# US 2003/0226832 A1 · Scribing sapphire substrates with a solid state UV laser

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0226832 A1
- Document ID: US20030226832A1
- Status: Published application
- Kind: A1
- Application number: 10/384,439
- Filed: 2003-03-06
- Published: 2003-12-11
- Earliest claimed: 2002-06-10
- Assignees: New Wave Research
- Inventors: Kuo-Ching Liu; Pei Hsien Fang; Dan Dere; Jenn Liu; Jih-Chuang Huang; Antonio Lucero; Scott Pinkham; Steven Oltrogge; Duane Middlebusher
- Web page: https://patentgrep.com/patent/US20030226832A1

## CPC

- B23K 26/40: taking account of the properties of the material involved
- B23K 26/032: {using optical means}
- B23K 26/0622: by shaping pulses
- B23K 26/073: Shaping the laser spot
- B23K 26/364: for making a groove or trench, e.g. for scribing a break initiation groove
- B28D 5/0011: {with preliminary treatment, e.g. weakening by scoring}
- B23K 2101/40: Semiconductor devices
- B23K 2103/36: {Wood or similar materials}
- B23K 2103/50: {Inorganic materials other than metals or composite materials}
- H01S 5/0201: {Separation of the wafer into individual elements, e.g. by dicing, cleaving, etching or directly during growth}
- H01S 5/0213: {Sapphire, quartz or diamond based substrates}
- H01S 5/32341: {blue laser based on GaN or GaP}
- H10H 20/01: Manufacture or treatment
- H10P 54/00: Cutting or separating of wafers, substrates or parts of devices
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B28D: WORKING STONE OR STONE-LIKE MATERIALS
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A process and system scribe sapphire substrates, by performing the steps of mounting a sapphire substrate, carrying an array of integrated device die, on a stage such as a movable X-Y stage including a vacuum chuck; and directing UV pulses of laser energy directed at a surface of the sapphire substrate using a solid-state laser. The pulses of laser energy have a wavelength below about 560 nanometers, and preferably between about 150 in 560 nanometers. In addition, energy density, spot size, and pulse duration are established at levels sufficient to induce ablation of sapphire. Control of the system, such as by moving the stage with a stationary beam path for the pulses, causes the pulses to contact the sapphire substrate in a scribe pattern at a rate of motion causing overlap of successive pulses sufficient to cut scribe lines in the sapphire substrate.

## Claims

### Claim 1

A method for manufacturing die from a sapphire substrate, comprising;
mounting the sapphire substrate on a stage, the sapphire substrate having a top surface and a bottom surface, the bottom surface facing the stage;
coupling laser energy having a wavelength below about 560 nanometers, directly into the top surface of the sapphire substrate by absorption sufficient to induce ablation of sapphire at the top surface; and
causing the laser energy to impact the sapphire substrate in a scribe pattern to cut scribe lines in the sapphire substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein said coupling includes directing pulses of laser energy at a surface of the sapphire substrate, the pulses having an energy density, a spot size, a repetition rate and a pulse duration inducing non-linear absorption of the laser energy by the sapphire substrate.

### Claim 3 (depends on 1)

The method of claim 1, including using a solid state laser to generate said laser energy.

### Claim 4 (depends on 1)

The method of claim 1, wherein said wavelength is about 355 nanometers.

### Claim 5 (depends on 1)

The method of claim 1, including using a Nd-doped solid state laser having a primary laser wavelength to generate said laser energy, and said wavelength of said laser energy is a fourth harmonic wavelength of said primary laser wavelength.

### Claim 6 (depends on 1)

The method of claim 1, including separating die defined by the scribe pattern from the sapphire substrate.

### Claim 7 (depends on 1)

The method of claim 1, wherein said coupling includes causing delivering a sequence of overlapping pulses of laser energy to the sapphire substrate.

### Claim 8 (depends on 1)

The method of claim 1, wherein the wavelength is between about 150 and 560 nanometers.

### Claim 9 (depends on 1)

The method of claim 1, wherein said coupling includes causing delivering a sequence of overlapping pulses of laser energy to the sapphire substrate with a repetition rate between about 10 kHz and 50 kHz.

### Claim 10 (depends on 1)

The method of claim 1, wherein said coupling includes causing delivering a sequence of overlapping pulses of laser energy to the sapphire substrate with a pulse duration between about 10 and 30 nanoseconds, and a spot size between about 5 and 25 microns.

### Claim 11 (depends on 1)

The method of claim 1, wherein the sapphire substrate has a thickness, and the scribe lines are cut to a depth of more than about one half said thickness.

### Claim 12 (depends on 1)

The method of claim 1, including:
during said coupling, detecting edges of the sapphire substrate, and in response to detected edges, preventing said laser energy from being directed off of the substrate.

### Claim 13 (depends on 1)

The method of claim 1, including:
placing the substrate on an adhesive tape prior to said coupling; and preventing said laser energy from directly impacting the adhesive tape.

### Claim 14 (depends on 1)

The method of claim 1, wherein said coupling includes generating pulses of laser energy using a Q-switched Nd:YAG laser.

### Claim 15 (depends on 1)

The method of claim 1, wherein said coupling includes generating pulses of laser energy using a Q-switched Nd:YVO4 laser.

### Claim 16 (depends on 1)

The method of claim 1, wherein said coupling includes generating pulses of laser energy using a diode pumped, Q-switched solid state laser.

### Claim 17 (depends on 1)

The method of claim 1, wherein the coupling includes providing laser energy with a spot size on the surface of the sapphire substrate between 5 and 15 microns.

### Claim 18 (depends on 1)

The method of claim 1, wherein the substrate has an active surface and a back side, and including placing the active surface of the substrate on an adhesive tape, and mounting the substrate on the stage to couple the laser energy into the back side of the substrate.

### Claim 19 (depends on 1)

The method of claim 1, wherein the substrate has an active surface and a back side, and including coupling the laser energy into the back side.