# US 2003/0227782 A1 · High temperature lighting bulb shield

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0227782 A1
- Document ID: US20030227782A1
- Status: Published application
- Kind: A1
- Application number: 10/139,861
- Filed: 2002-05-06
- Published: 2003-12-11
- Earliest claimed: 2002-05-06
- Assignees: North American Lighting, Inc.
- Inventors: Thomas J. Poorman
- Web page: https://patentgrep.com/patent/US20030227782A1

## CPC

- C25D 3/22: of zinc
- F21S 41/435: {Hoods or cap-shaped}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- F21S: NON-PORTABLE LIGHTING DEVICES; SYSTEMS THEREOF; VEHICLE LIGHTING DEVICES SPECIALLY ADAPTED FOR VEHICLE EXTERIORS

## Abstract

A method and apparatus for a high temperature corrosion resistant composition. The composition is formed into a bulb shield for a vehicle, including automobiles and motorcycles. An alloy composition may be used to stamp a bulb shield. The bulb shield may comprise a cup portion and a connector. Either the cup portion, the connector, or both may comprise an Inconel® alloy composition. The bulb shield may be positioned in front of a headlight bulb to steer light in a desired direction. The bulb shield may be electropolished to provide a decorative attribute to the lamp. The bulb shield may be exposed to high temperatures from the headlight bulb. The Inconel® composition resists deterioration and discoloration of the bulb shield due to the high temperatures. The Inconel® 600 composition also improves the durability of the bulb shield.

## Claims

### Claim 1

A method of forming a vehicle lighting device metal part comprising:
forming a deterioration resistant Nickel Chromium Iron alloy composition into at least a portion of a metal part having a cup portion and a connector;
electropolishing the metal part; and
applying a treatment onto at least a portion of the metal part.

### Claim 2 (depends on 1)

The method of claim 1, wherein the deterioration resistant alloy composition comprises at least 14% Chromium (Cr).

### Claim 3 (depends on 1)

The method of claim 1, wherein the deterioration resistant alloy composition comprises at least 6% Iron (Fe).

### Claim 4 (depends on 1)

The method of claim 1, wherein the deterioration resistant alloy composition comprises about 14-17% Chromium (Cr), about 6-10% Iron (Fe), and a balance Nickel (Ni).

### Claim 5 (depends on 1)

The method of claim 1, wherein the deterioration resistant alloy composition comprises about 14-17% Chromium (Cr), about 6-10% Iron (Fe), and about 72% Nickel (Ni).

### Claim 6 (depends on 1)

The method of claim 1, wherein the metal part is a bulb shield for a vehicle headlight on a motorcycle.

### Claim 7 (depends on 1)

The method of claim 1, wherein the treatment is selected from the group consisting of paint, metallization, chrome sputtering, and aluminum coating.

### Claim 8 (depends on 1)

The method of claim 1, wherein applying a treatment comprises painting an inner portion of the metal part.

### Claim 9 (depends on 1)

The method of claim 1, wherein the cup portion comprises the deterioration resistant alloy composition.

### Claim 10 (depends on 1)

The method of claim 1, wherein the connector comprises the deterioration resistant alloy composition.

### Claim 11 (depends on 1)

The method of claim 1, wherein the connector and the cup portion comprise the deterioration resistant alloy composition.

### Claim 12

An automotive lighting metal part comprising in combination:
a cup portion having an inner surface and an outer surface; and
a connector rigidly coupled to the cup portion,
wherein at least a portion of the cup portion comprises a deterioration resistant Inconel® alloy composition.

### Claim 13 (depends on 12)

The method of claim 12, wherein the deterioration resistant Inconel® alloy composition is electropolished on at least one surface.

### Claim 14 (depends on 12)

The method of claim 12, wherein the deterioration resistant Inconel® alloy composition comprises approximately 14-17% Chromium (Cr).

### Claim 15 (depends on 12)

The method of claim 12, wherein the deterioration resistant Inconel® alloy composition comprises approximately 6-10% Iron (Fe).

### Claim 16 (depends on 12)

The method of claim 12, wherein the deterioration resistant Inconel® alloy composition comprises approximately 14-17% Chromium (Cr), approximately 6-10% Iron (Fe), and approximately balance Nickel (Ni).

### Claim 17 (depends on 12)

The method of claim 12, wherein the deterioration resistant Inconel® alloy composition comprises approximately 14-17% Chromium (Cr), approximately 6-10% Iron (Fe), and approximately 72% Nickel (Ni).

### Claim 18 (depends on 12)

The automotive lighting metal part of claim 12, wherein the connector is comprised of the deterioration resistant Inconel® alloy composition.

### Claim 19 (depends on 12)

The automotive lighting metal part of claim 12, wherein the automotive lighting metal part is a bulb shield for a headlight on a motorcycle, or fog lamp, or automotive head lamp, or truck head lamp.

### Claim 20 (depends on 12)

The automotive lighting metal part of claim 12, wherein the inner surface of the cup portion is comprised of the deterioration resistant Inconel® alloy composition.

### Claim 21 (depends on 12)

The automotive lighting metal part of claim 12, wherein the outer surface of the cup portion is comprised of the deterioration resistant Inconel® alloy composition.

### Claim 22 (depends on 12)

The automotive lighting metal part of claim 12, wherein the outer surface and the inner surface of the cup portion are comprised of the deterioration resistant Inconel® alloy composition.

### Claim 23 (depends on 12)

The automotive lighting metal part of claim 12, wherein the inner portion of the cup portion has a treatment thereon.

### Claim 24 (depends on 22)

The automotive lighting metal part of claim 22, wherein the treatment is selected from the group consisting of paint, metallization, chrome sputtering, and aluminum coating.

### Claim 25

A method of shielding a lighting device comprising the steps of:
providing a bulb shield, the bulb shield having a cup portion for covering a lighting device and a connector rigidly affixed to the cup portion for coupling the bulb shield onto a housing of the lighting device; and
mounting the bulb shield onto the lighting device,
wherein at least a portion of the bulb shield comprises a deterioration resistant alloy composition.

### Claim 26 (depends on 25)

The method of claim 25, wherein the lighting device is selected from the group consisting of a headlight on a motorcycle, a headlight on an automobile or truck, and fog lamp.

### Claim 27 (depends on 25)

The method of claim 25, wherein the deterioration resistant alloy composition comprises substantially 14-17% Chromium (Cr).

### Claim 28 (depends on 25)

The method of claim 25, wherein the deterioration resistant alloy composition comprises substantially 6-10% Iron (Fe).

### Claim 29 (depends on 25)

The method of claim 25, wherein the deterioration resistant alloy composition comprises substantially 14-17% Chromium (Cr), substantially 6-10% Iron (Fe), balance Nickel (Ni).

### Claim 30 (depends on 25)

The method of claim 25, wherein the deterioration resistant alloy composition comprises substantially 14-17% Chromium (Cr), substantially 6-10% Iron (Fe), and substantially 72% Nickel (Ni).