# US 2003/0228770 A1 · Method of forming a thin film with a low hydrogen content on a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0228770 A1
- Document ID: US20030228770A1
- Status: Published application
- Kind: A1
- Application number: 10/403,572
- Filed: 2003-03-31
- Published: 2003-12-11
- Earliest claimed: 2002-06-05
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Seung-Hwan Lee; Jong-Ho Yang
- Web page: https://patentgrep.com/patent/US20030228770A1

## CPC

- H10P 14/6532: {by exposure to a plasma}
- C23C 16/4554: {Plasma being used non-continuously in between ALD reactions (C23C16/56 takes precedence)}
- C23C 16/45546: {specially adapted for a substrate stack in the ALD reactor}
- C23C 16/56: After-treatment
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method of forming a thin film with a low hydrogen contents is provided by positioning a substrate inside a processing chamber, and supplying reacting materials into the chamber, chemisorbing a portion of the reacting materials onto the substrate. Then, a nitrogen (N2) remote plasma treatment is performed to reduce the hydrogen content of thin film layer formed by chemisorption of the reacting materials on the substrate. Accordingly, a thin film is formed having a low hydrogen content, since the hydrogen bonds in the thin film layer formed by chemisorption of the reacting materials are removed.

## Claims

### Claim 1

A method of forming a semiconductor device, comprising: forming a thin film on a semiconductor substrate; and treating the thin film with a nitrogen (N2) plasma treatment to reduce the hydrogen concentration of the thin film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the nitrogen (N2) gas is activated in a plasma generator located on an outside portion of a reaction chamber.

### Claim 3 (depends on 1)

The method of claim 1, wherein the thin film includes a nitride layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the thin film is deposited using an atomic layer deposition (ALD) process.

### Claim 5 (depends on 1)

The method of claim 1, wherein the thin film is deposited using a chemical vapor deposition (CVD) process.

### Claim 6

A method of forming a semiconductor device, comprising:
(a) positioning the substrate inside a chamber;
(b) introducing reacting materials into the chamber;
(c) chemisorbing a portion of the reacting materials onto the substrate; and
(d) carrying out nitrogen(N2) remote plasma treatment to reduce hydrogen concentration in chemisorbed reacting materials.

### Claim 7 (depends on 6)

The method of claim 6, wherein the thin film includes a nitride layer.

### Claim 8 (depends on 6)

The method of claim 6, wherein in carrying out step (d) further comprises removing the non-chemisorbed reacting materials from the chamber.

### Claim 9 (depends on 6)

The method of claim 6, further comprises removing the non-chemisorbed reacting materials from the chamber before carrying out step (d).

### Claim 10

A method of forming a thin film, comprising the steps of:
(a) positioning a substrate inside a chamber;
(b) introducing first reacting materials into the chamber;
(c) forming a single atomic layer on the substrate by chemisorbing a portion of the first reacting materials onto the substrate;
(d) treating the single atomic layer with first nitrogen (N2) plasma treatment to reduce a hydrogen content in the single atomic layer;
(e) introducing second reacting materials into the chamber; and
(f) reacting a portion of the second reacting materials with the single atomic layer to form a thin film on the substrate.

### Claim 11 (depends on 10)

The method of claim 10, wherein the thin film includes a nitride layer.

### Claim 12 (depends on 10)

The method of claim 10, wherein in carrying out step (d) further comprises removing the non-chemisorbed first reacting materials from the chamber.

### Claim 13 (depends on 10)

The method of claim 10, further comprises removing the non-chemisorbed first reacting materials from the chamber before carrying out step (d).

### Claim 14 (depends on 10)

The method of claim 10, further comprising, after carrying out step (f), the step of:
(g) treating the thin film with second nitrogen (N2) plasma treatment to reduce a hydrogen content in the thin film.

### Claim 15 (depends on 14)

The method of claim 14, wherein in carrying out step (g) further comprises removing the non-chemisorbed second reacting materials from the chamber.

### Claim 16 (depends on 14)

The method of claim 14, further comprises removing the non-chemisorbed second reacting materials from the chamber before carrying out step (g).

### Claim 17 (depends on 10)

The method of claim 10, wherein the steps (b) to (f) are repeated at least once.

### Claim 18 (depends on 10)

The method of claim 10, wherein the step (d) further includes activating a nitrogen (N2) gas in a plasma generator located outside the chamber.

### Claim 19 (depends on 14)

The method of claim 14, wherein the step (g) further includes activating a nitrogen (N2) gas in a plasma generator located outside the chamber.

### Claim 20

A method of forming a thin film, comprising the steps of:
(a) positioning a substrate inside a chamber;
(b) introducing first reacting materials into the chamber;
(c) forming a single atomic layer on the substrate by chemisorbing a portion of the first reacting materials on the substrate;
(d) removing non-chemisorbed first reacting materials from the chamber;
(e) introducing second reacting materials into the chamber;
(f) forming a thin film on the substrate by reacting a portion of the second reacting materials with the single atomic layer; and
(g) treating the thin film with nitrogen (N2) plasma treatment to reduce a hydrogen content in the thin film.

### Claim 21 (depends on 20)

The method of claim 20, wherein the thin film includes a nitride layer.

### Claim 22 (depends on 20)

The method of claim 20, wherein in carrying out step (g) further comprises removing the non-reacted second reacting materials from the chamber.

### Claim 23 (depends on 20)

The method of claim 20, further comprises removing the non-reacted second reacting materials from the chamber before carrying out step (g).

### Claim 24 (depends on 20)

The method of claim 20, wherein steps (b) to (g) are repeated at least once.

### Claim 25 (depends on 20)

The method of claim 20, wherein the step (g) further includes activating a nitrogen (N2) gas in a plasma generator located outside the chamber.