# US 2003/0216240 A1 · Dielectric ceramic

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0216240 A1
- Document ID: US20030216240A1
- Status: Published application
- Kind: A1
- Application number: 10/354,074
- Filed: 2003-01-30
- Published: 2003-11-20
- Earliest claimed: 2002-05-20
- Assignees: Ngk Spark Plug Co., Ltd.
- Inventors: Eiji Kodera; Kazuyuki Fujii; Makoto Baba; Hidetoshi Mizutani; Manabu Sato
- Web page: https://patentgrep.com/patent/US20030216240A1

## CPC

- C03C 8/14: Glass frit mixtures having non-frit additions, e.g. opacifiers, colorants, mill-additions
- C03C 8/04: containing zinc
- H05K 1/0306: {Inorganic insulating substrates, e.g. ceramic, glass}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

The invention is to offer such a dielectric ceramic enabling to simultaneously sinter with the low resistant conductor of Ag based metals and Cu based metals, having the excellent mechanical strength and exhibiting the excellent dielectric characteristics in the GHz zone. Mixed powders of Si: 20 to 30 weight %, B: 5 to 30 weight %, Al: 20 to 30 weight %, Ca: 10 to 20 weight %, and Zn: 10 to 20 weight % are prepared, melted, and rapidly cooled to produce glass frits. The glass frits are granulated and mixed with gahnite filler and titania filler which are inorganic filler powders. Subsequently, a binder is thrown into the powders to produce a composition of dielectric ceramic, and then is formed, followed by sintering. The mixed powders may contain at least one kind of alkali metal of Li, K and Na.

## Claims

### Claim 1

A dielectric ceramic comprising an inorganic filler and glass,
wherein when the total amount of the inorganic filler and the glass is 100 weight %, the amount of the inorganic filler is 20 to 60 weight % and the amount of the glass is 40 to80 weight %; and when the total amount of the glass is 100 weight %, the glass contains, each in terms of oxide, Si in amount of 20 to 30 weight %, B in an amount of 5 to 30 weight %, Al in an amount of 20 to 30 weight %, Ca in an amount of 10 to 20 weight %, Zn in amount of 10 to 20 weight %, and at least one alkali metal selected from Li, Na and K in a total amount of 0.2 to 5 weight %.

### Claim 2 (depends on 1)

The dielectric ceramic according to claim 1, wherein the inorganic filler comprises a gahnite filler and a titania filler.

### Claim 3 (depends on 1)

The dielectric ceramic according to claim 1, which has a dielectric loss in 3 GHz of 50×10−4 or less.

### Claim 4 (depends on 1)

The dielectric ceramic according to claim 1, which has a relative dielectric constant in 3 GHz of 6 to 13.

### Claim 5 (depends on 1)

The dielectric ceramic according to claim 1, which has a coefficient of thermal expansion at 25 to 400° C. of 5 to 10 ppm/° C.

### Claim 6 (depends on 1)

The dielectric ceramic according to claim 1, which has a bending strength is 185 MPa or more.

### Claim 7

A dielectric ceramic comprising an inorganic filler and glass,
wherein when the total amount of the inorganic filler and the glass is 100 weight %, the amount of the inorganic filler is 20 to 60weight % and the amount of the glass is 40 to 80 weight %; when the total amount of the glass is 100 weight %, the glass contains, each in terms of oxide, Si in amount of 20 to 30 weight %, B in an amount of 5 to 30 weight %, Al in an amount of 20 to 30 weight %, Ca in an amount of 10 to 20 weight %, and Zn in amount of 10 to 20 weight %; and the glass does not contain any of Li, Na and K.

### Claim 8 (depends on 7)

The dielectric ceramic according to claim 7, wherein the inorganic filler comprises a gahnite filler and a titania filler.

### Claim 9 (depends on 7)

The dielectric ceramic according to claim 7, which has a dielectric loss in 3 GHz of 50×10−4 or less.

### Claim 10 (depends on 7)

The dielectric ceramic according to claim 7, which has a relative dielectric constant in 3 GHz of 6 to 13.

### Claim 11 (depends on 7)

The dielectric ceramic according to claim 7, which has a coefficient of thermal expansion at 25 to 400° C. of 5 to 10 ppm/° C.

### Claim 12 (depends on 7)

The dielectric ceramic according to claim 7, which has a bending strength of 185 MPa or more.

### Claim 13

A dielectric ceramic made by sintering at 1000° C. or lower a dielectric ceramic composition comprising an inorganic filler and glass,
wherein when the total amount of the inorganic filler and the glass is 100 weight %, the amount of the inorganic filler is 20to 60weight % and the amount of the glass is 40 to80 weight %; and when the total amount of the glass is 100 weight %, the glass contains, each in terms of oxide, Si in amount of 20 to 30 weight %, B in an amount of 5 to 30 weight %, Al in an amount of 20 to 30 weight %, Ca in an amount of 10 to 20 weight %, Zn in amount of 10 to 20 weight %, and at least one alkali metal selected from Li, Na and K in a total amount of 0.2 to 5 weight %.

### Claim 14 (depends on 13)

The dielectric ceramic according to claim 13, wherein the inorganic filler comprises a gahnite filler and a titania filler.

### Claim 15 (depends on 13)

The dielectric ceramic according to claim 13, wherein a glass transition point Tg is 560 to 670° C.

### Claim 16 (depends on 13)

The dielectric ceramic according to claim 13, which has a difference in temperature between a glass transition point Tg and a bending point Mg is 30 to 45° C.

### Claim 17 (depends on 13)

The dielectric ceramic according to claim 13, which has a dielectric loss in 3 GHz of 50×10−4 or less.

### Claim 18 (depends on 13)

The dielectric ceramic according to claim 13, which has a relative dielectric constant in 3 GHz of 6 to 13.

### Claim 19 (depends on 13)

The dielectric ceramic according to claim 13, which has a coefficient of thermal expansion at 25 to 400° C. of 5 to 10 ppm/° C.

### Claim 20 (depends on 13)

The dielectric ceramic according to claim 13, which has a bending strength of 185 MPa or more.

### Claim 21 (depends on 15)

The dielectric ceramic according to claim 15, wherein the inorganic filler comprises a gahnite filler and a titania filler.

### Claim 22 (depends on 15)

The dielectric ceramic according to claim 15, which has a glass transition point Tg of 560 to 670° C.

### Claim 23 (depends on 15)

The dielectric ceramic according to claim 15, which has a difference between a glass transition point Tg and a bending point Mg is 30 to 45° C.

### Claim 24 (depends on 15)

The dielectric ceramic according to claim 15, which has a dielectric loss in 3 GHz of 50×10−4 or less.

### Claim 25 (depends on 15)

The dielectric ceramic according to claim 15, which has a relative dielectric constant in 3 GHz of 6 to 13.

### Claim 26 (depends on 15)

The dielectric ceramic according to claim 15, which has a coefficient of thermal expansion at 25 to 400° C. of 5 to 10 ppm/° C.

### Claim 27 (depends on 13)

The dielectric ceramic according to claim 13, which has a bending strength of 185 MPa or more.

### Claim 28

A dielectric ceramic made by sintering at 1000° C. or lower a dielectric ceramic composition comprising an inorganic filler and glass,
wherein when the total amount of the inorganic filler and the glass is 100 weight %, the amount of the inorganic filler is 20 to 60 weight % and the amount of the glass is 40 to 80 weight %; when the total amount of the glass is 100 weight %, the glass contains, each in terms of oxide, Si in amount of 20 to 30 weight %, B in an amount of 5 to 30 weight %, Al in an amount of 20 to 30 weight %, Ca in an amount of 10 to 20 weight %, and Zn in amount of 10 to 20 weight %; and the glass does not contain any of Li, Na and K.

### Claim 29 (depends on 28)

The dielectric ceramic according to claim 28, wherein the inorganic filler comprises a gahnite filler and a titania filler.

### Claim 30 (depends on 28)

The dielectric ceramic according to claim 28, which has a glass transition point Tg of 560 to 670° C.

### Claim 31 (depends on 28)

The dielectric ceramic according to claim 28, which has a difference in temperature between a glass transition point Tg and a bending point Mg is 30 to 45° C.

### Claim 32 (depends on 28)

The dielectric ceramic according to claim 28, which has a dielectric loss in 3 GHz of 50×10−4 or less.

### Claim 33 (depends on 28)

The dielectric ceramic according to claim 28, which has a relative dielectric constant in 3 GHz of 6 to 13.

### Claim 34 (depends on 28)

The dielectric ceramic according to claim 28, which has a coefficient of thermal expansion at 25 to 400° C. of 5 to 10 ppm/° C.

### Claim 35 (depends on 28)

The dielectric ceramic according to claim 28, which has a bending strength of 185 MPa or more.

### Claim 36 (depends on 30)

The dielectric ceramic according to claim 30, wherein the inorganic filler comprises a gahnite filler and a titania filler.

### Claim 37 (depends on 30)

The dielectric ceramic according to claim 30, which has a difference in temperature between the glass transition point Tg and a bending point Mg of 30 to 45° C.

### Claim 38 (depends on 30)

The dielectric ceramic according to claim 30, which has a dielectric loss in 3 GHz of 50×10−4 or less.

### Claim 39 (depends on 30)

The dielectric ceramic according to claim 30, which has a relative dielectric constant in 3 GHz of 6 to 13.

### Claim 40 (depends on 30)

The dielectric ceramic according to claim 30, which has a coefficient of thermal expansion at 25 to 400° C. of 5 to 10 ppm/° C.

### Claim 41 (depends on 30)

The dielectric ceramic according to claim 30, which has a bending strength of 185 MPa or more.