# US 2003/0223928 A1 · Hydrometallurgical process for recovery of cobalt

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0223928 A1
- Document ID: US20030223928A1
- Status: Published application
- Kind: A1
- Application number: 10/157,915
- Filed: 2002-05-31
- Published: 2003-12-04
- Earliest claimed: 2002-05-31
- Assignees: Sherritt International Corporation
- Inventors: Gavin Kerry Wyllie Freeman; Ockert Gerbrandt Pauw; Russell Peter Kofluk; James John Budac
- Web page: https://patentgrep.com/patent/US20030223928A1

## CPC

- C01G 51/20: Complexes with ammonia
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)

## Abstract

There is provided an improvement in a process for producing cobalt (III) hexammine sulphate which process comprises oxidatively pressure leaching nickel cobalt sulphides in an ammoniacal ammonium sulphate solution. The nickel and cobalt sulphides are oxidized to sulphates, and an ammoniacal leach liquor in which dissolved cobalt is predominantly in the (III) oxidation state is produced. The ammoniacal leach liquor is combined with ammonia to precipitate the triple salt of cobalt (III) hexammine sulphate, nickel (II) hexammine and ammonium sulphate which is further treated to produce a crystalline cobalt (III) hexammine sulphate and a nickel enriched leach liquor. The improvement involves the provision of a second oxidative pressure treatment effective to maximize the formation of the desired cobalt (III) hexammine ion, prior to the triple salt precipitation step.

## Claims

### Claim 1

In a process for producing cobalt (III) hexammine sulphate, comprising leaching nickel-cobalt sulphides in an ammoniacal ammonium sulphate solution under elevated pressure of an oxygen-bearing gas and at an elevated temperature with an ammonia to metals mole ratio effective to oxidize nickel and cobalt sulphides to sulphates, and to produce an ammoniacal leach liquor in which dissolved cobalt is predominantly in the (III) oxidation state, and a leach residue, separating the leach liquor from the leach residue and ammoniating the leach liquor by combining it with an effective amount of ammonia and cooling the ammoniated leach liquor whereby the triple salt of cobalt (III) hexammine sulphate, nickel (II) hexammine sulphate and ammonium sulphate is precipitated, recovering the precipitated triple salt from the leach liquor, and repulping the triple salt with an effective amount of water to selectively leach nickel (II) hexammine sulphate and to produce a crystalline cobalt (III) hexammine sulphate and a nickel enriched leach liquor, the improvement comprising: subjecting the essentially residue-free leach liquor obtained from the oxidative pressure leach to a secondary oxidative pressure treatment at elevated temperature in the presence of an oxygen-bearing gas with an ammonia to metals mole ratio effective to produce a leach liquor whereby the formation of cobalt (III) hexammine sulphate therein has been increased.

### Claim 2 (depends on 1)

The process as set forth in claim 1 wherein the temperature of said secondary oxidative pressure treatment ranges between 110 to 150° C.

### Claim 3 (depends on 1)

The process as set forth in claim 1 wherein the concentration of titratable ammonia in said secondary oxidative pressure treatment ranges between 120 to 200 g/L.

### Claim 4 (depends on 1)

The process as set forth in claim 1 wherein the concentration of titratable ammonia ranges between 120 and 200 g/L and the temperature ranges between 110 to 150° C. in said secondary oxidative pressure treatment.

### Claim 5 (depends on 4)

The process as set forth in claim 4 wherein the nickel enriched leach liquor from the primary oxidative leach step is subjected to a polish filtration.

### Claim 6

In a process for producing cobalt metal powder from nickel-cobalt sulphides comprising leaching said nickel-cobalt sulphides in an ammoniacal ammonium sulphate solution under an elevated pressure of an oxygen bearing gas, at a temperature of at least 80° C., with an ammonia to metals mole ratio in the range of 5:1 to 6.5:1 effective to oxidize the nickel and cobalt sulphides to sulphates and to produce an ammoniacal leach liquor in which dissolved cobalt is predominantly in the (III) oxidation state, and a leach residue, separating the leach liquor from the leach residue, combining the leach liquor with an effective amount of anhydrous ammonia and cooling the ammoniated leach liquor to below 50° C., whereby the triple salt of cobalt (III) hexammine sulphate, nickel (I) hexammine sulphate and ammonium sulphate is precipitated, recovering the precipitated triple salt from the leach liquor, repulping the triple salt with an effective amount of water to selectively leach nickel (II) hexammine sulphate and to produce a crystalline cobalt (III) hexammine sulphate with a Co:Ni ratio of at least 100:1 and a nickel enriched leach liquor, redissolving the cobalt (III) hexammine sulphate in hot ammonium sulphate solution, and cooling the solution to precipitate recrystallized cobalt (III) hexammine sulphate having a Co:Ni ratio of at least about 1000:1 and treating the recrystallized cobalt (III) hexammine sulphate to produce cobalt metal therefrom, the improvement comprising: subjecting the essentially residue-free ammoniacal leach liquor obtained from the oxidative pressure leach after separation of leach liquor from leach residue to a secondary oxidative pressure treatment at elevated temperature and elevated pressure of an oxygen-bearing gas with an ammonia to metals mole ratio effective to produce a leach liquor whereby the formation of cobalt (III) hexammine sulphate therein has been increased.

### Claim 7 (depends on 6)

The process as set forth in claim 6 wherein the temperature in said secondary oxidative pressure treatment ranges between 110 to 150° C.

### Claim 8 (depends on 6)

The process as set forth in claim 6 wherein the concentration of titratable ammonia in said secondary oxidative pressure treatment ranges between 120 to 200 g/L.

### Claim 9 (depends on 6)

The process as set forth in claim 6 wherein the concentration of titratable ammonia ranges between 120 and 200 g/L and the temperature ranges between 110 to 150° C. in said secondary oxidative pressure treatment.

### Claim 10 (depends on 9)

The process as set forth in claim 9 wherein the nickel enriched leach liquor from the primary oxidative leach step is subjected to a polish filtration.