# US 2003/0228753 A1 · Method of making a semiconductor device that has copper damascene interconnects with enhanced electromigration reliability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0228753 A1
- Document ID: US20030228753A1
- Status: Published application
- Kind: A1
- Application number: 10/165,679
- Filed: 2002-06-06
- Published: 2003-12-11
- Earliest claimed: 2002-06-06
- Assignees: Intel Corporation
- Inventors: Stefan Hau-Riege; Christine Hau-Riege; Wen-Yue Zheng
- Web page: https://patentgrep.com/patent/US20030228753A1

## CPC

- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/049: {by diffusing alloying elements}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of making a semiconductor device is described. That method comprises forming a copper containing layer on a substrate, and forming an alloying layer that includes an alloying element on the copper containing layer. After applying heat to cause an intermetallic layer that includes copper and the alloying element to form on the surface of the copper containing layer, a barrier layer is formed on the intermetallic layer.

## Claims

### Claim 1

A method of making a semiconductor device comprising:
forming a copper containing layer on a substrate;
forming an alloying layer that includes an alloying element on the copper containing layer;
applying heat to cause an intermetallic layer that includes copper and the alloying element to form on the surface of the copper containing layer; and
forming a barrier layer on the intermetallic layer.

### Claim 2 (depends on 1)

The method of claim 1 further comprising:
polishing the copper containing layer, after it is formed, generating a recessed region on top of the copper containing layer;
filling that recessed region with the alloying layer, the alloying layer also forming on the substrate; and then
polishing the alloying layer, after the heating step, to remove it from the substrate, while retaining the intermetallic layer within the recessed region.

### Claim 3 (depends on 2)

The method of claim 2 wherein the recessed region is between about 5 and about 50 nanometers deep.

### Claim 4 (depends on 3)

The method of claim 3 wherein the alloying element comprises a metal selected from the group consisting of calcium, cerium, cadmium, erbium, manganese, tin, zirconium, gold, and nickel.

### Claim 5 (depends on 4)

The method of claim 4 wherein heat is applied at between about 300° C. and about 500° C. for a sufficient time to form the intermetallic layer.

### Claim 6

A method of making a semiconductor device comprising:
forming a dielectric layer on a substrate;
forming a trench within the dielectric layer;
forming a copper containing layer on the dielectric layer, the copper containing layer filling the trench;
removing the copper containing layer from the surface of the dielectric layer, while retaining the copper containing layer where it fills the trench;
forming an alloying layer that includes an alloying element on the copper containing layer and the dielectric layer;
applying heat to cause an intermetallic layer that includes copper and the alloying element to form on the surface of the copper containing layer;
removing the alloying layer from the dielectric layer, while retaining the intermetallic layer where it covers the copper containing layer; and
forming a barrier layer on the intermetallic layer.

### Claim 7 (depends on 6)

The method of claim 6 further comprising:
removing the copper containing layer by polishing it, generating a copper containing layer with a surface that is recessed below the top surface of the dielectric layer, where the copper containing layer fills the trench;
forming the alloying layer on the recessed surface of the copper containing layer and the dielectric layer; and then
polishing the alloying layer, after the heating step, to remove it from the dielectric layer, while retaining the intermetallic layer on the recessed surface of the copper layer.

### Claim 8 (depends on 7)

The method of claim 7 wherein the recessed surface of the copper containing layer is separated from the top surface of the dielectric layer by between about 5 and about 50 nanometers.

### Claim 9 (depends on 8)

The method of claim 8 wherein the alloying element comprises a metal selected from the group consisting of calcium, cerium, cadmium, erbium, manganese, tin, zirconium, gold, and nickel.

### Claim 10

A method of making a semiconductor device comprising:
forming a dielectric layer on a substrate;
forming a trench within the dielectric layer;
lining the trench with a first barrier layer;
forming a copper containing layer on the first barrier layer, the copper containing layer filling the trench;
polishing the copper containing layer until its surface is recessed below the top surface of the dielectric layer, where the copper containing layer fills the trench;
forming an alloying layer that includes an alloying element on the recessed surface of the copper containing layer and on the first barrier layer;
applying heat to cause an intermetallic layer that includes copper and the alloying element to form on the surface of the copper containing layer; and then
polishing the alloying layer to remove it from the first barrier layer, while retaining the intermetallic layer on the recessed surface of the copper layer; and
forming a second barrier layer on the intermetallic layer.

### Claim 11 (depends on 10)

The method of claim 10 wherein the intermetallic layer is between about 5 and about 50 nanometers thick.

### Claim 12 (depends on 11)

The method of claim 11 wherein the alloying element comprises a metal selected from the group consisting of calcium, cerium, cadmium, erbium, manganese, tin, zirconium, gold, and nickel.

### Claim 13 (depends on 12)

The method of claim 12 wherein the first barrier layer is also formed on the dielectric layer, and wherein the first barrier layer remains on the dielectric layer after the copper containing layer is polished.

### Claim 14 (depends on 13)

The method of claim 13 wherein the first barrier layer comprises tantalum and the copper containing layer is polished using a slurry that is selective to tantalum.

### Claim 15 (depends on 14)

The method of claim 14 wherein the first barrier layer is removed from the dielectric layer after the alloying layer is removed from the first barrier layer to generate a substantially planar surface along the intermetallic layer and the dielectric layer.