# US 2003/0228476 A1 · Methods of changing the visible light transmittance of coated articles and coated articles made thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0228476 A1
- Document ID: US20030228476A1
- Status: Published application
- Kind: A1
- Application number: 10/422,096
- Filed: 2003-04-24
- Published: 2003-12-11
- Earliest claimed: 2001-10-22
- Inventors: Harry Buhay; James J. Finley; James P. Thiel; John P. Lehan
- Web page: https://patentgrep.com/patent/US20030228476A1

## CPC

- C23C 14/5806: {Thermal treatment}
- B32B 17/10036: {comprising two outer glass sheets}
- B32B 17/10174: {Coatings of a metallic or dielectric material on a constituent layer of glass or polymer}
- B32B 17/10761: {containing vinyl acetal}
- C03C 17/3417: {all coatings being oxide coatings}
- C03C 17/36: at least one coating being a metal
- C03C 17/3618: {Coatings of type glass/inorganic compound/other inorganic layers, at least one layer being metallic}
- C03C 17/3639: {Multilayers containing at least two functional metal layers}
- C03C 17/3644: {the metal being silver}
- C03C 17/3652: {the coating stack containing at least one sacrificial layer to protect the metal from oxidation}
- C03C 17/366: {Low-emissivity or solar control coatings}
- C03C 17/3681: {the multilayer coating being used in glazing, e.g. windows or windscreens}
- C03C 17/38: at least one coating being a coating of an organic material
- C03C 17/42: at least one coating of an organic material and at least one non-metal coating
- C23C 14/08: Oxides (C23C14/10 takes precedence)
- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- G02B 1/111: using layers comprising organic materials
- C03C 2217/78: Coatings specially designed to be durable, e.g. scratch-resistant
- G02B 5/0808: {having a single reflecting layer (G02B5/0883, G02B5/0891 take precedence)}
- G02B 5/0875: {the reflecting layers comprising two or more metallic layers}
- G02B 5/208: {for use with infrared or ultraviolet radiation, e.g. for separating visible light from infrared and/or ultraviolet radiation}
- Y10T 428/265: 1 mil or less
- Y10T 428/266: of base or substrate
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method is provided for changing the visible light transmittance of a coated article having a functional coating having at least one anti-reflective material and at least one infrared reflective material. The anti-reflective material includes an alloying material capable of combining or alloying with the infrared reflective material. A protective coating is deposited over the functional coating to prevent or retard the diffusion of atmospheric gas and/or vapor into the functional coating. The coated article is heated to a temperature sufficient to cause at least some of the alloying material to combine with at least some of the infrared reflective material to form a substance having a different visible light transmittance than the infrared reflective material.

## Claims

### Claim 1

A method of changing the visible light transmittance of a coated article, comprising:
providing a substrate having a functional coating, the functional coating comprising at least one anti-reflective material and at least one infrared reflective material, wherein the anti-reflective material includes an alloying material capable of combining with the infrared reflective material;
depositing a protective coating over the functional coating, the protective coating preventing or retarding the diffusion of atmospheric gas and/or vapor into the functional coating; and
heating the coated article to a temperature sufficient to cause at least some of the alloying material to combine with at least some of the infrared reflective material to form a combination having a different visible light transmittance than the infrared reflective material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the anti-reflective material includes at least one of tin, antimony, bismuth, indium, or combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the alloying material is selected from tin, antimony, bismuth, indium, or combinations thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the infrared reflective material includes at least one of gold, copper, silver, or mixtures or combinations thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the protective coating includes at least one metal oxide selected from aluminum oxide, silicon oxide, and mixtures thereof.

### Claim 6 (depends on 1)

The method of claim 1, including forming the protective coating to a thickness in the range of greater than 100 Å to less than 10 microns.

### Claim 7 (depends on 1)

The method of claim 1, wherein the protective coating has a refractive index in the range of 1.4 to 1.8.

### Claim 8 (depends on 1)

The method of claim 1, including forming the protective coating to a thickness of greater than or equal to 1 micron.

### Claim 9 (depends on 1)

The method of claim 1, including forming the protective coating to a thickness of less than or equal to 5 microns.

### Claim 10 (depends on 1)

The method of claim 1, wherein the protective coating comprises 0 wt. % to 100 wt. % alumina and 100 wt. % to 0 wt. % silica.

### Claim 11 (depends on 1)

The method of claim 1, wherein the protective coating comprises at least 35 wt. % alumina.

### Claim 12

The method of claim, wherein the protective coating comprises 50 wt. % to 75 wt. % alumina and 25 wt. % to 50 wt. % silica.

### Claim 13 (depends on 1)

The method of claim 1, wherein the protective coating comprises 15 wt. % to 70 wt. % alumina and 85 wt. % to 30 wt. % silica.

### Claim 14 (depends on 1)

The method of claim 1, wherein the protective coating comprises 75 wt. % to 85 wt. % alumina and 15 wt. % to 25 wt. % silica.

### Claim 15 (depends on 1)

The method of claim 1, wherein the protective coating comprises a first layer formed over the functional coating and a second layer formed over the first layer, wherein the first layer comprises 50 wt. % to 100 wt. % alumina and 50 wt. % to 0 wt. % silica, and the second layer comprises 50 wt. % to 100 wt. % silica and 50 wt. % to 0 wt. % alumina.

### Claim 16 (depends on 15)

The method of claim 15, wherein the first layer comprises 70 wt. % to 100 wt. % alumina and 30 wt. % to 0 wt. % silica.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first layer has a thickness in the range of 50 Å to 1 micron.

### Claim 18 (depends on 16)

The method of claim 16, wherein the first layer has a thickness in the range of 100 Å to 250 Å.

### Claim 19 (depends on 15)

The method of claim 15, wherein the second layer comprises 70 wt. % to 100 wt. % silica and 30 wt. % to 0 wt. % alumina.

### Claim 20 (depends on 19)

The method of claim 19, wherein the second layer has a thickness in the range of 50 Å to 2,000 Å.

### Claim 21 (depends on 19)

The method of claim 19, wherein the second layer has a thickness in the range of 300 Å to 500 Å.

### Claim 22 (depends on 1)

The method of claim 1, wherein the protective coating provides an oxygen permeability of less than or equal to 1.5 cubic cm of oxygen gas at a thickness of one mil for 100 square inches over a period of twenty-four hours under an oxygen partial pressure differential of one atmosphere at 23° C. and a relative humidity of zero.

### Claim 23 (depends on 1)

The method of claim 1, further including depositing an alloy prevention layer adjacent the infrared reflective layer, the alloy prevention layer configured to prevent or reduce combination of the infrared reflective material with the alloying material.

### Claim 24 (depends on 23)

The method of claim 23, wherein the alloy prevention layer is at least partially crystalline.

### Claim 25 (depends on 24)

The method of claim 24, wherein the alloy prevention layer includes at least one of zinc oxide, titania, and zirconia.

### Claim 26

A method of making a coated article, comprising:
providing a substrate having a functional coating, the functional coating comprising at least one anti-reflective layer and at least one infrared reflective layer, wherein the anti-reflective layer includes an alloying material capable of combining with the material of the infrared reflective layer;
depositing an alloy prevention layer adjacent the infrared reflective layer, the alloy prevention layer configured to prevent or reduce combination of the infrared reflective material with the alloying material;
depositing a protective coating over the functional coating; and
heating the article.

### Claim 27 (depends on 26)

The method of claim 26, wherein the anti-reflective material includes at least one of tin, antimony, bismuth, indium, or combinations thereof.

### Claim 28 (depends on 26)

The method of claim 26, wherein the alloying material is selected from tin, antimony, bismuth, indium, or combinations thereof.

### Claim 29 (depends on 26)

The method of claim 26, wherein the infrared reflective material includes at least one of gold, copper, silver, or mixtures or combinations thereof.

### Claim 30 (depends on 26)

The method of claim 26, wherein the protective coating includes at least one metal oxide selected from aluminum oxide, silicon oxide, and mixtures thereof.

### Claim 31 (depends on 26)

The method of claim 26, including forming the protective coating to a thickness in the range of greater than 100 Å to less than 10 microns.

### Claim 32 (depends on 26)

The method of claim 26, wherein the protective coating comprises 0 wt. % to 100 wt. % alumina and 100 wt. % to 0 wt. % silica.

### Claim 33 (depends on 26)

The method of claim 26, wherein the protective coating comprises a first layer formed over the functional coating and a second layer formed over the first layer, wherein the first layer comprises 50 wt. % to 100 wt. % alumina and 50 wt. % to 0 wt. % silica, and the second layer comprises 50 wt. % to 100 wt. % silica and 50 wt. % to 0 wt. % alumina.

### Claim 34 (depends on 26)

The method of claim 26, wherein the alloy prevention layer is at least partially crystalline.

### Claim 35 (depends on 34)

The method of claim 34, wherein the alloy prevention layer includes at least one of zinc oxide, titania, and zirconia

### Claim 36

A coated article, comprising:
a substrate;
a functional coating deposited over at least a portion of the substrate, comprising:
at least on anti-reflective layer;
at least one alloy prevention layer deposited over at least a portion of the anti-reflective layer; and
at least one infrared reflective layer deposited over at least a portion of the alloy prevention layer, wherein the anti-reflective layer includes an alloying material capable of combining with the infrared reflective layer; and
a protective coating deposited over at least a portion of the infrared reflective layer.

### Claim 37 (depends on 36)

The article of claim 36, wherein the anti-reflective layer includes at least one of tin, antimony, bismuth, indium, or combinations thereof.

### Claim 38 (depends on 36)

The article of claim 36, wherein the alloying material is selected from tin, antimony, bismuth, indium, or combinations thereof.

### Claim 39 (depends on 36)

The article of claim 36, wherein the infrared reflective layer includes at least one of gold, copper, silver, or mixtures or combinations thereof.

### Claim 40 (depends on 36)

The article of claim 36, wherein the protective coating includes a metal oxide selected from aluminum oxide, silicon oxide, and mixtures thereof.

### Claim 41 (depends on 36)

The article of claim 36, wherein the protective coating has a thickness in the range of greater than 100 Å to less than 10 microns.

### Claim 42 (depends on 36)

The article of claim 36, wherein the protective coating has a refractive index in the range of 1.4 to 1.8.

### Claim 43 (depends on 36)

The article of claim 36, wherein the article is an automotive transparency.

### Claim 44 (depends on 36)

The article of claim 36, wherein the protective coating comprises 0 wt. % to 100 wt. % alumina and 100 wt. % to 0 wt. % silica.

### Claim 45 (depends on 36)

The article of claim 36, wherein the protective coating comprises 50 wt. % to 75 wt. % alumina and 25 wt. % to 50 wt. % silica.

### Claim 46 (depends on 36)

The article of claim 36, wherein the protective coating comprises a first layer formed over the functional coating and a second layer formed over the first layer, wherein the first layer comprises 50 wt. % to 100 wt. % alumina and 50 wt. % to 0 wt. % silica, and the second layer comprises 50 wt. % to 100 wt. % silica and 50 wt. % to 0 wt. % alumina.

### Claim 47 (depends on 36)

The article of claim 36, wherein the alloy prevention layer is adjacent the infrared reflective layer and is at least partially crystalline.

### Claim 48 (depends on 36)

The article of claim 36, wherein the alloy prevention layer includes at least one of zinc oxide, titania, and zirconia.

### Claim 49

A coated article, comprising:
a substrate;
a functional coating deposited over at least a portion of the substrate, the functional coating comprising:
an anti-reflective layer;
an infrared reflective layer deposited over at least a portion of the antireflective layer, wherein the anti-reflective layer contains a material capable of alloying with the material of the infrared reflective layer; and a protective coating deposited over at least a portion of the infrared reflective layer.

### Claim 50 (depends on 49)

The article of claim 49, wherein the anti-reflective layer includes at least one of tin, antimony, bismuth, indium, or combinations thereof.

### Claim 51 (depends on 49)

The article of claim 49, wherein the alloying material is selected from tin, antimony, bismuth, indium, or combinations thereof.

### Claim 52 (depends on 49)

The article of claim 49, wherein the infrared reflective layer includes at least one of gold, copper, silver, or mixtures or combinations thereof.

### Claim 53 (depends on 49)

The article of claim 49, wherein the protective coating includes a metal oxide selected from aluminum oxide, silicon oxide, and mixtures thereof.

### Claim 54 (depends on 49)

The article of claim 49, wherein the protective coating has a thickness in the range of greater than 100 Å to less than 10 microns.

### Claim 55 (depends on 49)

The article of claim 49, wherein the article is an automotive transparency.

### Claim 56 (depends on 49)

The article of claim 49, wherein the protective coating comprises 0 wt. % to 100 wt. % alumina and 100 wt. % to 0 wt. % silica.

### Claim 57 (depends on 49)

The article of claim 49, wherein the protective coating comprises 50 wt. % to 75 wt. % alumina and 25 wt. % to 50 wt. % silica.

### Claim 58 (depends on 49)

The article of claim 49, wherein the protective coating comprises a first layer formed over the functional coating and a second layer formed over the first layer, wherein the first layer comprises 50 wt. % to 100 wt. % alumina and 50 wt. % to 0 wt. % silica, and the second layer comprises 50 wt. % to 100 wt. % silica and 50 wt. % to 0 wt. % alumina.

### Claim 59 (depends on 49)

The article of claim 49, further including at least one alloy prevention layer deposited over at least a portion of the anti-reflective layer.

### Claim 60 (depends on 59)

The article of claim 59, wherein the alloy prevention layer is at least partially crystalline.

### Claim 61 (depends on 60)

The article of claim 60, wherein the alloy prevention layer includes at least one of zinc oxide, titania, and zirconia.