# US 2003/0228765 A1 · Semiconductor device manufacture method preventing dishing and erosion during chemical mechanical polishing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0228765 A1
- Document ID: US20030228765A1
- Status: Published application
- Kind: A1
- Application number: 10/326,378
- Filed: 2002-12-23
- Published: 2003-12-11
- Earliest claimed: 2002-06-07
- Assignees: Fujitsu Limited
- Inventors: Motoshu Miyajima; Toshiyuki Karasawa; Tsutomu Hosoda; Satoshi Otsuka
- Web page: https://patentgrep.com/patent/US20030228765A1

## CPC

- H10P 52/403: {of conductive or resistive materials}
- H10P 95/062: {involving a dielectric removal step}
- H10W 20/062: {by smoothing of conductive parts, e.g. by planarisation}
- H10W 20/085: {involving intermediate temporary filling with material}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A first insulating film is formed on an underlying substrate, the first insulating film being made of a first insulating material. A second insulating film is formed on the first insulating film, the second insulating film being made of a second insulating material different from the first insulating material. A trench is formed through the second and first insulating film, the trench reaching at least an intermediate depth of the first insulating film. A wiring layer made of a conductive material is deposited on the second insulating film, the wiring layer burying the trench. The wiring layer is polished to leave the wiring layer in the trench. The wiring layer and second insulating film are polished until the first insulating film is exposed. Irregularity such as dishing and erosion can be suppressed from being formed.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising the steps of:
(a) forming a first insulating film on an underlying substrate, the first insulating film comprising a first insulating material;
(b) forming a second insulating film on the first insulating film, the second insulating film comprising a second insulating material different from the first insulating material;
(c) forming a trench through the second and first insulating films, the trench reaching at least an intermediate depth of the first insulating film;
(d) depositing a wiring layer comprising a conductive material on the second insulating film, the wiring layer burying the trench;
(e) polishing the wiring layer to leave the wiring layer in the trench; and
(f) polishing the wiring layer and the second insulating film until the first insulating film is exposed.

### Claim 2 (depends on 1)

A method according to claim 1, wherein said step (e) polishes the wiring layer under a condition that a polishing speed of the wiring layer is faster than a polishing speed of the second insulating film.

### Claim 3 (depends on 1)

A method according to claim 1, wherein said step (f) polishes the wiring layer and the second insulating film until the first insulating film is exposed, under a condition that a polishing speed of the second insulating film is faster than a polishing speed of the wiring layer.

### Claim 4 (depends on 1)

A method according to claim 1, wherein said step (e) stops polishing in a state that a deepest position of dishing formed on a surface of the wiring layer is higher than a bottom of the second insulating film.

### Claim 5 (depends on 1)

A method according to claim 1, wherein a surface of the first insulating film is hydrophobic.

### Claim 6 (depends on 1)

A method according to claim 1, wherein said step (d) includes a step of depositing a barrier metal layer for preventing diffusion of the conductive material of the wiring layer before the wiring layer is deposited, and the wiring layer is deposited on the barrier metal layer.

### Claim 7 (depends on 6)

A method according to claim 6, wherein said step (e) polishes the wiring layer until the barrier metal layer or the second insulating film is exposed.

### Claim 8 (depends on 1)

A method according to claim 1, wherein:
said step (a) includes a step of forming a third insulating film on the underlying substrate before the first insulating film is formed, the third insulating film comprising an organic insulating material or a porous insulating material having a dielectric constant smaller than a dielectric constant of the first insulating film; and
said step (c) forms the trench reaching at least an intermediate depth of the third insulating film.

### Claim 9 (depends on 1)

A method according to claim 1, wherein the first insulating film comprising a material selected from a group consisting of SiC, SiOC and SiOCH.

### Claim 10 (depends on 1)

A method according to claim 1, wherein the second insulating film comprising silicon oxide.

### Claim 11 (depends on 1)

A method according to claim 1, wherein the wiring layer comprising copper or alloy mainly containing copper.

### Claim 12

A method of forming a wiring layer, comprising the steps of:
(a) forming a first insulating film on an underlying substrate, the first insulating film comprising a first insulating material;
(b) forming a second insulating film on the first insulating film, the second insulating film comprising a second insulating material different from the first insulating material;
(c) forming a trench through the second and first insulating films, the trench reaching at least an intermediate depth of the first insulating film;
(d) depositing a wiring layer comprising a conductive material on the second insulating film, the wiring layer burying the trench;
(e) polishing the wiring layer to leave the wiring layer in the trench; and
(f) polishing the wiring layer and the second insulating film until the first insulating film is exposed.