# US 2003/0216028 A1 · Hydrogen barrier layer and method for fabricating semiconductor device having the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0216028 A1
- Document ID: US20030216028A1
- Status: Published application
- Kind: A1
- Application number: 10/330,129
- Filed: 2002-12-30
- Published: 2003-11-20
- Earliest claimed: 2002-05-18
- Assignees: Hynix Semiconductor Inc.
- Inventors: Dong-Soo Yoon
- Web page: https://patentgrep.com/patent/US20030216028A1

## CPC

- H10D 1/688: {comprising barrier layers to prevent diffusion of hydrogen or oxygen}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention provides a hydrogen barrier layer able to prevent diffusions of hydrogen into a capacitor and a method for fabricating a semiconductor device having the same. The inventive method includes the steps of: forming a capacitor on an upper portion of a substrate providing a transistor; forming a first hydrogen barrier layer covering the capacitor, the first hydrogen barrier layer containing Al and Ti; forming a metal line connecting the capacitor to the transistor; forming a second hydrogen barrier layer containing Al and Ti on the metal line; and forming a protection layer on the second hydrogen barrier layer.

## Claims

### Claim 1

A semiconductor device comprising a hydrogen barrier layer for preventing hydrogen from diffusing into a capacitor, wherein the hydrogen barrier layer includes titanium (Ti) and oxygen (O2) to aluminum (Al).

### Claim 2 (depends on 1)

The semiconductor device as recited in claim 1, wherein the a hydrogen barrier layer prevents hydrogen from diffusing into a capacitor in processes for forming an insulating layer or a protection layer over the capacitor.

### Claim 3 (depends on 1)

The semiconductor device as recited in claim 1, wherein the complex oxide material has a compositional ratio of Al ranging from about 50 at % to about 90 at %, a compositional ratio of Ti ranging from about 10 at % to about 50 at % and a compositional ratio of O2 ranging from about 1 at % to about 80 at %.

### Claim 4

A method for forming a hydrogen barrier layer, comprising the steps of:
loading a substrate to a deposition chamber; and
supplying Al and Ti sources and a reaction gas to the deposition chamber so to deposit a complex oxide material includes Ti and O2 to Al on the substrate.

### Claim 5 (depends on 4)

The method as recited in claim 4, wherein the Al source is AlX3, where X is any one substrate selected from a group consisting of H, alkyl having about 1 to 10 carbon branches, alkenyl having about 2 to 10 carbon branches, alkoxy having about 1 to 8 carbon branches, aryl having about 6 to 12 carbon branches, β-diketonates, cyclopentadienyl, alkylcyclopentadienyl having about 1 to 8 carbon branches and derivatives of the above listed substrates added with one of halogen elements.

### Claim 6 (depends on 4)

The method as recited in claim 4, wherein the Ti source is either TiX4 or TiX2, where X is any one substrate selected from a group consisting of H, alkyl having about 1 to 10 carbon branches, alkenyl having about 2 to 10 carbon branches, alkoxy having about 1 to 8 carbon branches, aryl having about 6 to 12 carbon branches, β-diketonates, cyclopentadienyl, alkylcyclopentadienyl having about 1 to 8 carbon branches and derivatives of the above listed substrates added with one of halogen elements.

### Claim 7 (depends on 4)

The method as recited in claim 4, wherein the reaction gas uses such gas as O2, N2O, NH3, H2O, H2O2, ROH, RCOOH, diol having about 2 to 10 carbon branches or a mixed gas of the above gases, and the R is any one substrate selected from a group consisting of H, alkyl having about 1 to 10 carbon branches, alkenyl having about 2 to 10 carbon branches, alkoxy having about 1 to 8 carbon branches, aryl having about 6 to 12 carbon braches and derivatives of the above listed substrates added with one of halogen elements.

### Claim 8 (depends on 4)

The method as recited in claim 4, wherein the complex oxide material is formed to a thickness ranging from about 200 Å to about 1000 Å at a temperature ranging from about 100° C. to about 900° C.

### Claim 9

A method for fabricating a semiconductor device having a hydrogen barrier layer, comprising the steps of:
forming a capacitor on a substrate including a transistor; and
forming a first hydrogen barrier layer covering the capacitor, the first hydrogen barrier layer containing Al and Ti.

### Claim 10 (depends on 9)

The method as recited in claim 9, wherein the step of forming the hydrogen barrier layer employs either an atomic layer deposition (ALD) technique or a chemical vapor deposition (CVD) technique.

### Claim 11 (depends on 9)

the method as recited in claim 9, after forming the first hydrogen barrier layer, further comprising the steps of:
forming a metal line connecting the capacitor to the transistor;
forming a second hydrogen barrier layer containing Al and Ti on the metal line; and
forming a protection layer on the second hydrogen barrier layer.