# US 2003/0226375 A1 · Method for making extreme ultraviolet lithography structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0226375 A1
- Document ID: US20030226375A1
- Status: Published application
- Kind: A1
- Application number: 10/302,347
- Filed: 2002-11-22
- Published: 2003-12-11
- Earliest claimed: 2001-11-27
- Assignees: Corning Incorporated
- Inventors: James J. Bernas; Bradley F. Bowden; Kenneth E. Hrdina
- Web page: https://patentgrep.com/patent/US20030226375A1

## CPC

- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03B 19/06: by sintering, {e.g. by cold isostatic pressing of powders and subsequent sintering, by hot pressing of powders, by sintering slurries or dispersions not undergoing a liquid phase reaction}
- B33Y 80/00: Products made by additive manufacturing
- C03B 2201/42: doped with titanium
- C03C 2201/42: containing titanium
- C03C 2203/10: Melting processes
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

A method for forming EUV LITHOGRAPHY GLASS STRUCTURES WITH VOIDS is disclosed which includes forming a slurry mixture including silica soot particles, and inserting the slurry mixture into a casting mold. The method provides low weight mass reduced rigid glass structures with beneficial thermal stability. The casting mold includes therein a casting form. The casting form is adapted to provide selected geometry void spaces within the glass lithography structure. The slurry mixture is dried to form a green ware object. The casting form is removed from the green ware and the green ware object is consolidated into a lithography glass structure with voids.

## Claims

### Claim 1

A method for forming an EUV lithography glass substrate, comprising:
forming a slurry comprising titanium doped silica glass particles;
providing a casting mold including therein a casting form, the casting form adapted to provide selected geometry void spaces within the EUV lithography glass substrate,
inserting the titanium doped silica glass particle slurry into the casting mold;
drying the slurry to form a green ware EUV lithography substrate;
removing the casting form; and
consolidating the green ware into a consolidated glass EUV lithography substrate having a homogeneous titanium silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2 and a homogeneous CTE in the range of +30 ppb/° C. to −30 ppb/° C. at 20-26° C.

### Claim 2 (depends on 1)

The method as defined in claim 1 wherein the casting form comprises microcrystalline wax.

### Claim 3 (depends on 1)

The method as defined in claim 1 wherein the removing the casting form comprises vacuum pyrolysis.

### Claim 4 (depends on 1)

The method as defined in claim 1 wherein the removing the casting form comprises extraction through pore spaces in the green ware.

### Claim 5 (depends on 1)

The method as defined in claim 1 wherein providing a casting mold including therein a casting form includes extruding a casting form through a die.

### Claim 6 (depends on 1)

The method as defined in claim 1 wherein the casting form comprises channels connecting individual elements of the form, the channels forming gas channels in the green ware.

### Claim 7 (depends on 1)

The method as defined in claim 1 wherein the titanium doped silica glass particles is a flame hydrolysis formed titanium doped silica glass particle soot.

### Claim 8 (depends on 1)

The method as defined in claim 1 wherein the titanium doped silica glass particle has a dopant level in the range from 6 wt. % TiO2 to about 8 wt. % TiO2 and said consolidated glass EUV lithography substrate titanium silica glass dopant level is in the range from 6 wt. % TiO2 to about 8 wt. % TiO2.

### Claim 9 (depends on 1)

The method as defined in claim 1 wherein the consolidating comprises heating in a substantially non-reducing atmosphere.

### Claim 10 (depends on 1)

The method as defined in claim 1 wherein the forming the slurry comprises mixing titanium doped silica glass particles with water and ammonia.

### Claim 11

A method for forming a glass substrate with void spaces, comprising:
forming a slurry comprising Ti doped silica soot and H2O, said doped silica soot having a silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2;
providing a glass substrate casting mold including therein a casting form, the casting form adapted to provide selected geometry void spaces within the glass substrate, inserting the Ti doped silica soot and H2O slurry into the casting mold;
drying the Ti doped silica soot and H2O slurry to form a green ware Ti doped silica substrate;
removing the casting form; and
consolidating the green ware into a consolidated glass substrate with void spaces, said consolidated glass having a homogeneous titanium silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2 and a homogeneous CTE is in the range of +30 ppb/° C. to −30 ppb/° C. at 20-26° C.

### Claim 12 (depends on 11)

The method as defined in claim 11 wherein, said doped silica soot silica glass dopant level is 6 to 8 wt. % TiO2 and said consolidated glass homogeneous titanium dopant level is from 6 to 8 wt. % TiO2.

### Claim 13 (depends on 11)

The method as defined in claim 11 wherein, said doped silica soot silica glass dopant level is 6.8-7.5 wt. % TiO2 and said consolidated glass homogeneous titanium dopant level is 6.8-7.5 wt. % TiO2.

### Claim 14 (depends on 12)

The method as defined in claim 12 wherein said consolidated glass homogeneous CTE is in the range of +20 ppb/° C. to −20 ppb/° C. at 20-26° C.

### Claim 15 (depends on 12)

The method as defined in claim 12 wherein said CTE has a variation in coefficient of thermal expansion ≦10 ppb/° C.

### Claim 16 (depends on 14)

The method as defined in claim 14 wherein said CTE has a variation in coefficient of thermal expansion ≦5 ppb/° C.

### Claim 17

A method for forming a lithography structure with void spaces, comprising:
forming a slurry comprising Ti doped silica soot and H2O, said doped silica soot having a silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2;
providing a lithography structure glass substrate casting mold including therein a casting form, the casting form adapted to provide selected geometry void spaces within the lithography structure;
inserting the Ti doped silica soot and H2O slurry into the casting mold;
drying the Ti doped silica soot and H2O slurry to form a green ware Ti doped silica substrate lithography structure;
removing the casting form; and
consolidating the green ware into a consolidated glass lithography structure with void spaces, said consolidated glass having a homogeneous titanium silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2 and a homogeneous CTE is in the range of +30 ppb/° C. to −30 ppb/° C. at 20-26° C.

### Claim 18

A method for forming an EUV lithography glass substrate, comprising:
forming a mixture comprising titanium doped silica glass particles;
providing a casting mold including therein a casting form, the casting form adapted to provide selected geometry void spaces within the EUV lithography glass substrate,
inserting the titanium doped silica glass particle mixture into the casting mold;
drying the mixture to form a green ware EUV lithography substrate;
removing the casting form; and
consolidating the green ware into a consolidated glass EUV lithography substrate having a homogeneous titanium silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2 and a homogeneous CTE in the range of +30 ppb/° C. to −30 ppb/° C. at 20-26° C.

### Claim 19 (depends on 18)

The method as defined in claim 18 wherein the casting form comprises microcrystalline wax.

### Claim 20 (depends on 18)

The method as defined in claim 18 wherein the removing the casting form comprises vacuum pyrolysis.

### Claim 21 (depends on 18)

The method as defined in claim 18 wherein the removing the casting form comprises extraction through pore spaces in the green ware.

### Claim 22 (depends on 18)

The method as defined in claim 18 wherein providing a casting mold including therein a casting form includes extruding a casting form through a die.

### Claim 23 (depends on 18)

The method as defined in claim 18 wherein the casting form comprises channels connecting individual elements of the form, the channels forming gas channels in the green ware.

### Claim 24 (depends on 18)

The method as defined in claim 18 wherein the titanium doped silica glass particles is a flame hydrolysis formed titanium doped silica glass particle soot.

### Claim 25 (depends on 18)

The method as defined in claim 18 wherein the titanium doped silica glass particle has a dopant level in the range from 6 wt. % TiO2 to about 8 wt. % TiO2 and said consolidated glass EUV lithography substrate titanium silica glass dopant level is in the range from 6 wt. % TiO2 to about 8 wt. % TiO2.

### Claim 26 (depends on 18)

The method as defined in claim 18 wherein the consolidating comprises heating in a substantially non-reducing atmosphere.

### Claim 27

A method for forming a glass substrate with void spaces, comprising:
forming a mixture comprising Ti doped silica particles, said doped silica having a silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2;
providing a glass substrate casting mold including therein a casting form, the casting form adapted to provide selected geometry void spaces within the glass substrate, inserting the Ti doped silica mixture into the casting mold;
drying the Ti doped silica mixture to form a green ware Ti doped silica substrate;
removing the casting form; and
consolidating the green ware into a consolidated glass substrate with void spaces, said consolidated glass having a homogeneous titanium silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2 and a homogeneous CTE is in the range of +30 ppb/° C. to −30 ppb/° C. at 20-26° C.

### Claim 28 (depends on 27)

The method as defined in claim 27 wherein, said doped silica glass dopant level is 6 to 8 wt. % TiO2 and said consolidated glass homogeneous titanium dopant level is from 6 to 8 wt. % TiO2.

### Claim 29 (depends on 27)

The method as defined in claim 27 wherein, said doped silica glass dopant level is 6.8-7.5 wt. % TiO2 and said consolidated glass homogeneous titanium dopant level is 6.8-7.5 wt. % TiO2.

### Claim 30 (depends on 27)

The method as defined in claim 27 wherein said consolidated glass homogeneous CTE is in the range of +20 ppb/° C. to −20 ppb/° C. at 20-26° C.

### Claim 31 (depends on 30)

The method as defined in claim 30 wherein said CTE has a variation in coefficient of thermal expansion ≦10 ppb/° C.

### Claim 32 (depends on 30)

The method as defined in claim 30 wherein said CTE has a variation in coefficient of thermal expansion ≦5 ppb/° C.

### Claim 33

A method for forming a lithography structure with void spaces, comprising:
forming a mixture comprising Ti doped silica particles, said doped silica having a silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2;
providing a lithography structure glass substrate casting mold including therein a casting form, the casting form adapted to provide selected geometry void spaces within the lithography structure;
inserting the Ti doped silica particles into the casting mold;
drying the Ti doped silica particles to form a green ware Ti doped silica substrate lithography structure;
removing the casting form; and
consolidating the green ware into a consolidated glass lithography structure with void spaces, said consolidated glass having a homogeneous titanium silica glass dopant level in the range from 6 wt. % TiO2 to about 9 wt. % TiO2 and a homogeneous CTE is in the range of +30 ppb/° C. to −30 ppb/° C. at 20-26° C.