# US 2003/0226476 A1 · Method for producing basalt flaky filler for composites

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0226476 A1
- Document ID: US20030226476A1
- Status: Published application
- Kind: A1
- Application number: 10/366,055
- Filed: 2003-02-13
- Published: 2003-12-11
- Earliest claimed: 2000-12-13
- Inventors: Vera Vasilyevna Efanova
- Web page: https://patentgrep.com/patent/US20030226476A1

## CPC

- C03B 37/005: Manufacture of flakes
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C09C 1/00: Treatment of specific inorganic materials other than fibrous fillers (tenebrescent materials C09K9/00; luminescent materials C09K11/00); Preparation of carbon black
- C09C 1/0018: {uncoated and unlayered plate-like particles}
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}

## Abstract

A method produces basalt flaky filler for composites by crushing and melting basalt, shaping hard flaky vitreous particles from the melt, and subjecting such particles to thermochemical treatment in an oxidizing atmosphere until a crystal phase is developed, with the thermochemical treatment the flaky particles performed at a temperature ranging from about 680° C. to about 850° C. until at least about 12% by weight of the crystal phase is obtained, and at least 7×1019 spin/cm3 of the reactive paramagnetic centers are developed, followed by air cooling of the flakes to form the filler.

## Claims

### Claim 1

A method for producing basalt flaky filler for composites, the method comprising the steps of:
(a) obtaining hard vitreous flakes by:
(a1) crushing basalt to sizes suitable for insertion into a melting furnace;
(a2) heating the crushed basalt to obtain a thin melt; and
(a3) breaking up a stream of the melt flowing through a heated die into hard vitreous flakes by a whirler and/or an airstream;
(b) performing thermochemical treatment of the hard vitreous flakes from step (a) in an oxidizing atmosphere at temperature ranging from about 680° C. to about 850° C. until an incomplete crystallization of at least about 12% by weight of the crystal phase is obtained, and at least 7×1019 spin/cm3 of the reactive paramagnetic centers are developed; and
(c) air cooling the thermochemically treated flakes to form the basalt flaky filler.

### Claim 2 (depends on 1)

The method according to claim 1 wherein the step (b) of performing the thermochemical treatment of the vitreous flakes is carried out in air at a temperature ranging from about 680° C. to about 780° C.

### Claim 3 (depends on 1)

The method according to claim 1 further comprising the step of:
(c1) mechanical treating the thermochemically treated flakes by fragmentation and separation according to size until the basalt flaky filler containing at least about 30% of particles having a mean size of about 100 μm. across to the total amount of the particles and at least about 14×1019 spin/cm3 of the reactive paramagnetic centers are obtained.

### Claim 4 (depends on 2)

The method according to claim 2 further comprising the step of:
(c1) mechanical treating the thermochemically treated flakes by fragmentation and separation according to size until the basalt flaky filler containing at least about 30% of particles having a mean size of about 100 μm. across to the total amount of the particles and at least about 14×1019 spin/cm3 of the reactive paramagnetic centers are obtained.

### Claim 5 (depends on 1)

The basalt flaky filler formed by the method of claim 1.

### Claim 6 (depends on 2)

The basalt flaky filler formed by the method of claim 2.

### Claim 7 (depends on 3)

The basalt flaky filler formed by the method of claim 3.

### Claim 8 (depends on 4)

The basalt flaky filler formed by the method of claim 4.