A is any of strontium, barium and calcium, B is any of magnesium and zinc, a range of x is: 0<x<0.2, and a range of y is: 0<y≦0.2, and δ is an oxygen deficit.

### Claim 3 (depends on 1)

A lanthanum gallate-based sintered body according to claim 1,
wherein the grains having a K2NiF4 structure are a compound represented by the following general formula (II):
(La1-xAx)2(Ga1-yBy)O4-δ (II)
where A is any of strontium, barium and calcium, B is any of magnesium and zinc, a range of x is: 0<x<0.5, and a range of y is: 0<y≦0.2, and δ is an oxygen deficit.

### Claim 4 (depends on 1)

A lanthanum gallate-based sintered body according to claim 1,
wherein, a length in a longitudinal direction of the grains having the K2NiF4 structure ranges from 5 μm to 200 μm inclusive, and
a shape of the grains having the K2NiF4 structure is needle-shaped.

### Claim 5 (depends on 1)

A lanthanum gallate-based sintered body according to claim 1,
wherein, on a cross-section of the sintered body, when an area of grains having the K2NiF4 structure of which grain diameter is 0.2 μm or more is measured by a linear intercept method, the area of grains having the K2NiF4 structure ranges from 2 area % to 30 area % inclusive with respect to an area of the cross-section.

### Claim 6 (depends on 1)

A lanthanum gallate-based sintered body according to claim 1,
wherein the grains having a layered perovskite structure are a compound represented by the following general formula (III):
(La1-xAx)2(Ga1-yBy)3O7-δ (III)
where A is any of strontium, barium and calcium, B is any of magnesium and zinc, a range of x is: 0<x<0.5, and a range of y is: 0<y≦0.2, and δ is an oxygen deficit.

### Claim 7 (depends on 1)

A lanthanum gallate-based sintered body according to claim 1,
wherein, a length in a longitudinal direction of the grains having the layered perovskite structure ranges from 5 μm to 50 μm inclusive, and
a shape of the grains having the layered perovskite structure is needle-shaped.

### Claim 8 (depends on 1)

A lanthanum gallate-based sintered body according to claim 1,
wherein, on a cross-section of the sintered body, when an area of grains having the layered perovskite structure of which grain diameter is 0.2 μm or more is measured by a linear intercept method, the area of grains having the layered perovskite structure ranges from 1 area % to 15 area % inclusive with respect to an area of the cross-section.

### Claim 9

A method of manufacturing a lanthanum gallate-based sintered body, comprising:
prefiring a raw material of the lanthanum gallate-based sintered body at a temperature ranging from 1050° C. to 1200° C. inclusive for a time ranging from 2 hours to 10 hours inclusive;
milling the prefired raw material to prepare raw material powder;
molding the raw material powder; and
sintering the molded raw material powder to separate a phase formed of lanthanum gallate-based oxide and a phase having a K2NiF4 structure and/or a layered perovskite structure.

### Claim 10 (depends on 9)

The method of manufacturing a lanthanum gallate-based sintered body of claim 9,
wherein conditions of the sintering are a temperature ranging from 1350° C. to 1550° C. inclusive and a time ranging from 10 hours to 100 hours inclusive.

### Claim 11

A solid oxide fuel cell, comprising:
a lanthanum gallate-based sintered body including a base material formed of lanthanum gallate-based oxide,
wherein grains having a K2NiF4 structure and/or grains having a layered perovskite structure are dispersed into the base material.