# US 2003/0216036 A1 · Method of reducing plasma charging damage during dielectric etch process for dual damascene interconnect structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0216036 A1
- Document ID: US20030216036A1
- Status: Published application
- Kind: A1
- Application number: 10/456,190
- Filed: 2003-06-05
- Published: 2003-11-20
- Earliest claimed: 2001-12-07
- Inventors: Shawming Ma
- Web page: https://patentgrep.com/patent/US20030216036A1

## CPC

- H10W 20/033: {in openings in dielectrics}
- H10W 20/034: {bottomless barrier, adhesion or liner layers}
- H10W 20/076: {in via holes or trenches}
- H10W 20/085: {involving intermediate temporary filling with material}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Charging damage, caused by electron shading during plasma etching in a dual damascene structure, is alleviated by first depositing a protective conductive layer which provides a conductive path for maintaining charge balance in the etched structures. This conductive layer reduces the buildup of unbalanced positive charge in the contact opening, and the damage done to underlying layers caused by the resultant tunneling current. Further, if the protective conductive layer comprises a material which can also serve as an interdiffusion barrier layer for the contact opening fill material, a separate subsequent step to deposit such a barrier layer on the contact opening sidewall is avoided. Further, in the process of doing lithography on the trench etch resist layer, the protective conductive layer also functions as an antireflective coating, permitting the stepper to accurately focus the desired pattern.

## Claims

### Claim at position 1

1 A method of reducing plasma-induced charging damage during etching of a trench in a dielectric layer which forms part of a dual damascene semiconductor structure, the method comprising:
(a) providing a semiconductor structure including an electrical contact opening through a dielectric layer overlying an etch barrier layer, which barrier layer overlies a conductive region in said semiconductor structure;
(b) applying a protective layer of a conductive material over surfaces of said electrical contact opening and over adjacent exposed horizontal surfaces;
(c) applying a layer of photoresist material over said adjacent exposed horizontal surfaces;
(d) patterning said layer of photoresist material; and
(e) etching a trench overlying said electrical contact opening and through a portion of said adjacent exposed horizontal surfaces, wherein charging damage to said semiconductor structure which occurs during etching is reduced by the presence of said protective layer of conductive material.

### Claim 2 (depends on 1)

The method of claim 1, wherein said protective conductive layer deposited in step b comprises a material capable of functioning as a diffusion barrier layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein said protective conductive layer deposited in step b comprises a material capable of functioning as an antireflective coating.

### Claim 4 (depends on 1)

The method of claim 1, wherein said dielectric layer comprises a low-k dielectric material exhibiting a relative dielectric permitivity less of than about 3.9.

### Claim 5 (depends on 1)

The method of claim 1, wherein said protective conductive layer comprises a metal, or a conductive metal nitride, or a conductive metal oxide, or a combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein said protective conductive layer is formed from a material selected from the group consisting of Al, Pt, Rh, Ag, Ti, TiN, Ta, TaN, W, WN, Ir, IrOx, Ru, RuOx, and alloys and combinations thereof.

### Claim 7 (depends on 2)

The method of claim 2, wherein said protective conductive layer is formed from a material selected from the group consisting of Ti, TiN, Ta, TaN, W, WN, and combinations thereof.

### Claim 8 (depends on 7)

The method of claim 7, wherein said protective conductive layer comprises Ti, TiN, or combinations thereof.

### Claim 9 (depends on 7)

The method of claim 7, wherein said protective conductive layer comprises Ta, TaN, or combinations thereof.

### Claim 10 (depends on 7)

The method of claim 7, wherein said protective conductive layer comprises W, WN, or combinations thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein said protective conductive layer is selected from the group consisting of Al, Pt, Ir, Ru, Rh, Ag, Ti, Ta, W, and alloys and combinations thereof.

### Claim 12 (depends on 11)

The method of claim 11, wherein said protective conductive layer is Al and non-diffusing alloys thereof.

### Claim 13

A method of reducing plasma-induced charging damage in a dielectric trench etch process for a dual damascene semiconductor structure, said method comprising the following steps, in the order stated:
(a) providing a semiconductor structure comprising from bottom to top
(1) a semiconductor substrate
(2) a conductor embedded in said substrate, having an upper portion of said conductor contacted at its sidewall by a layer of dielectric hardmask, an upper surface of said conductor and an upper surface of said hardmask layer being covered by an etch stop layer,
(3) a layer of a first dielectric material overlying said etch stop layer,
(4) a second dielectric hardmask layer overlying said layer of said second dielectric material,
(5) a contact opening etched downward from a top surface of said second dielectric hardmask layer, through said second dielectric layer, said contact opening comprising a sidewall extending downward through said second dielectric hardmask layer and said second dielectric layer, and ending at a floor of said contact opening at said etch stop layer;
(b) depositing upon an exposed upper surface of said second dielectric hardmask layer, and upon said sidewall of said contact opening, and upon said floor of said contact opening, a continuous layer of a protective conductive material;
(c) applying a layer of photoresist material;
(d) patterning said layer of photoresist material in a manner defining the location for plasma etching of a trench in an upper surface of said second dielectric hardmask layer, immediately over and communicating with said contact opening;
(e) anisotropically plasma etching said trench downward and through said second dielectric hardmask layer, and downward into, but not through, said second dielectric layer, to a nominal trench depth;
(f) removing said photoresist layer which remains following said etching of said trench;
(g) anisotropically plasma etching away said protective conductive layer, if any, which remains upon said second dielectric hardmask layer or upon said floor of said contact opening, and that portion of said etch stop layer which is exposed beneath said floor of said contact opening, but not said protective conductive layer which remains upon said sidewall of said contact opening; and
(h) anisotropically plasma etching away any of said etch stop layer material remaining on the floor of said contact opening after completion of step (g), thereby exposing a surface of said conductor beneath said floor of said contact opening.

### Claim 14 (depends on 13)

The method of claim 13, wherein said protective conductive layer deposited in step b comprises a material capable of functioning as a diffusion barrier layer.

### Claim 15 (depends on 13)

The method of claim 13, wherein said protective conductive layer deposited in step b comprises a material capable of functioning as an antireflective coating.

### Claim 16 (depends on 13)

The method of claim 13, wherein said dielectric layer comprises a low-k dielectric material exhibiting a relative dielectric permitivity less of than about 3.9.

### Claim 17 (depends on 13)

The method of claim 13, wherein said protective conductive layer comprises a metal, or a conductive metal nitride, or a conductive metal oxide, or a combination thereof.

### Claim 18 (depends on 13)

The method of claim 13, wherein said protective conductive layer is formed from a material selected from the group consisting of Al, Pt, Rh, Ag, Ti, TiN, Ta, TaN, W, WN, Ir, IrOx, Ru, RuOx, and alloys and combinations thereof.

### Claim 19 (depends on 14)

The method of claim 14, wherein said protective conductive layer is formed from a material selected from the group consisting of Ti, TiN, Ta, TaN, W, WN, and combinations thereof.

### Claim 20 (depends on 19)

The method of claim 19, wherein said protective conductive layer comprises Ti, TiN, or combinations thereof.

### Claim 21 (depends on 19)

The method of claim 19, wherein said protective conductive layer comprises Ta, TaN, or combinations thereof.

### Claim 22 (depends on 19)

The method of claim 19, wherein said protective conductive layer comprises W, WN, or combinations thereof.

### Claim 23 (depends on 13)

The method of claim 13, wherein said protective conductive layer is selected from the group consisting of Al, Pt, Ir, Ru, Rh, Ag, Ti, Ta, W, and alloys and combinations thereof.

### Claim 24 (depends on 23)

The method of claim 23, wherein said protective conductive layer is Al and non-diffusing alloys thereof.