# US 2003/0216042 A1 · CMP slurry for oxide film and method of forming semiconductor device using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0216042 A1
- Document ID: US20030216042A1
- Status: Published application
- Kind: A1
- Application number: 10/331,359
- Filed: 2002-12-30
- Published: 2003-11-20
- Earliest claimed: 2002-05-17
- Inventors: Sang Ick Lee; Hyung Hwan Kim
- Web page: https://patentgrep.com/patent/US20030216042A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- H10P 95/062: {involving a dielectric removal step}
- H10W 20/092: {by smoothing the dielectric parts}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A chemical mechanical polishing(abbreviated as “CMP”) slurry composition for oxide films, and a method of forming a self-aligned floating gate of a flash memory device are disclosed for performing a CMP process using slurry having higher polishing selectivity to an oxide film than to a nitride film which is an etching barrier film.

## Claims

### Claim 1

A CMP slurry composition for an oxide film comprising a solvent, an abrasive and an additive, the additive selected from the group consisting of:
a homo-polymer of hydrocarbon compound including carboxylic acid(—COOH) group, a homo-polymer of hydrocarbon compound including nitro(—NO2) group and a homo-polymer of hydrocarbon compound including amide(—NH—CO—) group; a copolymer of hydrocarbon compound including carboxylic acid(—COOH) group, a copolymer of hydrocarbon compound including nitro(—NO2) group and a copolymer of hydrocarbon compound including amide(—NH—CO—) group; and mixtures thereof,
wherein the composition has a pH ranging from 2 to 7.

### Claim 2 (depends on 1)

The CMP slurry composition according to claim 1, wherein the pH of the composition ranges from pH 4 to 7.

### Claim 3 (depends on 1)

The CMP slurry composition according to claim 1, further comprising hydrochloric acid as a pH adjusting agent.

### Claim 4 (depends on 1)

The CMP slurry composition according to claim 1, wherein the additive is selected from the group consisting of alpha-cellulose, carboxymethylcellulose sodium salt, methyl vinyl ether, poly(acrylic acid), poly(ethylene glycol), poly-galacturonic acid and combinations thereof.

### Claim 5 (depends on 1)

The CMP slurry composition according to claim 1, wherein the additive is present in amount ranging from 0.1 to 1.5 weight parts based on 100 weight parts of the solvent.

### Claim 6 (depends on 1)

The CMP slurry composition according to claim 1, wherein the abrasive is Ceria(CeO2) or silica(SiO2).

### Claim 7 (depends on 6)

The CMP slurry composition according to claim 6, wherein the CeO2 is present in amount ranging from 0.5 to 2 weight parts based on 100 weight parts of the solvent.

### Claim 8 (depends on 6)

The CMP slurry composition according to claim 6, wherein the SiO2 is present in amount ranging from 10 to 33 weight parts based on 100 weight parts of the solvent.

### Claim 9 (depends on 1)

The CMP slurry composition according to claim 1, wherein a polishing selectivity ratio of the slurry composition for nitride film:oxide film is 1:20˜1:200.

### Claim 10 (depends on 1)

The CMP slurry composition according to claim 1, wherein a polishing selectivity ratio of the slurry composition for nitride film:oxide film is 1:50˜1:200.

### Claim 11 (depends on 1)

A method of forming a semiconductor device, comprising:
(a) forming a pad oxide film and a pad nitride film on a substrate;
(b) selectively patterning the pad nitride film, the pad oxide film and the substrate to form a trench of a predetermined depth;
(c) depositing an isolation oxide film on the patterned pad nitride film, the pad oxide film and substrate; and
(d) performing a CMP process onto the resultant structure using the CMP slurry composition of claim 1 until the pad nitride film is exposed.

### Claim 12 (depends on 1, 11)

The method according to claim 11, wherein the (d) step comprises:
a first step of performing a CMP process using a slurry for an oxide film of which a polishing selectivity ratio for nitride film:oxide film is 1:2˜1:4 until a predetermined thickness of the isolation oxide film remains; and
a second step of performing a CMP process using a slurry of claim 1 until the pad nitride film is exposed.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the first step is performed until the thickness isolation oxide film on the pad nitride film ranges from 1 to 50% relative to the thickness before the CMP process.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the slurry for an oxide film comprises an abrasive of SiO2 and has a pH ranging from 7 to 8.