# US 2003/0215713 A1 · Method of manufacturing a sulfated paste for use in a lead acid cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0215713 A1
- Document ID: US20030215713A1
- Status: Published application
- Kind: A1
- Application number: 10/412,926
- Filed: 2003-04-11
- Published: 2003-11-20
- Earliest claimed: 1996-09-20
- Assignees: GP Batteries International Limited
- Inventors: Shawn W. Snyder; Leland M. Gillman
- Web page: https://patentgrep.com/patent/US20030215713A1

## CPC

- H01M 4/20: of pasted electrodes
- H01M 4/56: of lead
- H01M 4/685: {Lead alloys}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/4911: including sealing
- Y10T 29/49115: including coating or impregnating
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An active paste for an lead-acid electrochemical cell which in a preferred embodiment includes tin; a method of manufacturing the same; and an electrochemical cell utilizing the same. The tin may be a tin sulfate, tin oxide, or metallic tin. The active paste sandwiches a primarily lead film which may, but need not, also include tin, to form a positive electrode. One or more positive electrodes are interleafed with a number of negative electrodes, separated by a separator material. The assembly is placed in a container and electrolyte is introduced. In alternate embodiments, the paste may include some combination of antimony, arsenic, germanium, indium, selenium, gallium, tellurium or other semiconductor materials with or without tin compounds.

## Claims

### Claim 1

A method of manufacturing a lead acid electrochemical cell, comprising: preparing a sulfated electrochemically active material to which has been added an oxide of lead, sulfuric acid and a tin-containing compound, said preparation step including introducing the tin-containing compound to the material subsequent to adding the sulfuric acid to the material; coating said electrochemically active material onto a first electrode of a first polarity; arranging said first electrode adjacent to a second electrode of a polarity opposite the first electrodes, the first electrode and second electrode being separated by a separator; and containing said first electrode, second electrode and separator in a container.

### Claim 2 (depends on 1)

The method of claim 1, wherein said tin-containing compound is selected from the group consisting of SnSO4, SnO, metallic tin, a tin(II) salt and a tin(IV) salt.

### Claim 3 (depends on 2)

The method of claim 2, wherein said tin-containing compound includes SnSO4.

### Claim 4 (depends on 1)

The method of claim 1, wherein said electrochemically active material is approximately 0.001 to 5% SnSO4 by weight.

### Claim 5 (depends on 4)

The method of claim 4, wherein said electrochemically active material is approximately 0.1 to 1% SnSO4 by weight.

### Claim 6 (depends on 5)

The method of claim 5, wherein said electrochemically active material is approximately 0.3% SnSO4 by weight.

### Claim 7 (depends on 1)

The method of claim 1, wherein said first electrode includes a material selected from the group consisting of substantially pure lead and a lead/tin alloy.

### Claim 8 (depends on 8)

The method of claim 8, wherein said first electrode is approximately 1 to 3% tin by weight.

### Claim 9 (depends on 8)

The method of claim 8, wherein said first electrode is approximately 0.5 to 1.5% tin by weight.

### Claim 10

A method of manufacturing a sulfated electrochemically active material for use in a lead acid electrochemical cell, comprising introducing sulfuric acid to an oxide of lead, and subsequently introducing a tin-containing compound.

### Claim 11 (depends on 10)

The method of claim 10, wherein said tin-containing compound is selected from the group consisting of SnSO4, SnO, metallic tin, a tin(II) salt and a tin(IV) salt.

### Claim 12

A sulfated electrochemically active material for a lead acid electrochemical cell produced by introducing sulfuric acid to an oxide of lead and subsequently introducing a tin-containing compound.

### Claim 13 (depends on 12)

The material of claim 12, wherein said tin-containing compound is selected from the group consisting of SnSO4, SnO, metallic tin, a tin(II) salt and a tin(IV) salt.

### Claim 14

An electrochemical cell, comprising: a first electrode of a first polarity, said first electrode being coated with a sulfated electrochemically active material to which has been added an oxide of lead, sulfuric acid and a tin-containing compound, said electrochemically active material being prepared by introducing the tin-containing compound to the material subsequent to introducing the sulfuric acid to the material; a second electrode of a polarity opposite the first electrode; and a separator between the first electrode and second electrode.

### Claim 15 (depends on 14)

The cell of claim 14, wherein said tin-containing compound is selected from the group consisting of SnSO4, SnO, metallic tin, a tin(II) salt and a tin(IV) salt.

### Claim 16 (depends on 15)

The cell of claim 15, wherein said electrochemically active material is approximately 0.001 to 5% to SnSO4 by weight.

### Claim 17 (depends on 16)

The cell of claim 16, wherein said electrochemically active material is approximately 0.1 to 1% SnSO4 by weight.

### Claim 18 (depends on 17)

The cell of claim 17, wherein said electrochemically active material is approximately 0.3% SnSO4 by weight.

### Claim 19 (depends on 14)

The cell of claim 14, wherein said first electrode includes a material selected from the group consisting of substantially pure lead and a lead/tin alloy.

### Claim 20 (depends on 19)

The cell of claim 19, wherein said first electrode is approximately zero to 3% tin by weight.

### Claim 21 (depends on 20)

The cell of claim 20, wherein said first electrode is approximately 0.5 to 1.5% tin by weight.

### Claim 22

A method of manufacturing a lead acid electrochemical cell, comprising: preparing an unsulfated electrochemically active material to which has been added an oxide of lead and including a compound selected from the group consisting of tin, antimony, arsenic, germanium, indium, selenium, gallium, tellurium and other semiconductors; coating said electrochemically active material onto a first electrode of a first polarity; arranging said first electrode adjacent to a second electrode of a polarity opposite the first electrodes, the first electrode and second electrode being separated by a separator; and containing said first electrode, second electrode and separator in a container.

### Claim 23 (depends on 22)

The method of claim 22, wherein said compound is selected from the group consisting of SnSO4, SnO, metallic tin, a tin(II) salt and a tin(IV) salt.

### Claim 24 (depends on 23)

The method of claim 23, wherein said compound includes SnSO4.

### Claim 25 (depends on 22)

The method of claim 22, wherein said electrochemically active material is approximately 0.001 to 5% SnSO4 by weight.

### Claim 26 (depends on 25)

The method of claim 25, wherein said electrochemically active material is approximately 0.1 to 1% SnSO4 by weight.

### Claim 27 (depends on 26)

The method of claim 26, wherein said electrochemically active material is approximately 0.3% SnSO4 by weight.

### Claim 28 (depends on 22)

The method of claim 22, wherein said first electrode includes a material selected from the group consisting of substantially pure lead and a lead/tin alloy.

### Claim 29 (depends on 28)

The method of claim 28, wherein said first electrode is less than 3% tin by weight.

### Claim 30 (depends on 29)

The method of claim 29, wherein said first electrode is approximately 0.5 to 1.5% tin by weight.

### Claim 31

A method of manufacturing an unsulfated electrochemically active material for use in a lead acid electrochemical cell, comprising introducing an oxide of lead to water; and introducing a compound selected from the group consisting of tin, antimony, arsenic, germanium, indium, selenium, gallium, tellurium and other semiconductors.

### Claim 32 (depends on 31)

The method of claim 31, wherein said compound is selected from the group consisting of SnSO4, SnO, metallic tin, a tin(II) salt and a tin(IV) salt.

### Claim 33

An unsulfated electrochemically active material for a lead acid electrochemical cell produced by introducing an oxide of lead to water; and introducing a compound selected from the group consisting of tin, antimony, arsenic, germanium, indium, selenium, gallium, tellurium and other semiconductors.

### Claim 34 (depends on 33)

The material of claim 33, wherein said compound is selected from the group consisting of SnSO4, SnO, metallic tin, a tin(II) salt and a tin(IV) salt.

### Claim 35

An electrochemical cell, comprising: a first electrode of a first polarity; and a coating coated onto said first electrode, the coating including an unsulfated electrochemically active material to which has been added an oxide of lead and a compound selected from the group consisting of tin, antimony, arsenic, germanium, indium, selenium, gallium, tellurium and other semiconductors.

### Claim 36 (depends on 35)

The cell of claim 35, wherein said compound is selected from the group consisting of SnSO4, SnO, metallic tin, a tin(II) salt and a tin(IV) salt.

### Claim 37 (depends on 36)

The cell of claim 36, wherein said electrochemically active material is approximately 0.001 to 5% to SnSO4 by weight.

### Claim 38 (depends on 37)

The cell of claim 37, wherein said electrochemically active material is approximately 0.1 to 1% SnSO4 by weight.

### Claim 39 (depends on 38)

The cell of claim 38, wherein said electrochemically active material is approximately 0.3% SnSO4 by weight.

### Claim 40 (depends on 35)

The cell of claim 35, wherein said first electrode includes a material selected from the group consisting of substantially pure lead and a lead/tin alloy.

### Claim 41 (depends on 40)

The cell of claim 40, wherein said first electrode is approximately zero to 3% tin by weight.

### Claim 42 (depends on 41)

The cell of claim 41, wherein said first electrode is approximately 0.5 to 1.5% tin by weight.