# US 2003/0224599 A1 · Semiconductor device with a copper line having an increased resistance against electromigration and a method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0224599 A1
- Document ID: US20030224599A1
- Status: Published application
- Kind: A1
- Application number: 10/304,579
- Filed: 2002-11-26
- Published: 2003-12-04
- Earliest claimed: 2002-05-31
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Christian Zistl; Jorg Hohage; Hartmut Rulke; Peter Hubler
- Web page: https://patentgrep.com/patent/US20030224599A1

## CPC

- H10W 20/064: {by modifying the conductivity of conductive parts, e.g. by alloying}
- H10P 70/277: {the processing being a planarisation of conductive layers}
- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/055: {by formation methods other than physical vapour deposition [PVD], chemical vapour deposition [CVD] or liquid deposition}
- H10P 50/267: {using plasmas}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A copper line that is formed in a patterned dielectric layer has a copper/silicon film formed on a surface thereof to substantially suppress an electromigration path through this surface. In an in situ process, the exposed copper surface is first cleaned by a reactive plasma ambient including nitrogen and ammonia and after a certain clean period, a gaseous compound comprising silicon, for example silane, is added to the reactive plasma ambient to form the copper/silicon film. Additionally, a capping layer may be deposited, wherein due to the copper/silicon film, any deposition technique or even spin-coating may be used.

## Claims

### Claim 1

A method of protecting a copper surface comprising:
providing a substrate having formed thereon a dielectric layer with a recessed portion and copper structure positioned in the recessed portion, wherein the copper structure has at least one exposed copper surface;
creating a first reactive plasma environment comprising nitrogen and ammonia;
exposing the at least one exposed copper surface to the first reactive plasma environment for a first time interval;
creating a second reactive plasma environment comprising nitrogen, ammonia and a gaseous compound including silicon; and
exposing the at least one exposed copper surface to the second reactive plasma environment for a second time interval that is shorter than the first time interval to form a copper/silicon film on the at least one exposed copper surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first time interval is in the range of approximately 20-100 seconds.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second time interval is in the range of approximately 3-10 seconds.

### Claim 4 (depends on 3)

The method of claim 3, wherein the second time interval is approximately 5 seconds.

### Claim 5 (depends on 1)

The method of claim 1, wherein a temperature of said substrate during exposure to the first and second reactive plasma environments is adjusted to approximately 350-420° C.

### Claim 6 (depends on 5)

The method of claim 5, wherein said temperature is adjusted to approximately 400° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein a flow rate of nitrogen is between approximately 4000-10000 sccm during the first and second time intervals.

### Claim 8 (depends on 1)

The method of claim 1, wherein a flow rate of ammonia is approximately within 100-500 sccm during the first and second time intervals.

### Claim 9 (depends on 1)

The method of claim 1, wherein a flow rate of said gaseous compound including silicon is within approximately 100-350 sccm.

### Claim 10 (depends on 1)

The method of claim 1, wherein said gaseous compound, including silicon, is silane.

### Claim 11 (depends on 1)

The method of claim 1, wherein a pressure of said first and second reactive plasma environments is maintained at approximately 3-6 Torr.

### Claim 12 (depends on 1)

The method of claim 1, further comprising forming a dielectric layer on said copper/silicon film.

### Claim 13 (depends on 12)

The method of claim 12, wherein forming a dielectric layer comprises at least one of depositing and spin-coating at least one of silicon nitride, silicon oxynitride, silicon dioxide, glass and a polymer material.

### Claim 14

A method of protecting a copper surface in a semiconductor device, the method comprising:
providing a substrate having formed thereon a dielectric layer having a recessed portion and copper structure positioned in the recessed portion, wherein the copper structure has at least one exposed copper surface;
cleaning the at least one exposed surface; and
forming a copper/silicon film on the at least one exposed copper surface in situ.

### Claim 15 (depends on 14)

The method of claim 14, wherein cleaning the at least one exposed copper surface includes establishing a reactive plasma ambient in the presence of nitrogen and ammonia.

### Claim 16 (depends on 15)

The method of claim 15, wherein forming a copper/silicon film includes adding a silicon-containing gas to the reactive plasma ambient after a predefined cleaning period.

### Claim 17 (depends on 16)

The method of claim 16, wherein said cleaning period is approximately 20-100 seconds.

### Claim 18 (depends on 16)

The method of claim 16, wherein said silicon-containing gas is supplied for approximately 5 seconds.

### Claim 19 (depends on 18)

The method of claim 18, wherein said silicon-containing gas is silane.

### Claim 20 (depends on 14)

The method of claim 14, wherein said copper/silicon film is a copper suicide film.

### Claim 21 (depends on 14)

The method of claim 14, wherein a temperature of said substrate is maintained within the range of approximately 350-450° C.

### Claim 22 (depends on 21)

The method of claim 21, wherein said temperature is maintained at approximately 400° C.

### Claim 23 (depends on 14)

The method of claim 14, further comprising forming a dielectric material on the surface of said copper/silicon film.

### Claim 24 (depends on 23)

The method of claim 23, wherein forming a dielectric material comprises at least one of depositing and spin-coating at least one of silicon nitride, silicon oxynitride, silicon dioxide, glass and a polymer material.

### Claim 25

A semiconductor device including a metallization layer, the metallization layer comprising at least one copper structure formed in an insulating material, wherein said copper structure has a surface that has a copper/silicon film formed thereon.

### Claim 26 (depends on 25)

The semiconductor device of claim 25, wherein the copper/silicon film at least partially comprises copper silicide.

### Claim 27 (depends on 25)

The semiconductor device of claim 25, wherein the copper/silicon film is covered by a dielectric material.

### Claim 28 (depends on 25)

The semiconductor device of claim 25, wherein a thickness of the copper/silicon film ranges from approximately 5-20 nm.

### Claim 29 (depends on 27)

The semiconductor device of claim 27, wherein said dielectric material is at least one of silicon dioxide, glass and a polymer material.