# US 2003/0222287 A1 · Hard mask etch for gate polyetch

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0222287 A1
- Document ID: US20030222287A1
- Status: Published application
- Kind: A1
- Application number: 10/157,192
- Filed: 2002-05-30
- Published: 2003-12-04
- Earliest claimed: 2002-05-30
- Assignees: Sharp Kabushiki Kaisha
- Inventors: Koji Tamura
- Web page: https://patentgrep.com/patent/US20030222287A1

## CPC

- H10P 50/71: {using masks for conductive or resistive materials}
- H10P 50/268: {of silicon-containing layers}
- H10P 50/283: {by chemical means}
- H10D 64/01306: {the conductor comprising a layer of silicon contacting the insulator, e.g. polysilicon}
- Y10S 438/952: Utilizing antireflective layer
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A transistor gate structure that is free from notches is formed by using a hard mask. The hard mask has a bilayer structure of a BARC (bottom antireflective coating) over a silicon dioxide layer. A photoresist layer is formed over a portion corresponding to the gates. A first etch forms the gate structure. Following removal of the photoresist, a second etch completely removes the BARC. The silicon dioxide layer can be removed by a subsequent wet etch with HF.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, which comprises:
providing a substrate;
forming an oxide layer over the substrate;
forming a silicon layer over the oxide layer;
forming a hard mask over the silicon layer;
forming a layer of photoresist over a portion of the silicon layer corresponding to a gate;
performing a first etching;
removing the photoresist; and
performing a second etching.

### Claim 2 (depends on 1)

The method of claim 1, wherein the hard mask comprises a layer of antireflective coating over a layer of silicon oxide.

### Claim 3 (depends on 2)

The method of claim 2, wherein the antireflective coating comprises silicon oxynitride.

### Claim 4 (depends on 2)

The method of claim 2, wherein the second etching removes the antireflective coating.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first etching is a dry etch.

### Claim 6 (depends on 1)

The method of claim 1, wherein the second etching is a dry etch.

### Claim 7 (depends on 1)

The method of claim 1, wherein no notch is formed in the gate.

### Claim 8 (depends on 1)

The method of claim 1, wherein the gate undercut is less than about 50 Å.

### Claim 9 (depends on 1)

The method of claim 1, wherein the substrate comprises silicon and the oxide layer over the substrate comprises silicon oxide.

### Claim 10 (depends on 1)

The method of claim 1, wherein the silicon layer comprises non-doped or n-doped poly-Si.

### Claim 11 (depends on 1)

The method of claim 1, wherein the silicon layer has a thickness of about 2000 Å.

### Claim 12 (depends on 1)

The method of claim 1, wherein the photoresist is a 248 nm photoresist.

### Claim 13 (depends on 2)

The method of claim 2, wherein the layer of silicon oxide has a thickness of about 300-700 Å.

### Claim 14 (depends on 2)

The method of claim 2, wherein the antireflective coating has a thickness of about 300-700 Å.

### Claim 15

A semiconductor device that comprises:
a substrate;
an oxide layer over the substrate; and
a silicon layer over the oxide layer, the silicon layer forming a notch-free gate structure,
wherein the gate structure has been formed using a hard mask comprising an antireflective layer over a silicon oxide layer, the mask having been subsequently removed.

### Claim 16 (depends on 15)

The semiconductor device of claim 15, wherein the antireflective layer comprises silicon oxynitride.

### Claim 17 (depends on 15)

The method of claim 15, wherein the silicon oxide layer has a thickness of about 300-700 Å.

### Claim 18 (depends on 15)

The method of claim 15, wherein the antireflective coating has a thickness of about 300-700 Å.

### Claim 19 (depends on 15)

The method of claim 15, wherein the silicon layer comprises non-doped or n-doped poly-Si.

### Claim 20 (depends on 15)

The method of claim 15, wherein the silicon layer has a thickness of about 2000 Å.