# US 2003/0226828 A1 · Part interface design for welding materials that are difficult to weld

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0226828 A1
- Document ID: US20030226828A1
- Status: Published application
- Kind: A1
- Application number: 10/166,100
- Filed: 2002-06-10
- Published: 2003-12-11
- Earliest claimed: 2002-06-10
- Assignees: International Business Machines Corporation
- Inventors: Satya P. Arya
- Web page: https://patentgrep.com/patent/US20030226828A1

## CPC

- B23K 33/00: Specially-profiled edge portions of workpieces for making soldering or welding connections; Filling the seams formed thereby
- B23K 11/002: {specially adapted for particular articles or work}
- B23K 11/11: Spot welding
- B23K 26/32: taking account of the properties of the material involved
- B23K 2103/10: Aluminium or alloys thereof
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A joining technique and design for welding hard to weld elements of a disk drive suspension machines or coins the parts to be welded at their weld interface. A small pocket is formed at the weld interface to let evaporated material gases escape during welding and reduce gas bubble trapping in the weld nugget. For laser welding, a pocket is formed in thick parts to control the welded web thickness for fast melting and thorough mixing of top and bottom materials. For resistance spot welding, it may be necessary to form pockets in both materials on the electrode contact side to reduce material thickness. This technique provides a weld interface design that solves joint reliability and dynamic variation problems. This technique can be used to attach aluminum-to-aluminum or other materials that are difficult to weld due to porous welds, and to improve weld quality of both spot and seam welds.

## Claims

### Claim 1

A method of joining materials, comprising:
providing a first component with a gas release pocket in a first surface that extends from an interior portion of the first component to an exterior of the first component;
positioning a second component adjacent to the first component such that the gas release pocket is located therebetween and is in communication with an atmosphere;
welding the first component to the second component by applying local heat to a weld site on one of the components to form a weld nugget that extends through the gas release pocket and between the first and second components; and
releasing weld-related gases to the atmosphere through the gas release pocket to reduce a porosity of the weld nugget.

### Claim 2 (depends on 1)

The method of claim 1, further comprising the step of forming the gas release pocket in the first component at a depth of approximately 10 to 200 μm.

### Claim 3 (depends on 1)

The method of claim 1, further comprising the step of supplying an inert gas to reduce oxidation of the weld.

### Claim 4 (depends on 1)

The method of claim 1 wherein a device for applying local heat during the welding step is selected from the group consisting of a laser beam, a resistance welder, and an arc welder.

### Claim 5 (depends on 1)

The method of claim 1 wherein the welding step comprises forming a single spot weld or a weld seam.

### Claim 6 (depends on 1)

The method of claim 1, further comprising the step of forming a weld pocket at said weld site in order to reduce a welded web thickness and reduce the input heat energy required to complete the weld.

### Claim 7 (depends on 1)

The method of claim 1, further comprising the step of providing a formed shape of welding rod material at the weld site to form a stronger homogenous weld nugget.

### Claim 8 (depends on 1)

The method of claim 1, further comprising the steps of:
shearing off the first component to form a sheared weld nugget having protrusions extending from the second component;
locating a replacement first component on the second component such that a replacement gas release pocket on the replacement first component accommodates the protrusions;
welding the replacement first component to the second component by applying local heat to a replacement weld site on one of the replacement first component and the second component to melt the sheared weld nugget and form a replacement weld nugget that extends through the replacement gas release pocket and between the first and second components, and excess material of the sheared weld nugget, now as part of the replacement weld nugget, grows into the replacement gas release pocket; and
releasing weld-related gases to the atmosphere through the replacement gas release pocket to reduce a porosity of the replacement weld nugget.

### Claim 9

A method of joining materials, comprising:
providing a first component with a gas release pocket in a first surface that extends from an interior portion of the first component to an exterior of the first component, and a weld pocket that is formed on a second surface of the first component opposite a portion of the gas release pocket;
positioning a second component adjacent to the first component such that the gas release pocket is located therebetween and is in communication with an atmosphere;
welding the first component to the second component by applying local heat to the weld pocket to form a weld nugget that extends through the gas release pocket and between the first and second components; and
releasing weld-related gases to the atmosphere through the gas release pocket to reduce a porosity of the weld nugget.

### Claim 10 (depends on 9)

The method of claim 9, further comprising the step of forming the gas release pocket in the first component at a depth of approximately 10 to 200 μm.

### Claim 11 (depends on 9)

The method of claim 9, further comprising the step of supplying an inert gas to reduce oxidation of the weld.

### Claim 12 (depends on 9)

The method of claim 9 wherein a device for applying local heat during the welding step is selected from the group consisting of a laser beam, a resistance welder, and an arc welder.

### Claim 13 (depends on 9)

The method of claim 9 wherein the welding step comprises forming a single spot weld or a weld seam.

### Claim 14 (depends on 9)

The method of claim 9, further comprising the step of providing a formed shape of welding rod material in the weld pocket to form a stronger homogenous weld nugget.

### Claim 15 (depends on 9)

The method of claim 9, further comprising the steps of:
shearing off the first component to form a sheared weld nugget having protrusions extending from the second component;
locating a replacement first component on the second component such that a replacement gas release pocket on the replacement first component accommodates the protrusions;
welding the replacement first component to the second component by applying local heat to a replacement weld site on one of the replacement first component and the second component to melt the sheared weld nugget and form a replacement weld nugget that extends through the replacement gas release pocket and between the first and second components, and excess material of the sheared weld nugget, now as part of the replacement weld nugget, grows into the replacement gas release pocket; and
releasing weld-related gases to the atmosphere through the replacement gas release pocket to reduce a porosity of the replacement weld nugget.

### Claim 16

A weld assembly, comprising:
a first component having a first surface with a weld pocket formed therein, a second surface with a gas release pocket formed therein that extends from a location opposite the weld pocket to an exterior of the first component;
a second component having a first surface adjacent to the second surface of the first component such that the gas release pocket is located therebetween; and
a weld nugget extending between the first and second components through the gas release pocket such that weld-related gases formed during the welding process escape through the gas release pocket.

### Claim 17 (depends on 16)

The weld assembly of claim 16 wherein the gas release pocket has a depth, relative to the second surface of the first component, of approximately 10 to 200 μm.

### Claim 18 (depends on 16)

The weld assembly of claim 16 wherein the nugget is a single spot weld or a weld seam.