# US 2003/0224157 A1 · Aqueous polymer composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0224157 A1
- Document ID: US20030224157A1
- Status: Published application
- Kind: A1
- Application number: 10/162,457
- Filed: 2002-06-04
- Published: 2003-12-04
- Earliest claimed: 2002-06-04
- Inventors: Mary Anne Regina Matthews; Robert David Solomon
- Web page: https://patentgrep.com/patent/US20030224157A1

## CPC

- C04B 41/009: {characterised by the material treated}
- C04B 41/483: {Polyacrylates}
- C04B 41/63: Macromolecular compounds
- C09D 5/02: Emulsion paints {including aerosols}
- E04D 1/00: Roof covering by making use of tiles, slates, shingles, or other small roofing elements (roofing supports {or underlayers} E04D12/00)
- C04B 2111/00594: {Concrete roof tiles}
- C04B 2111/21: Efflorescence resistance
- Y10T 428/254: Polymeric or resinous material
- Y10T 428/2998: including synthetic resin or polymer
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- E04D: ROOF COVERINGS; SKY-LIGHTS; GUTTERS; ROOF-WORKING TOOLS (coverings of outer walls by plaster or other porous material E04F13/00)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An aqueous polymer composition containing particles of a first polymer and particles of a second polymer with preferred molecular weight ranges, and wax is provided. Coatings prepared from the aqueous polymer composition may be employed as coatings which have water whitening resistance, bead water, and provide resistance to efflorescence to cementitious substrates, such as roof tiles. A method of preparing a coated cementitious substrate with the aqueous polymer composition and an article containing the coated cementitious substrate are also provided.

## Claims

### Claim 1

An aqueous polymer composition comprising:
a) particles of a first polymer;
b) particles of a second polymer; and
c) from 0.1 to 10 weight % wax, based on the total weight of said first polymer and said second polymer;
wherein said first polymer has a weight average molecular weight of 250,000 or greater; wherein said second polymer has a weight average molecular weight of 150,000 or less; and wherein the weight ratio of said first polymer to said second polymer is in the range of 1:3 to 3:1.

### Claim 2 (depends on 1)

The aqueous polymer composition according to claim 1 wherein the average glass transition temperature of a film formed from said aqueous polymer composition is in the range of 0° C. to 50° C.

### Claim 3 (depends on 1)

The aqueous polymer composition according to claim 1 wherein the difference in the glass transition temperature of said first polymer and the glass transition temperature of said second polymer is less than 10° C.

### Claim 4 (depends on 1)

The aqueous polymer composition according to claim 1 wherein said particles of said second polymer are in the range of 20 nm to 350 nm.

### Claim 5

A method for providing a coated cementitious substrate comprising the steps of:
a) preparing an aqueous polymer composition comprising:
1) particles of a first polymer;
2) particles of a second polymer; and
3) from 0.1 to 10 weight % wax, based on the total weight of said first polymer and said second polymer; wherein said first polymer has a weight average molecular weight of 250,000 or greater; wherein said second polymer has a weight average molecular weight of 150,000 or less; and wherein the weight ratio of said first polymer to said second polymer is in the range of 1:3 to 3:1;
b) applying said aqueous polymer composition onto a green cementitious substrate to form a coated green cementitious substrate; and
c) curing or allowing to cure said coated green cementitious substrate to form said coated cementitious substrate.

### Claim 6 (depends on 5)

The method according to claim 5 wherein the average glass transition temperature of a film formed from said aqueous polymer composition is in the range of 0° C. to 50° C.

### Claim 7 (depends on 5)

The method according to claim 5 wherein the difference in the glass transition temperature of said first polymer and the glass transition temperature of said second polymer is less than 10° C.

### Claim 8 (depends on 5)

The method according to claim 5 wherein said particles of said second polymer are in the range of 20 nm to 350 nm.

### Claim 9

An article comprising a coated cementitious substrate comprising:
a) a cementitious substrate; and
b) a coating formed from aqueous polymer composition comprising:
1) particles of a first polymer;
2) particles of a second polymer; and
3) from 0.1 to 10 weight % wax, based on the total weight of said first polymer and said second polymer; wherein said first polymer has a weight average molecular weight of 250,000 or greater; wherein said second polymer has a weight average molecular weight of 150,000 or less; and wherein the weight ratio of said first polymer to said second polymer is in the range of 1:3 to 3:1.

### Claim 10 (depends on 9)

The article according to claim 9 wherein said aqueous polymer composition is applied onto said cementitious substrate prior to cure of said cementitious substrate.