# US 2004/0001958 A1 · Method of and apparatus for protecting thin copper foil and other shiny substrates during handling and rigorous processing, as in PCB manufacture and the like, by electric-charge adherence thereto of thin release-layered plastic films and the like, and improved products produced thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0001958 A1
- Document ID: US20040001958A1
- Status: Published application
- Kind: A1
- Application number: 10/186,866
- Filed: 2002-06-28
- Published: 2004-01-01
- Earliest claimed: 2002-06-28
- Assignees: Metallized Products, Inc.
- Inventors: Martin J. Wilheim
- Web page: https://patentgrep.com/patent/US20040001958A1

## CPC

- B32B 15/08: of synthetic resin
- B29C 63/0043: {Fixing the layers by electrostatic charges, by the use of structured surfaces or by mechanical means}
- B32B 7/06: permitting easy separation
- B32B 27/36: comprising polyesters
- B32B 37/00: Methods or apparatus for laminating, e.g. by curing or by ultrasonic bonding
- H05K 3/022: {Processes for manufacturing precursors of printed circuits, i.e. copper-clad substrates}
- B29C 63/0056: {Provisional sheathings}
- B29L 2031/3425: {Printed circuits}
- B32B 2310/025: Electrostatic charges
- B32B 2311/12: Copper
- B32B 2457/08: PCBs, i.e. printed circuit boards
- Y10T 29/49826: Assembling or joining
- Y10T 156/1067: Continuous longitudinal slitting
- Y10T 428/31681: Next to polyester, polyamide or polyimide [e.g., alkyd, glue, or nylon, etc.]
- Y10T 428/31909: Next to second addition polymer from unsaturated monomers
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An improved method of and apparatus for producing preferably thin plastic protective film layers for thin shiny copper foils and the like, as for PCB applications, with electric-charge adhering of the same to the foil and with peel-off releasable properties to provide the same original pristine, shiny copper foil surface without contamination, marring or other physical, chemical or other residue despite handling and other processing procedures.

## Claims

### Claim 1

A method of protecting a smooth high finish shiny thin conducting copper foil as for PCB and copper clad laminate use, that comprises, electrostatically permanently charging a protective masking insulating plastic film pre-treated with a release surface; laminating the film to the foil to charge-adhere the film release surface against the foil; and subsequently, after the protection is no longer required, stripping the film from the foil.

### Claim 2

A method of protecting a smooth high finish shiny surface substrate, that comprises, electrostatically permanently charging a protective masking insulating plastic or paper film pre-treated with or without a release surface; applying the film upon the shiny substrate surface to charge-adhere the film release treated or untreated surface against said shiny substrate surface; and subsequently, after the protection is no longer required, stripping the film from the substrate surface.

### Claim 3 (depends on 1)

The method as claimed in claim 1 wherein the plastic film is provided in rolls and unwound and fed through a web-charging station, and then rewound as charged-film rolls available for laminating to roll-fed foil.

### Claim 4 (depends on 3)

The method of claim 3 wherein the film after charging is slit prior to the rewinding.

### Claim 5 (depends on 1)

The method of claim 1 wherein the film is a polyester plastic laminate having a coating of a thin release layer of a cured release acrylated/epoxy/urethane oligomer and/or oligomer blended resin on at least one side of the film.

### Claim 6 (depends on 5)

The method of claim 5 wherein said coating is applied to both sides of the film.

### Claim 7 (depends on 5)

The method of claim 5 wherein the film side that is charge-adhered to the foil is smooth and the other side is relatively rougher.

### Claim 8 (depends on 3)

The method of claim 3 wherein the film is substantially transparent.

### Claim 9 (depends on 3)

The method of claim 3 wherein the film is selected from the group consisting of polyester, polypropylene, biaxially oriented polypropylene, polyvinylidine fluoride, polyethylene, paper and silicone TPX (polymethylpentene) and co-extruded films with releasable surface properties treated films.

### Claim 10 (depends on 2)

The method of claim 2 wherein the substrate surface is selected from the group consisting of copper, stainless steel, chrome, glass, acrylics, Lucite, plexiglass and high finish furniture surfaces.

### Claim 11 (depends on 1)

The method of claim 1 wherein the film-release peel strength is less than about 25 grams, per lineal inch.

### Claim 12 (depends on 1)

The method of claim 1 wherein the charge-adhered film remains releasable after exposure to process temperatures of up to about 400° F. and pressures of up to about 700 pounds per square inch for periods of time up to several hours.

### Claim 13

Apparatus for producing a protective smooth high finish thin conducting copper foil as for PCB use, having, in combination, a plastic film web roll unwinding station; an electrostatic web-charging station; means for passing the unwinding film web through the web-charging station; a film-web roll rewinding station; and means for conveying the charged film web from the web-charging station to the roll rewinding station.

### Claim 14 (depends on 13)

The apparatus of claim 13 wherein the film-web roll rewinding station is provided with a plurality of roll rewinders, and a web slitter is interposed prior to the rewinders for slitting the charged film web into a plurality of charged film webs for conveying to the respective of the rewinders.

### Claim 15 (depends on 13)

The apparatus of claim 13 wherein means is provided for laminating the charged film from the rewind roll(s) to a web of thin copper foil.

### Claim 16

A protected copper foil laminate product comprising a thin copper foil as for PCB use, having laminated on a surface of the foil, a substantially permanently electrostatically charge-attached protective plastic film.

### Claim 17 (depends on 16)

The product of claim 16 wherein the plastic film is a polyester film having a coating of a thin release layer of a cured release acrylated acrylated/epoxy/urethane oligomer and/or oligomer-blended resin on at least one side of the film.

### Claim 18 (depends on 17)

The product of claim 17 wherein said coating is applied to both sides of the film.

### Claim 19 (depends on 17)

The product of claim 17 wherein the film side that is charge-adhered to the foil is smooth and the other side is relatively rough.

### Claim 20 (depends on 16)

The product of claim 16 wherein the film is substantially transparent.

### Claim 21 (depends on 16)

The product of claim 16 wherein the film is selected from the group consisting of polyester, polypropylene, biaxially oriented polypropylene, polyethylene, polyvinylidene fluoride, paper and silicone TPX (polymethylpentene) and co-extruded films with releasable surface properties treated films.

### Claim 22 (depends on 16)

The product of claim 16 wherein the film-release peel strength is less than about 25 grams per lineal inch.

### Claim 23 (depends on 16)

The product of claim 16 wherein the charge-adhered film remains releasable after exposure to process temperatures of up to about 400° F. and pressures of up to about 700 pounds per square inch, for periods of several hours.

### Claim 24

A rolled web of permanently electrostatically surface-charged polyester plastic film laminate having a coating of a thin release layer of a cured release acrylated/epoxy, urethane oligomer and/or oligomer-blended resin on at least one side of the film.

### Claim 25 (depends on 24)

The rolled web of claim 24 wherein said coating is applied to both sides of the film.

### Claim 26 (depends on 25)

The rolled web of claim 25 wherein the film side that is charged is smooth and the other side is relatively rough.

### Claim 27 (depends on 24)