# US 2003/0224567 A1 · Method for forming dielectric layer of capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0224567 A1
- Document ID: US20030224567A1
- Status: Published application
- Kind: A1
- Application number: 10/293,530
- Filed: 2002-11-12
- Published: 2003-12-04
- Earliest claimed: 2002-05-31
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Jae-Hyoung Choi; Cha-Young Yoo; Suk-Jin Chung; Wan-Don Kim
- Web page: https://patentgrep.com/patent/US20030224567A1

## CPC

- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6544: {to change the morphology of the insulating materials, e.g. transformation of an amorphous layer into a crystalline layer}
- H10D 1/682: {having dielectrics comprising perovskite structures}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A fabrication method for forming a semiconductor device having a capacitor is provided. A capacitor dielectric layer is formed by depositing a first layer and a second layer. The second layer is a major portion of the capacitor dielectric layer. The first layer acts as a seed layer, while the second layer is expitaxially grown. The material of the second layer as deposited is partially crystal. Nuclear generation and crystal growth occur separately so that the crystalline characteristic of the capacitor dielectric layer and the capacitance characteristic of the capacitor are enhanced. Moreover, the capacitor dielectric layer is crystallized at a relatively low temperature or for a relatively short time, thereby reducing leakage current as well as reducing deformation in the lower electrode. Optionally, The material of the second layer as deposited is not partially crystal but amorphous.

## Claims

### Claim 1

A method of fabricating a semiconductor device, comprising:
providing a substrate;
forming a first layer on the substrate, wherein the material of the first layer is amorphous;
crystallizing the first layer; and
forming a second layer on the first layer, wherein the first layer is formed of the same material as the second layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the second layer is formed such that the first layer acts as a seed layer and the atomic arrangement of a portion of the first layer is extended into that of a portion of the second layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second layer is formed by expitaxial growth.

### Claim 4 (depends on 2)

The method of claim 2, which further comprises crystallizing the second layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first and second layers are crystallized by thermal treatment at a first and a second temperature respectively.

### Claim 6 (depends on 5)

The method of claim 5, wherein the second temperature is lower than the first temperature.

### Claim 7 (depends on 6)

The method of claim 6, wherein the first temperature is within a range of 650 to 750° C. and the second temperature is within a range of 450 to 650° C.

### Claim 8 (depends on 2)

The method of claim 2, wherein the first and second layers are formed at a range of 300 to 550° C.

### Claim 9 (depends on 8)

The method of claim 8, wherein the first and second layers are formed at a range of 400 to 480° C.

### Claim 10 (depends on 2)

The method of claim 2, wherein the first layer is formed at the same temperature as the second layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first and second layers are formed at a range of 300 to 500° C.

### Claim 12 (depends on 2)

The method of claim 2, wherein the first and second layers are formed at different temperatures respectively.

### Claim 13 (depends on 12)

The method of claim 12, wherein the second layer is formed at higher temperature than the first layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first layer is formed at a range of 300 to 500° C. and the second layer is formed at a range of 400 to 550° C.

### Claim 15 (depends on 2)

The method of claim 2, wherein the thickness of the first layer is approximately 11˜100% of the thickness of the second layer.

### Claim 16 (depends on 2)

The method of claim 2, wherein the first and second layers are dielectric layers.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first and second layers are tantalum oxide layers.

### Claim 18 (depends on 2)

The method of claim 2, which further comprises:
forming a lower electrode between the substrate and the first layer; and
forming an upper electrode on the second layer;
wherein the composite layer of the first and the second layers is a capacitor dielectric layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein the lower and the upper electrodes are formed of a noble metal.

### Claim 20 (depends on 1)

The method of claim 1, wherein the second layer is formed such that the material of the second layer is amorphous.

### Claim 21 (depends on 20)

The method of claim 20, which further comprises crystallizing the second layer.

### Claim 22 (depends on 21)

The method of claim 21, wherein the first and second layers are crystallized by thermal treatment at a first and a second temperature respectively.

### Claim 23 (depends on 22)

The method of claim 22, wherein the second temperature is lower than the first temperature.

### Claim 24 (depends on 23)

The method of claim 23, wherein the first temperature is within a range of 650 to 750° C. and the second temperature is within a range of 450 to 650° C.

### Claim 25 (depends on 20)

The method of claim 20, wherein the first and second layers are formed at a range of 300 to 550° C.

### Claim 26 (depends on 20)

The method of claim 20, wherein the first layer is formed at a range of 300 to 500° C.

### Claim 27 (depends on 26)

The method of claim 26, wherein the first layer is formed at a range of 400 to 480° C.

### Claim 28 (depends on 20)

The method of claim 20, wherein the second layer is formed at a range of 300 to 550° C.

### Claim 29 (depends on 20)

The method of claim 20, wherein the thickness of the first layer is approximately 11˜100% of the thickness of the second layer.

### Claim 30 (depends on 20)

The method of claim 20, wherein the first and second layers are dielectric layers.

### Claim 31 (depends on 30)

The method of claim 30, wherein the first and second layers are tantalum oxide layers.

### Claim 32 (depends on 20)

The method of claim 20, which further comprises:
forming a lower electrode between the substrate and the first layer; and
forming an upper electrode on the second layer;
wherein the composite layer of the first and the second layers is a capacitor dielectric layer.

### Claim 33 (depends on 32)

The method of claim 32, wherein the lower and the upper electrodes are formed of a noble metal.

### Claim 34

A method of fabricating a semiconductor device, comprising:
providing a substrate;
forming a first layer on the substrate;
crystallizing the first layer; and
forming a second layer on the first layer such that the first layer acts as a seed layer and the atomic arrangement of a portion of the first layer is extended into that of a portion of the second layer.

### Claim 35 (depends on 34)

The method of claim 34, wherein the second layer is formed by expitaxial growth.

### Claim 36 (depends on 34)

The method of claim 34, which further comprises crystallizing the second layer.

### Claim 37 (depends on 36)

The method of claim 36, wherein the first and second layers are crystallized by thermal treatment at a first and a second temperature respectively.

### Claim 38 (depends on 37)

The method of claim 37, wherein the second temperature is lower than the first temperature.

### Claim 39 (depends on 34)

The method of claim 34, wherein the first layer is formed at the same temperature as the second layer.

### Claim 40 (depends on 34)

The method of claim 34, wherein the first and second layers are formed at different temperatures respectively.

### Claim 41 (depends on 40)

The method of claim 40, wherein the second layer is formed at higher temperature than the first layer.

### Claim 42 (depends on 34)

The method of claim 34, which further comprises:
forming a lower electrode between the substrate and the first layer; and
forming an upper electrode on the second layer;
wherein the composite layer of the first and the second layers is a capacitor dielectric layer.

### Claim 43

A method of fabricating a semiconductor device, comprising:
providing a substrate;
forming a first layer on the substrate;
crystallizing the first layer; and
forming a second layer on the first layer, wherein the material of the second layer is amorphous.

### Claim 44 (depends on 43)

The method of claim 43, which further comprises crystallizing the second layer.

### Claim 45 (depends on 44)

The method of claim 44, wherein the first and second layers are crystallized by thermal treatment at a first and a second temperature respectively.

### Claim 46 (depends on 45)

The method of claim 45, wherein the second temperature is lower than the first temperature.

### Claim 47 (depends on 43)

The method of claim 43, which further comprises:
forming a lower electrode between the substrate and the first layer; and
forming an upper electrode on the second layer;
wherein the composite layer of the first and the second layers is a capacitor dielectric layer.