# US 2003/0215756 A1 · Photothermographic material and image forming method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0215756 A1
- Document ID: US20030215756A1
- Status: Published application
- Kind: A1
- Application number: 10/336,920
- Filed: 2002-12-27
- Published: 2003-11-20
- Earliest claimed: 2002-01-08
- Assignees: Konica Corporation
- Inventors: Kiyokazu Morita; Narito Goto; Ayumu Nishijima
- Web page: https://patentgrep.com/patent/US20030215756A1

## CPC

- G03C 1/49827: {Reducing agents}
- G03C 1/49845: {Active additives, e.g. toners, stabilisers, sensitisers}
- G03C 1/49881: {characterised by the process or the apparatus}
- G03C 1/04: with macromolecular additives; with layer-forming substances
- G03C 1/061: {Hydrazine compounds}
- G03C 1/07: Substances influencing grain growth during silver salt formation
- G03C 1/46: having more than one photosensitive layer {(G03F7/0952 takes precedence)}
- G03C 1/49818: {Silver halides}
- G03C 1/49863: {Inert additives, e.g. surfactants, binders}
- G03C 2001/03564: {Mixed grains or mixture of emulsions}
- G03C 2001/03594: {Size of the grains}
- G03C 2007/3025: {Silver content}
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

A photothermographic material comprising a support and having thereon an image forming layer containing an organic silver salt, light-sensitive silver halide grains, binder and a reducing agent, wherein the reducing agent comprises: a reducing agent A containing at least a bisphenol derivative represented by following Formula (A-1); and a reducing agent B containing at least a bisphenol derivative not represented by the Formula (A-1), and the amount of reducing agent A is 5 to 45 weight % of the total weight of the reducing agent A and reducing agent B. 1

## Claims

### Claim 1

A photothermographic material comprising a support and having thereon an image forming layer containing an organic silver salt, light-sensitive silver halide grains, binder and a reducing agent,
wherein the reducing agent comprises:
a reducing agent A containing at least a bisphenol derivative represented by following Formula (A-1); and
a reducing agent B containing at least a bisphenol derivative not represented by the General Formula (A-1), and the amount of reducing agent A is 5 to 45 weight % of the total weight of the reducing agent A and reducing agent B,
85
wherein each of R1 is alkyl group, and at least one of them is a secondary or tertiary alkyl group; each of R2 is a hydrogen atom or a group capable of substituted on a benzen ring; Q0 is a group capable of being substituted on a benzen ring; n and m are each an integer of 0 to 2; plural R1s, R2s or Q0s may be the same or different from each other; and X is a chalcogen atom or CHR, in which R is a hydrogen atom, a halogen atom or an alkyl group.

### Claim 2 (depends on 1)

The photothermographic material of claim 1, wherein the bisphenol derivative in the reducing agent B is represented by following Formula A-2,
86
wherein Z is an atom group necessary to form a 3- to 10-membered non-aromatic ring together with a carbon atom; Rx is a hydrogen atom or an alkyl group; R3 and R4 are a hydrogen atom, an alkyl group, an aryl group or a heterocyclic group; Q0 is a group capable of being substituted on a benzen ring; n and m are each an integer of 0 to 2; and plural R3s, R4s or Q0s may be the same or different from each other.

### Claim 3 (depends on 2)

The photothermographic material of claim 2, wherein the non-aromatic ring formed by z in Formula (A-2) is a 6-membered non-aromatic ring.

### Claim 4 (depends on 1)

The photothermographic material of claim 1, wherein the bisphenol derivative in the reducing agent B is represented by following Formula (A-3),
87
wherein Q1 is a halogen atom, an alkyl group, an aryl group or a heterocyclic group; Q2 is a hydrogen atom, a halogen atom, an alkyl group, an aryl group or a heterocyclic group; G is a nitrogen atom or a carbon atom; n is 0 when G is a nitrogen atom; n is 0 or 1 when G is a carbon atom; Z2 is an atom group necessary to form a 3- to 10-membered non-aromatic ring together with a carbon atom; Rx is a hydrogen atom or an alkyl group; R3 and R4 are a hydrogen atom, an alkyl group, an aryl group or a heterocyclic group; Q0 is a group capable of being substituted on a benzen ring; n and m are each an integer of 0 to 2; and plural R3s, R4s or Q0s may be the same or different from each other.

### Claim 5 (depends on 4)

The photothermographic material of claim 4, wherein the non-aromatic ring formed by Z2 in Furmula (A-3) is a non-aromatic 6-membered ring.

### Claim 6 (depends on 1)

The photothermographic material of claim 1, wherein the photothermographic material comprises a layer containing at least a silver-saving agent selected from the group consisting of a vinyl compound, a hydrazine derivative and a a quaternary onium salt.

### Claim 7 (depends on 1)

The photothermographic material of claim 1, wherein the average diameter of the silver halide grain is 10 to 35 nm.

### Claim 8 (depends on 1)

The photothermographic material of claim 1, wherein the photothermographic material comprises a silver halide grains having an average diameter of 10 to 35 nm and a silver halide grains having an average diameter of 45 to 100 nm.

### Claim 9 (depends on 1)

The photothermographic material of claim 1, wherein the silver halide grains are chemically sensitized by utilizing a chalcogen compound.

### Claim 10 (depends on 1)

The photothermographic material of claim 1, wherein the silver amount contained in the image forming layer is 0.3 to 1.5 g/m2.

### Claim 11 (depends on 1)

The photothermographic material of claim 1, wherein the photothermographic material further comprises a cross-linking agent containing at least a poly-functional carbodiimide compound.

### Claim 12

A photothermographic material comprising a support and having thereon an image forming layer containing an organic siver salt, light-sensitive silver halide grains, a reducing agent, a binder and a cross-linking agent,
wherein the cross-linking agent contains at least a poly-functional carbodiimide compound.

### Claim 13 (depends on 12)

The photothermographic material of claim 12, wherein the silver amount of the photothermographic material is 0.5 to 1.5 g/m2.

### Claim 14 (depends on 12)

The photothermographic material of claim 12, wherein the image forming layer has a thermal transition point of 46 to 200° C. after the photothermographic material being subjected to developing at a temperature of not less than 100° C.

### Claim 15 (depends on 12)

The photothermographic material of claim 12, wherein the poly-functional carbodiimide compound is a poly-functional aromatic carbodiimide.

### Claim 16 (depends on 12)

The photothermographic material of claim 12, wherein the binder is a compound having a glass transition temperature (Tg) of 70 to 105° C.

### Claim 17 (depends on 12)

The photothermographic material of claim 12, wherein the organic silver salt is grains prepared in the presence of a compound functioning as a crystal growth retarder or a dispersing agent of the grains.

### Claim 18 (depends on 17)

The photothermographic material of claim 17, wherein the compound functioning as a crystal growth retarder or a dispersing agent of the grains is an organic compound having a hydroxyl group or a carboxyl group.

### Claim 19 (depends on 12)

The photothermographic material of claim 12, the poly-functional carbodiimide compound is represented by following
R1—J1—N═C═N—J2—(L)n—(J3—N═C═N—J4—R2)v Formula (CI)
wherein R1 and R2 are each an aryl group or an alkyl group; J1 and J4 are each a bivalent linkage group; J2 and J3 are each an arylene group or an alkylene group; L is an alkyl group, an alkenyl group, an aryl group, or a heterocyclic group which is (v+1)-valent, or a bond; v is an integer of 1 or more; and n is 1 or 2.

### Claim 20 (depends on 12)

The photothermographic material of claim 12, the photothermographic material further comprises a silver-saving agent.

### Claim 21 (depends on 12)

The photothermographic material of claim 12, the photothermographic material comprises plural light-sensitive layers.

### Claim 22 (depends on 1)

An image forming method utilizing a thermal development apparatus comprising a photothermographic material supplying section, an image exposing section, and a thermally developing section, the method comprising the steps of:
transporting the photothermographic material of claim 1 from the photothermographic material supplying section to the image exposing section at transporting rate of 20 to 200 mm/sec;
exposing the photothermographic material to light at the image exposing section while transporting the photothermographic material at transporting rate of 20 to 200 mm/sec; and
thermally developing the photothermographic material at the thermally developing section while transporting the photothermographic material at transporting rate of 20 to 200 mm/sec.