# US 2003/0231996 A1 · Method for adsorbing lithium ions from a lithium-containing aqueous solution by a granular adsorbent

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0231996 A1
- Document ID: US20030231996A1
- Status: Published application
- Kind: A1
- Application number: 10/173,177
- Filed: 2002-06-18
- Published: 2003-12-18
- Earliest claimed: 2002-06-18
- Assignees: Industrial Technology Research Institute
- Inventors: Jer-Yuan Shiu; Jiunn-Ren Lin; Dzu-Chi Lee; Yung-Min Chen; Chih-Chung Liu
- Web page: https://patentgrep.com/patent/US20030231996A1

## CPC

- B01J 20/2803: {Sorbents comprising a binder, e.g. for forming aggregated, agglomerated or granulated products}
- B01J 20/06: comprising oxides or hydroxides of metals not provided for in group B01J20/04
- C02F 1/281: {using inorganic sorbents}
- B01J 2220/42: Materials comprising a mixture of inorganic materials (materials coated or impregnated on a carrier B01J20/32)
- C02F 1/66: by neutralisation; pH adjustment (for degassing C02F1/20; using ion-exchange C02F1/42; for flocculation or precipitation of suspended impurities C02F1/52; for removing dissolved compounds C02F1/58)
- C02F 2101/20: Heavy metals or heavy metal compounds
- C02F 2103/08: Seawater, e.g. for desalination
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)

## Abstract

A lithium-containing aqueous solution is contacted with a granular adsorbent of lithium-containing manganese oxide to adsorb lithium ions from the aqueous solution on the adsorbent, wherein an alkali is added to the aqueous solution to raise the pH value thereof to about 10 or above prior to the adsorption, thereby the saturated amount of lithium ions adsorbed per gram of adsorbent is increased from about 6 mg to about 25 mg.

## Claims

### Claim 1

A method for adsorbing lithium ions from a lithium-containing aqueous solution by an adsorbent comprising contacting a lithium-containing aqueous solution to an adsorbent of lithium-containing manganese oxide, so that lithium ions in the aqueous solution are adsorbed on the adsorbent, characterized in that said lithium-containing aqueous solution has a pH value not less than 10.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said lithium-containing aqueous solution has a pH value of 11.

### Claim 3 (depends on 1)

The method according to claim 1, wherein said adsorbent of lithium-containing manganese oxide is a granular adsorbent comprising powder of lithium-containing manganese oxide, and a polymer as a binder.

### Claim 4 (depends on 3)

The method according to claim 3, wherein said binder is poly(vinyl chloride).

### Claim 5 (depends on 1)

The method according to claim 1, wherein said adsorbent of lithium-containing manganese oxide comprises LiMn2O4 or Li2MnO3.

### Claim 6 (depends on 3)

The method according to claim 3, wherein said powder of lithium-containing manganese oxide is prepared by (a) mixing Li2O and a manganese compound; (b) heating the resulting mixture at a temperature of 300-1200° C. to form a product containing lithium and manganese; and (c) leaching lithium out of the product with an acidic solution.

### Claim 7 (depends on 6)

The method according to claim 6, wherein said granular adsorbent of lithium-containing manganese oxide is prepared by dissolving poly(vinyl chloride) as said binder in an organic solvent; mixing said powder of lithium-containing manganese oxide with the resulting solution to form a slurry; passing said slurry through a capillary into a liquid to form granules, wherein said liquid has affinity to the organic solvent and is a nonsolvent to the poly(vinyl chloride); and contacting the granules with an aqueous solution of an acid to elute lithium.

### Claim 8 (depends on 7)

The method according to claim 7, wherein said organic solvent is N-methyl-2-pyrrolidone (NMP).

### Claim 9 (depends on 7)

The method according to claim 7, wherein said liquid is water or a mixed liquid of water and alcohol.

### Claim 10 (depends on 1)

The method according to claim 1, wherein said lithium-containing aqueous solution comprises seawater, or brine generated from a process for producing salt from seawater or a pure water producing process from seawater; and an alkali added to said seawater or said brine.

### Claim 11 (depends on 10)

The method according to claim 10, wherein said lithium-containing aqueous solution comprises said brine; and said alkali is NaOH.