In an ink jet recording method, a surface of a recording paper, in which a base paper contains a pulp fiber and a filler, one surface of the base paper being coated with a polyvalent metal salt in a coating amount of from 0.1 to 3 g/m2, having a basis weight of from 63 to 100 g/m2 and an internal bond strength of from 0.05 to 0.2 N·m is printed using an ink of at least one color made of at least a pigment, a water-soluble organic solvent, water and a surfactant and having a surface tension of from 25 to 37 mN/m. According to the method, the color reproduction is improved, the inter color bleeding and the feathering of characters are reduced, the double-sided printability is provided by reducing curling and cockling occurring immediately after printing, and curling and cockling occurring after allowing to stand and drying are also reduced.
An ink jet recording method comprising a step of printing on a recording paper by using a pigment ink of at least one color, the recording paper containing a base paper and a coating, the base paper containing a pulp fiber and a filler, the coating containing a polyvalent metal salt, and the coating amount on one surface of the base paper being from 0.1 to 3 g/m2, the recording paper having a basis weight of from 63 to 100 g/m2 and an internal bond strength of from 0.05 to 0.2 N·m, the pigment ink containing a water-soluble organic solvent, water and a surfactant and having a surface tension of from 25 to 37 mN/m.
An ink jet recording paper comprising a base paper and a coating, the base paper containing a pulp fiber and a filler, the coating containing a polyvalent metal salt and the coating amount on one surface of the base paper being from 0.1 to 3 g/m2, the recording paper having a basis weight of from 63 to 100 g/m2 and an internal bond strength of from 0.05 to 0.2 N·m.
Dependencies are inferred from the claim text.