# US 2003/0232906 A1 · Stabilized coating compositions containing isothiazolone

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0232906 A1
- Document ID: US20030232906A1
- Status: Published application
- Kind: A1
- Application number: 10/454,264
- Filed: 2003-06-04
- Published: 2003-12-18
- Earliest claimed: 2002-06-06
- Inventors: Tirthankar Ghosh
- Web page: https://patentgrep.com/patent/US20030232906A1

## CPC

- C08K 5/46: with oxygen or nitrogen in the ring
- C09D 133/04: Homopolymers or copolymers of esters {(C09D143/04 takes precedence)}
- C08K 5/0058: {Biocides; (macromolecular substances as carriers for biocide material A01N25/10)}
- C08K 5/47: Thiazoles
- C08K 2003/085: {Copper}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

High pH aqueous coating compositions containing 3-isothiazolone microbicide that have been stabilized against the degradation of the 3-isothiazolone by the addition of low levels of copper ion are disclosed. In particular, aqueous paint compositions containing pH-adjusting amine compounds, where the pH is above 9.5, are effectively stabilized when 1 to 200 ppm of copper ion is added to the paint composition before the 3-isothiazolone is combined with other paint components or if copper ion is added together with the 3-isothiazolone to the remaining paint components or if the 3-isothiazolone is added no more than 1 hour before copper ion is added to the composition.

## Claims

### Claim 1

An aqueous coating composition comprising:
(a) a film-forming polymeric coating composition selected from one or more of the group consisting of acrylic polymer, polyvinylacetate polymer, polyvinylchloride polymer and styrene-acrylic polymer;
(b) a 3-isothiazolone compound as represented by formula I:
3
wherein:
Y is an unsubstituted or substituted (C1-C18)alkyl group, an unsubstituted or substituted (C2-C18)alkenyl or alkynyl group, an unsubstituted or substituted (C6-C12)cycloalkyl group, an unsubstituted or substituted (C7-C10)aralkyl group, or a substituted (C7-C10)aryl group;
R and R1 are independently hydrogen, halogen or (C1-C4)alkyl groups; or
R and R1 can be taken together with the C═C double bond of the isothiazolone ring to form an unsubstituted or substituted benzene ring;
(c) a pH-adjusting compound selected from one or more of ammonia and organic amines having a pKa greater than 9.0;
(d) from 1 to 200 parts per million, based on weight of the composition, of copper ion; and
(e) water;
wherein the aqueous composition has a pH greater than 9.5.

### Claim 2 (depends on 1)

The composition of claim 1 wherein the copper ion is provided by a copper compound selected from one or more of nitrate, chloride, acetate and organic acid carboxylate salts.

### Claim 3 (depends on 1)

The composition of claim 1 comprising from 1 to 75 parts of the polymeric coating composition (a), from 0.02 to 0.2 parts of the 3-isothiazolone (b), from 0.02 to 1 parts of the pH-adjusting compound (c), from 0.0001 to 0.02 parts of copper ion (d), from 25 to 99 parts of water (e), and further comprising from zero up to 10 parts of a solvent selected from one or more of the group consisting of aliphatic hydrocarbons, aromatic hydrocarbons, dihydric alcohols and monoalkyl ethers of dihydric alcohols; wherein the parts of (a), (b) and (c) are expressed per 100 parts of total aqueous composition.

### Claim 4 (depends on 3)

The composition of claim 3 wherein the composition comprises from 0.05 to 0.1 parts of the 3-isothiazolone (b) and from 0.001 to 0.005 parts of copper ion (d).

### Claim 5 (depends on 1)

The composition of claim 1 wherein the 3-isothiazolone is selected from one or more of the group consisting of 2-n-octyl-3-isothiazolone and 4,5-dichloro-2-n-octyl-3-isothiazolone.

### Claim 6

A method for stabilizing an aqueous coating composition against degradation of a 3-isothiazolone compound contained therein, comprising adding 1 to 200 parts per million, based on weight of the aqueous coating composition, of copper ion to a mixture of:
(a) a film-forming polymeric coating composition selected from one or more of the group consisting of acrylic polymer, polyvinylacetate polymer, polyvinylchloride polymer and styrene-acrylic polymer;
(b) a pH-adjusting compound selected from one or more of ammonia and organic amines having a pKa greater than 9.0; and
(c) water;
wherein pH of the coating composition is greater than 9.5; and wherein components (a), (b), (c) and the copper compound may be combined in any order provided that a 3-isothiazolone compound is further added at a point no more than 1 hour before addition of the copper compound.

### Claim 7 (depends on 6)

The method of claim 6 comprising adding 10 to 50 parts per million, based on weight of the aqueous coating composition, of copper ion to the mixture.

### Claim 8 (depends on 6)

The method of claim 6 wherein the a 3-isothiazolone compound is added at a point after addition of the copper compound.

### Claim 9 (depends on 6)

The method of claim 6 wherein the 3-isothiazolone compound is represented by formula I:
4
wherein:
Y is an unsubstituted or substituted (C1-C18)alkyl group, an unsubstituted or substituted (C2-C18)alkenyl or alkynyl group, an unsubstituted or substituted (C6-C12)cycloalkyl group, an unsubstituted or substituted (C7-C10)aralkyl group, or a substituted (C7-C10)aryl group;
R and R1 are independently hydrogen, halogen or (C1-C4)alkyl groups; or
R and R1 can be taken together with the C═C double bond of the isothiazolone ring to form an unsubstituted or substituted benzene ring.

### Claim 10

A method for stabilizing an aqueous coating composition against degradation of a 3-isothiazolone compound contained therein, comprising:
(a) combining 1 to 200 parts per million, based on weight of the aqueous coating composition, of a copper compound with a 3-isothiazolone compound to form a first mixture; and
(b) adding the first mixture to a second mixture to form the aqueous coating composition, wherein the second mixture has a pH of greater than 9.5 and comprises:
(i) a film-forming polymeric coating composition selected from one or more of the group consisting of acrylic polymer, polyvinylacetate polymer, polyvinylchloride polymer and styrene-acrylic polymer;
(ii) a pH-adjusting compound selected from one or more of ammonia and organic amines having a pKa greater than 9.0; and
(iii) water.