# US 2003/0232279 A1 · Negative resist composition comprising base polymer having epoxy ring and Si-containing crosslinker and patterning method for semiconductor device using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0232279 A1
- Document ID: US20030232279A1
- Status: Published application
- Kind: A1
- Application number: 10/395,914
- Filed: 2003-03-24
- Published: 2003-12-18
- Earliest claimed: 2002-06-14
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Sang-Jun Choi
- Web page: https://patentgrep.com/patent/US20030232279A1

## CPC

- G03F 7/0757: {Macromolecular compounds containing Si-O, Si-C or Si-N bonds (G03F7/0752 takes precedence)}
- G03F 7/038: Macromolecular compounds which are rendered insoluble or differentially wettable (G03F7/075 takes precedence; macromolecular azides G03F7/012; macromolecular diazonium compounds G03F7/021)
- G03F 7/0385: {using epoxidised novolak resin}
- G03F 7/0755: {Non-macromolecular compounds containing Si-O, Si-C or Si-N bonds (G03F7/0752 takes precedence)}
- Y10S 430/115: Cationic or anionic
- Y10S 430/122: Sulfur compound containing
- Y10S 430/126: Halogen compound containing
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A negative resist composition and a patterning method for semiconductor devices using the composition are provided. In one aspect, a negative resist composition comprises an alkali-soluble base polymer having an epoxy ring substituent, a silicon-containing crosslinker having multiple hydroxy groups, and a photoacid generator. In another aspect, a patterning method includes using the negative resist composition in a bi-layer resist process to form fine patterns.

## Claims

### Claim 1

A negative resist composition comprising:
an alkali-soluble base polymer having an epoxy ring substituent;
a crosslinker comprising silicon and multiple hydroxy functional groups; and
a photoacid generator.

### Claim 2 (depends on 1)

The negative resist composition of claim 1, wherein the alkali-soluble base polymer is an epoxy phenol-novolac resin or an epoxy (o,m,p)-cresol novolac resin.

### Claim 3 (depends on 1)

The negative resist composition of claim 1, wherein the alkali-soluble base polymer is an epoxy-substituted polyhydroxystyrene.

### Claim 4 (depends on 1)

The negative resist composition of claim 1, wherein the alkali-soluble base polymer comprises a glycidyl (meth)acrylate repeating unit or a (meth)acrylate repeating unit with an alicyclic epoxy group.

### Claim 5 (depends on 4)

The negative resist composition of claim 4, wherein the alicyclic epoxy group is selected from the group consisting of 3,4-epoxy-1-cyclohexylmethyl radical, 5,6-epoxy-2-bicyclo[2.2.1]heptyl radical, 5(6)-epoxyethyl-2-bicyclo-[2.2.1]heptyl radical, 5,6-epoxy-2-bicyclo-[2.2.1]heptylmethyl radical, 3,4-epoxytricyclo-[5.2.1.02,6]decyl radical, 3,4-epoxytricyclo-[5.2.1.02,6]decyloxyethyl radical, 3,4-epoxytetracyclo-[4.4.0.12,5.17,10]dodecyl radical, and 3,4-epoxytetracyclo-[4.4.0.12,5.17,10]dodecylmethyl radical.

### Claim 6 (depends on 1)

The negative resist composition of claim 1, wherein the silicon-containing crosslinker is a dihydroxy-terminated poly (dimethylsiloxane) oligomer or polymer.

### Claim 7 (depends on 1)

The negative resist composition of claim 1, wherein the amount of the silicon-containing crosslinker is in the range of about 5.0-50% by weight based on the total weight of the alkali-soluble base polymer.

### Claim 8 (depends on 1)

The negative resist composition of claim 1, wherein the amount of the photoacid generator is in the range of about 1.0-10% by weight based on the total weight of the alkali-soluble base polymer.

### Claim 9 (depends on 1)

The negative resist composition of claim 1, wherein the photoacid generator is a triarylsulfonium salt, a diaryliodonium salt, or a mixture of the foregoing salts.

### Claim 10 (depends on 9)

The negative resist composition of claim 9, wherein the photoacid generator is triphenylsulfonium triflate, diphenyliodonium triflate, di-t-butylphenyliodium triflate, or a mixture of the foregoing materials.

### Claim 11 (depends on 1)

The negative resist composition of claim 1, further comprising an organic base.

### Claim 12 (depends on 11)

The negative resist composition of claim 11, wherein the amount of the organic base is in a range of about 0.01-2.0% by weight based on contents of the photoacid generator.

### Claim 13 (depends on 11)

The negative resist composition of claim 11, wherein the organic base is selected from the group consisting of triethylamine, triisobutylamine, trioctylamine, triisodecylamine, triethanolamine, and a mixture of the foregoing materials.

### Claim 14

A method for forming patterns for a semiconductor device, comprising:
forming a first resist layer on a target layer to be etched on a semiconductor substrate;
forming a second resist layer by coating the first resist layer with a negative resist composition, wherein the negative resist composition comprises an alkali-soluble base polymer having an epoxy ring substituent, a silicon-containing crosslinker having multiple hydroxy groups, and a photoacid generator;
pre-baking the second resist layer;
exposing the second resist layer;
performing post-exposure baking on the exposed second resist layer;
developing the exposed second resist layer to form a second resist layer pattern;
etching the first resist layer using the second resist layer pattern as an etching mask to form a first resist layer pattern; and
etching the target layer using the first resist layer pattern as an etching mask.

### Claim 15 (depends on 14)

The method of claim 14, wherein a KrF, ArF, or F2 eximer laser is used to expose the second resist layer.

### Claim 16 (depends on 14)

The method of claim 14, wherein the alkali-soluble base polymer of the negative resist composition is an epoxy phenol-novolac resin or an epoxy (o,m,p)-cresol novolac resin.

### Claim 17 (depends on 14)

The method of claim 14, wherein the alkali-soluble base polymer of the negative resist composition is epoxy-substituted polyhydroxystyrene.

### Claim 18 (depends on 14)

The method of claim 14, wherein the alkali-soluble base polymer of the negative resist composition comprises a glycidyl (meth)acrylate repeating unit or a (meth)acrylate repeating unit with an alicyclic epoxy group.

### Claim 19 (depends on 18)

The method of claim 18, wherein the alicyclic epoxy group is selected from the group consisting of 3,4-epoxy-1-cyclohexylmethyl radical, 5,6-epoxy-2-bicyclo[2.2.1]heptyl radical, 5(6)-epoxyethyl-2-bicyclo-[2.2.1]heptyl radical, 5,6-epoxy-2-bicyclo-[2.2.1]heptylmethyl radical, 3,4-epoxytricyclo-[5.2.1.02,6]decyl radical, 3,4-epoxytricyclo-[5.2.1.02,6]decyloxyethyl radical, 3,4-epoxytetracyclo-[4.4.0.12,5.17,10]dodecyl radical, and 3,4-epoxytetracyclo-[4.4.0.12,5.17,10]dodecylmethyl radical.

### Claim 20 (depends on 14)

The method of claim 14, wherein the silicon-containing crosslinker of the negative resist composition is a dihydroxy-terminated poly (dimethylsiloxane) oligomer or polymer.

### Claim 21 (depends on 14)

The method of claim 14, wherein the amount of the silicon-containing crosslinker in the negative resist composition is in the range of about 5.0-50% by weight based on the total weight of the alkali-soluble base polymer.

### Claim 22 (depends on 14)

The method of claim 14, wherein the amount of the photoacid generator in the negative resist composition is in the range of about 1.0-10% by weight based on the total weight of the alkali-soluble base polymer.

### Claim 23 (depends on 14)

The method of claim 14, wherein the photoacid generator of the negative resist composition is a triarylsulfonium salt, a diaryliodonium salt, or a mixture of the foregoing salts.

### Claim 24 (depends on 23)

The method of claim 23, wherein the photoacid generator is triphenylsulfonium triflate, diphenyliodonium triflate, di-t-butylphenyliodium triflate, or a mixture of the foregoing materials.

### Claim 25 (depends on 14)

The method of claim 14, wherein the negative resist composition further comprises an organic base.

### Claim 26 (depends on 25)

The method of claim 25, wherein the amount of the organic base is in a range of about 0.01-2.0% by weight based on the content of the photoacid generator.

### Claim 27 (depends on 25)

The method of claim 25, wherein the organic base is selected from the group consisting of triethylamine, triisobutylamine, trioctylamine, triisodecylamine, triethanolamine, and a mixture of the foregoing materials.