# US 2003/0222379 A1 · Method of manufacturing metal clad laminate for printed circuit board

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0222379 A1
- Document ID: US20030222379A1
- Status: Published application
- Kind: A1
- Application number: 10/375,915
- Filed: 2003-02-21
- Published: 2003-12-04
- Earliest claimed: 2002-02-25
- Inventors: Eun Song Baik; Jong Seok Song; Rae Ook Cho; Yu Cheol Yang
- Web page: https://patentgrep.com/patent/US20030222379A1

## CPC

- H05K 3/381: {by special treatment of the substrate}
- B32B 15/08: of synthetic resin
- B32B 37/04: characterised by the partial melting of at least one layer
- B32B 38/0012: {Mechanical treatment, e.g. roughening, deforming, stretching}
- B32B 37/08: characterised by the cooling method
- B32B 2037/0092: {in which absence of adhesives is explicitly presented as an advantage}
- B32B 2038/0016: {Abrading}
- B32B 2311/00: Metals, their alloys or their compounds
- B32B 2327/12: containing fluorine
- B32B 2457/08: PCBs, i.e. printed circuit boards
- H05K 1/034: {containing halogen}
- H05K 3/382: {by special treatment of the metal}
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

The present invention relates to a method of manufacturing a metal clad laminate for printed circuit board, characterized by direct adhesion of a conductive metal foil without use of a thermosetting resin having low melting points, an adherent film or an adhesive. The method includes forming fine protrusions on at least one surface of a fluorine-based resin insulation layer, roughening one surface of a conductive metal foil, laminating the fluorine-based resin insulation layer having fine protrusions on the roughened metal foil so that the roughened surface of the metal foil and the protrusion-formed surface of the insulation layer face each other to form a laminated body, and compressing the laminated body under vacuum, pressure and heat. The method of manufacturing the metal clad laminate by directly adhering the conductive metal foil with a single dielectric structure has advantages in terms of lower manufacturing costs compared to conventional dual dielectric structures, and very stable operation of the metal clad laminate in high frequency regions due to minimized variations of electrical and mechanical properties. Thus, the present method is effective in manufacturing the printed circuit board usable in the high frequency regions.

## Claims

### Claim 1

A method of manufacturing a metal clad laminate for printed circuit boards, comprising:
(a) forming fine protrusions on at least one surface of a fluorine-based resin insulation layer;
(b) roughening one surface of a conductive metal foil;
(c) laminating the fluorine-based resin insulation layer having fine protrusions on the roughened metal foil so that the roughened surface of the metal foil and the protrusion-formed surface of the insulation layer face each other, to form a laminated body; and
(d) compressing the laminated body under vacuum, pressure and heat.

### Claim 2 (depends on 1)

The method as defined in claim 1, further comprising sequentially laminating, on a surface of the fluorine-based resin insulation layer not having fine protrusions in the laminated body before the (d) operation is performed, at least one fluorine-based resin insulation layer not subjected to the (a) operation, a second fluorine-based resin insulation layer subjected to the (a) operation, and a second conductive metal foil subjected to the (b) operation, wherein the roughened surface of the second metal foil subjected to the (b) operation and the protrusion-formed surface of the second insulation layer subjected to the (a) operation face each other.

### Claim 3 (depends on 1, 2)

The method as defined in claim 1 or 2, wherein the fine protrusions formed on the insulation layer have an average diameter of 0.01-2 μm and an average aspect ratio of 1:20 or less.

### Claim 4 (depends on 1, 2)

The method as defined in claim 1 or 2, wherein the fluorine-based resin is all fluorine resins containing fluorine, comprising polytetrafluoroethylene, polytetrafluoroethylene-impregnated glass cloth, polychlorotrifluoroethylene, tetrafluoroethylene-hexafluoropropylene copolymer, polyvinylidene fluoride, polyvinyl fluoride, ethylenetetrafluoroethylene, perfluoroalkoxy, chlorotrifluoroethylene, and ethylenechlorotrifluoroethylene.

### Claim 5 (depends on 1, 2)

The method as defined in claim 1 or 2, wherein at least two of the insulation layers each having a thickness of 0.05-0.508 mm are laminated so that the metal clad laminate has a thickness of 0.127-5.08 mm.

### Claim 6 (depends on 1, 2)

The method as defined in claim 1 or 2, wherein the conductive metal foil is made of copper, aluminum or alloys thereof.

### Claim 7 (depends on 1, 2)

The method as defined in claim 1 or 2, wherein the (d) operation is performed under conditions of a maximal temperature of a hot press ranging from a glass transition temperature of the fluorine-based resin to a temperature 20% higher than a melting point of the fluorine-based resin, a hot press pressure of 10-90 kg/cm2 and a vacuum level ranging from 1 mTorr to 500 Torr, within 3 hours.