# US 2003/0229180 A1 · Disposable bakeware with improved drip resistance at elevated temperatures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0229180 A1
- Document ID: US20030229180A1
- Status: Published application
- Kind: A1
- Application number: 10/163,382
- Filed: 2002-06-07
- Published: 2003-12-11
- Earliest claimed: 2002-06-07
- Assignees: S.C. Johnson & Son, Inc.
- Inventors: John S. Trent; Thayer A. Brown JR.; Kent B. McReynolds; Jeffrey T. Brown
- Web page: https://patentgrep.com/patent/US20030229180A1

## CPC

- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- C08L 27/18: Homopolymers or copolymers or tetrafluoroethene
- Y10S 220/912: Cookware, i.e. pots and pans
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A thermoplastic bakeware article (i.e., an article formed to hold, contain or support food, while being heated in a microwave, conventional oven, convection oven, or the like) that is food-grade and resistant to dripping, stringing, and melting at high temperatures. The article has a composition comprising a partially crystalline polyester resin and a phenoxy resin. The composition is formulated so as to allow cross-linking between the polyester resin and the phenoxy resin at temperatures above about 400° F.

## Claims

### Claim 1

An article having a composition, the composition comprising:
(a) a partially crystalline polyester resin; and
(b) a phenoxy resin,
wherein said article is formed as a food-grade bakeware article, and the composition is formulated so as to allow cross-linking between said polyester resin and said phenoxy resin at temperatures above about 400° F.

### Claim 2 (depends on 1)

The article recited in claim 1, wherein, in the composition, the polyester resin is in an amount of about 64.5 percent to about 85.9 percent, by weight.

### Claim 3 (depends on 2)

The article recited in claim 2, wherein, in the composition, the phenoxy resin is in an amount of about 1 percent to about 25 percent, by weight.

### Claim 4 (depends on 1)

The article recited in claim 1, the composition further comprising a filler in an amount less than about 5 percent, by weight.

### Claim 5 (depends on 4)

The article recited in claim 4, the composition further comprising a fibrillated polytetrafluoroethylene.

### Claim 6 (depends on 5)

The article recited in claim 5, the composition further comprising a nucleating agent.

### Claim 7 (depends on 6)

The article recited in claim 6, the composition further comprising an impact modifier.

### Claim 8 (depends on 7)

The article recited in claim 7, the composition further comprising an antioxidant.

### Claim 9 (depends on 5)

The article recited in claim 5, wherein the fibrillated polytetrafluoroethylene is in an amount of about 0.01 to about 2 percent, by weight, of the composition.

### Claim 10 (depends on 6)

The article recited in claim 6, wherein the nucleating agent is present in an amount of about 0.1 percent to about 10 percent, by weight, of the composition.

### Claim 11 (depends on 7)

The article recited in claim 7, wherein the impact modifier is present in an amount of about 0.5 percent to about 25 percent, by weight, of the composition.

### Claim 12 (depends on 8)

The article recited in claim 8, wherein the antioxidant is in an amount of about 0.01 percent to about 1 percent, by weight, of the composition.

### Claim 13

A thermoformed article having a composition, the composition comprising:
(a) a partially crystalline polyester resin;
(b) a phenoxy resin; and
(c) less than about 5 percent, by weight, of reinforcing agent,
wherein said thermoformed article is formed as a food-grade bakeware article, and the composition is formulated so as to allow cross-linking between said polyester resin and said phenoxy resin at temperatures above 400° F.

### Claim 14 (depends on 13)

The article recited in claim 13, wherein the polyester resin is chosen from the group consisting of poly (ethylene terephthalate) and THERMX™ Copolyester 6761.

### Claim 15 (depends on 13)

The article recited in claim 13, wherein, in the composition, the polyester resin is in an amount of about 64.5 percent to about 85.9 percent, by weight.

### Claim 16 (depends on 15)

The article recited in claim 15, wherein, in the composition, the phenoxy resin is in an amount of about 1 percent to about 25 percent, by weight.

### Claim 17 (depends on 16)

The article recited in claim 16, wherein, in the composition, the phenoxy resin is in an amount of about 5 percent to about 10, by weight.

### Claim 18 (depends on 13)

The article recited in claim 13, the composition further comprising a fibrillated polytetrafluoroethylene resin.

### Claim 19 (depends on 18)

The article recited in claim 18, wherein the polytetrafluoroethylene resin is in an amount of about 0.01 percent to about 2 percent, by weight.

### Claim 20 (depends on 13)

The article recited in claim 13, the composition further comprising a nucleating agent.

### Claim 21 (depends on 20)

The article recited in claim 20, wherein the nucleating agent is in an amount of about 0.1 percent to about 10, by weight.

### Claim 22 (depends on 13)

The article recited in claim 13, the composition further comprising an impact modifier.

### Claim 23 (depends on 22)

The article recited in claim 22, wherein the impact modifier is an acrylic impact modifier.

### Claim 24 (depends on 22)

The article recited in claim 22, wherein the impact modifier is in an amount of about 0.5 percent to about 25 percent, by weight.

### Claim 25 (depends on 13)

The article recited in claim 13, the composition further comprising an antioxidant.

### Claim 26 (depends on 25)

The article recited in claim 25, wherein the antioxidant is present in an amount of about 0.01 percent to about 1 percent, by weight.

### Claim 27 (depends on 13)

The article recited in claim 13, wherein, in the composition, the polyester is in an amount of about 64.5 percent to about 85.9 percent, by weight, and the phenoxy resin is in an amount of about 1 percent to about 25 percent, by weight, the composition further comprising:
(a) a nucleating agent in an amount of about 0.1 percent to about 10 percent, by weight;
(b) an impact modifier in an amount of about 0.5 percent to about 25 percent, by weight; and
(c) an antioxidant in an amount of about 0.01 percent to about 1 percent, by weight.

### Claim 28

A process of making a thermoformed article comprising:
(a) providing a sheet of thermoplastic composition comprising:
(i) a polyester resin;
(ii) a phenoxy resin; and
(iii) less than about 5 percent, by weight, of reinforcing filler; and
(b) thermoforming the sheet into a food-grade bakeware article,
wherein the thermoplastic composition is formulated to allow cross-linking between the polyester resin and the phenoxy resin at temperatures above 400° F.

### Claim 29 (depends on 28)

The process recited in claim 28, wherein the polyester resin is in an amount of about 64.5 percent to about 85.9 percent, by weight, of the composition.

### Claim 30 (depends on 28)

The process recited in claim 28, wherein the phenoxy resin is in an amount of about 1 percent to about 25 percent, by weight, of the composition.

### Claim 31 (depends on 28)

The process recited in claim 28, wherein the sheet provided in said providing step further comprises at least one component selected from the group consisting of a fibrillated polytetrafluoroethylene resin, an impact modifier, and an antioxidant.

### Claim 32 (depends on 31)

The process recited in claim 31, wherein the sheet includes the polytetrafluoroethylene resin in an amount of about 0.01 percent to about 2 percent, by weight.

### Claim 33 (depends on 31)

The process recited in claim 31, wherein the sheet includes the impact modifier in an amount of about 0.5 percent to about 25 percent, by weight.

### Claim 34 (depends on 31)

The process recited in claim 31, wherein the sheet includes the antioxidant in an amount of about 0.01 percent to about 1 percent, by weight.

### Claim 35

An article having a composition comprising:
(a) a partially crystalline polyester resin selected from the group consisting of:
(i) a poly (ethylene terephthalate); and
(ii)THERMX™ Copolyester 6761; and
(b) a phenoxy resin,
wherein said article is formed as a food-grade bakeware article, and the composition is formulated so as to allow cross-linking between said polyester resin and said phenoxy resin at temperatures above 400° F.

### Claim 36 (depends on 35)

The article recited in claim 35, wherein the polyester resin of the composition consists of poly (ethylene terephthalate).

### Claim 37 (depends on 35)

The article recited in claim 35, wherein, in the composition, the polyester resin is in an amount of about 64.5 percent to about 85.9 percent, by weight.

### Claim 38 (depends on 37)

The article recited in claim 37, wherein, in the composition, the phenoxy resin is in an amount of about 1 percent to about 25 percent, by weight.

### Claim 39 (depends on 35)

The article recited in claim 35, the composition further comprising at least one of a fibrillated polytetrafluoroethylene resin, a nucleating agent, an impact modifier, and an antioxidant.

### Claim 40 (depends on 39)

The article recited in claim 39, wherein the composition comprises the polytetrafluoroethylene resin in an amount of about 0.01 percent to about 2 percent, by weight.

### Claim 41 (depends on 39)

The article recited in claim 39, wherein the composition comprises the nucleating agent in an amount of about 0.1 percent to about 10 percent, by weight.

### Claim 42 (depends on 39)

The article recited in claim 39, wherein the composition comprises the impact modifier in an amount of about 0.5 percent to about 25 percent, by weight.

### Claim 43 (depends on 39)

The article recited in claim 39, wherein the composition comprises the antioxidant in an amount of about 0.01 percent to about 1 percent, by weight.

### Claim 44

A process of making an article comprising:
(a) providing a sheet of thermoplastic composition comprising:
(i) a polyester resin selected from the group consisting of:
(1) a poly (ethylene terephthalate); and
(2) THERMX™ Copolyester 6761; and
(b) a phenoxy resin; and
(c) thermoforming the sheet into a food-grade bakeware article,
wherein the thermoplastic composition is formulated to allow cross-linking between the polyester resin and the phenoxy resin at temperatures above 400° F.

### Claim 45 (depends on 44)

The process recited in claim 44, wherein the sheet provided in said providing step comprises less than about 5 percent, by weight, of reinforcing filler.

### Claim 46 (depends on 44)

The process recited in claim 44, wherein, in the sheet provided in said providing step, the polyester consists of poly (ethylene terephthalate).

### Claim 47 (depends on 44)

The process recited in claim 44, wherein, in the sheet provided in said providing step, the polyester resin is in an amount of about 64.5 percent to about 85.9 percent, by weight.

### Claim 48 (depends on 44)

The process recited in claim 44, wherein, in the sheet provided in said providing step, the phenoxy resin is in an amount of about 1 percent to about 25 percent, by weight.