# US 2003/0215624 A1 · Electrospinning of vinyl alcohol polymer and copolymer fibers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0215624 A1
- Document ID: US20030215624A1
- Status: Published application
- Kind: A1
- Application number: 10/407,322
- Filed: 2003-04-04
- Published: 2003-11-20
- Earliest claimed: 2002-04-05
- Inventors: John M. Layman; Gary Wnek; El-Refaie Kenawy
- Web page: https://patentgrep.com/patent/US20030215624A1

## CPC

- D01D 5/0038: {the fibre formed by solvent evaporation, i.e. dry electro-spinning}
- A61L 27/50: Materials characterised by their function or physical properties {, e.g. injectable or lubricating compositions, shape-memory materials, surface modified materials}
- A61L 27/54: Biologically active materials, e.g. therapeutic substances {(A61L27/227 takes precedence)}
- D01F 6/30: comprising olefins as the major constituent
- A61L 2300/25: Peptides having up to 20 amino acids in a defined sequence
- A61L 2300/602: Type of release, e.g. controlled, sustained, slow
- Y10T 428/249921: Web or sheet containing structurally defined element or component
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Electrospinning of EVOH copolymer fiber is accomplished by dissolving the copolymers in a 2-propanol/water solution. The mixture is heated until the EVOH copolymers are fully dissolved in the solution. The copolymers fibers are then electrospun after the mixture is allowed to cool. Additionally, fully hydrolyzed PVA was able to be electrospun through use of a non-ionic surfactant. This electrospun matrix can be stabilized against disintegration and water by soaking of the matrix in methanol.

## Claims

### Claim 1

A polymer matrix comprising electrospun poly(ethylene-co-vinyl alcohol) fibers.

### Claim 2

A solution for use in electrostatic processing of a polymer, the solution comprising poly(ethylene-co-vinyl alcohol) and 2-propanol.

### Claim 3 (depends on 2)

The solution described in claim 2, wherein the solution comprises about 50/50% to 90/10% v/v 2-propanol/water.

### Claim 4 (depends on 3)

The solution described in claim 3, wherein the solution comprises about 70/30% v/v 2-propanol/water.

### Claim 5

A method of preparing a solution for use in electrostatic processing of a polymer, the method comprising:
providing an effective amount of poly(ethylene-co-vinyl alcohol);
providing a solution of 2-propanol and water;
dissolving the poly(ethylene-co-vinyl alcohol) in the 2-propanol and water by heating the mixture thereof to a temperature above an upper critical solution temperature;
allowing the mixture to cool to a temperature below the upper critical solution temperature.

### Claim 6 (depends on 5)

The method described in claim 5, wherein the poly(ethylene-co-vinyl alcohol) content is in the range of about 55-70 mole %.

### Claim 7 (depends on 5)

The method described in claim 5, wherein the effective amount of poly(ethylene-co-vinyl alcohol) to 2-propanol and water is at least about 2.5 w/v %.

### Claim 8 (depends on 7)

The method described in claim 7, wherein the effective amount of poly(ethylene-co-vinyl alcohol) to 2-propanol and water is at least about 5 w/v %.

### Claim 9 (depends on 5)

The method described in claim 5, wherein the mixture is heated to at least about 50° C.

### Claim 10 (depends on 5)

The method describe in claim 5, wherein the mixture is heated to at least about 60° C.

### Claim 11 (depends on 5)

The method described in claim 5, wherein the mixture is allowed to cool below about 40° C.

### Claim 12 (depends on 5)

The method described in claim 5, further comprising the step of reheating the mixture to a temperature lower than the upper critical solution temperature.

### Claim 13

A method of electrospinning poly(ethylene-co-vinyl alcohol) fibers comprising:
providing an effective amount of poly(ethylene-co-vinyl alcohol);
providing a solution of 2-propanol and water;
dissolving the poly(ethylene-co-vinyl alcohol) in the 2-propanol and water by heating the mixture thereof to a temperature above an upper critical solution temperature;
allowing the mixture to cool to a temperature below the upper critical solution temperature; and
electrospinning the cooled mixture.

### Claim 14 (depends on 13)

The method described in claim 13, wherein the poly(ethylene-co-vinyl alcohol) content is in the range of about 55-70 mole %.

### Claim 15 (depends on 13)

The method described in claim 13, wherein the effective amount of poly(ethylene-co-vinyl alcohol) to 2-propanol and water is at least about 2.5 w/v %.

### Claim 16 (depends on 13)

The method described in claim 13, wherein the effective amount of poly(ethylene-co-vinyl alcohol) to 2-propanol and water is at least about 5 w/v %.

### Claim 17 (depends on 13)

The method described in claim 13, wherein the mixture is heated to at least about 50° C.

### Claim 18 (depends on 13)

The method describe in claim 13, wherein the mixture is heated to at least about 60° C.

### Claim 19 (depends on 13)

The method described in claim 13, wherein the mixture is allowed to cool below about 40° C.