# US 2003/0213987 A1 · MIS capacitor and method of formation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0213987 A1
- Document ID: US20030213987A1
- Status: Published application
- Kind: A1
- Application number: 10/145,993
- Filed: 2002-05-16
- Published: 2003-11-20
- Earliest claimed: 2002-05-16
- Assignees: Micron Technology, Inc.
- Inventors: Cem Basceri; Garo J. Derderian
- Web page: https://patentgrep.com/patent/US20030213987A1

## CPC

- H10D 1/68: Capacitors having no potential barriers
- H10D 1/042: {using deposition processes to form electrode extensions}
- H10D 1/66: Conductor-insulator-semiconductor capacitors, e.g. MOS capacitors
- H10D 1/682: {having dielectrics comprising perovskite structures}
- H10D 1/712: {being rough surfaces, e.g. using hemispherical grains}
- H10D 1/716: {having vertical extensions}
- H10B 12/033: {the capacitor extending over the transistor}
- H10P 14/6328: {Deposition from the gas or vapour phase}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69391: {the material containing aluminium, e.g. Al2O3}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10P 14/69397: {the material containing two or more metal elements}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

An MIS capacitor with low leakage and high capacitance is disclosed. A layer of hemispherical grained polysilicon (HSG) is formed as a lower electrode. Prior to the dielectric formation, the hemispherical grained polysilicon layer may be optionally subjected to a nitridization or anneal process. A dielectric layer of aluminum oxide (Al2O3), or a composite stack of interleaved layers of aluminum oxide and other metal oxide dielectric materials, is fabricated over the hemispherical grained polysilicon layer and after the optional nitridization or anneal process. The dielectric layer of aluminum oxide (Al2O3) or the aluminum oxide composite stack may be optionally subjected to a post-deposition treatment to further increase the capacitance and decrease the leakage current. A metal nitride upper electrode is formed over the dielectric layer or the composite stack by a deposition technique or by atomic layer deposition.

## Claims

### Claim 1

An MIS capacitor comprising:
a lower electrode formed over a semiconductor substrate;
a dielectric layer comprising aluminum oxide formed over said lower electrode; and
a metal nitride upper electrode formed over said dielectric layer.

### Claim 2 (depends on 1)

The MIS capacitor of claim 1, wherein said dielectric layer further comprises a material incorporated with said aluminum oxide.

### Claim 3 (depends on 2)

The MIS capacitor of claim 2, wherein said material is selected from the group consisting of tantalum oxide, zirconium oxide, hafnium oxide, hafnium-aluminum-oxygen alloys and lanthanum-aluminum-oxygen alloys.

### Claim 4 (depends on 3)

The MIS capacitor of claim 3, wherein said dielectric layer comprises aluminum oxide and tantalum oxide.

### Claim 5 (depends on 3)

The MIS capacitor of claim 3, wherein said dielectric layer is formed of interleaved layers of aluminum oxide and tantalum oxide.

### Claim 6 (depends on 1)

The MIS capacitor of claim 1, wherein said dielectric layer comprises an aluminum oxide/tantalum oxide/aluminum oxide composite stack.

### Claim 7 (depends on 1)

The MIS capacitor of claim 1, wherein said dielectric layer consists essentially of an aluminum oxide dielectric layer.

### Claim 8 (depends on 1)

The MIS capacitor of claim 1, wherein said dielectric layer is an ALD aluminum oxide layer.

### Claim 9 (depends on 8)

The MIS capacitor of claim 8, wherein said dielectric layer is an annealed ALD aluminum oxide layer.

### Claim 10 (depends on 8)

The MIS capacitor of claim 8, wherein said ALD aluminum oxide layer has a thickness of about 10 Angstroms to about 100 Angstroms.

### Claim 11 (depends on 1)

The MIS capacitor of claim 1, wherein said upper electrode is a tungsten nitride layer.

### Claim 12 (depends on 11)

The MIS capacitor of claim 11, wherein said upper electrode is an ALD tungsten nitride layer.

### Claim 13 (depends on 12)

The MIS capacitor of claim 12, wherein said ALD tungsten nitride layer is a nitridized ALD tungsten nitride layer.

### Claim 14 (depends on 1)

The MIS capacitor of claim 1, wherein said upper electrode is a titanium nitride layer.

### Claim 15 (depends on 14)

The MIS capacitor of claim 14, wherein said upper electrode is an ALD titanium nitride layer.

### Claim 16 (depends on 15)

The MIS capacitor of claim 15, wherein said ALD titanium nitride layer is a nitridized ALD titanium nitride layer.

### Claim 17 (depends on 1)

The MIS capacitor of claim 1, wherein said upper electrode is a boron-doped titanium nitride layer.

### Claim 18 (depends on 17)

The MIS capacitor of claim 17, wherein said boron-doped titanium nitride layer is a nitridized boron-doped titanium nitride layer.

### Claim 19 (depends on 18)

The MIS capacitor of claim 18, wherein said boron-doped titanium nitride layer has a boron concentration of about 0.01% to about 30%.

### Claim 20 (depends on 1)

The MIS capacitor of claim 1, wherein said lower electrode is formed of a material selected from the group consisting of hemispherical grained polysilicon, silica, germanium and silicon.

### Claim 21 (depends on 20)

The MIS capacitor of claim 20, wherein said lower electrode is formed of hemispherical grained polysilicon.

### Claim 22 (depends on 21)

The MIS capacitor of claim 21, wherein said lower electrode is formed of etched hemispherical grained polysilicon with activated hemispherical grained polysilicon grains.

### Claim 23 (depends on 22)

The MIS capacitor of claim 22, wherein said etched hemispherical grained polysilicon is a nitridized etched hemispherical grained polysilicon.

### Claim 24 (depends on 22)

The MIS capacitor of claim 22, wherein said etched hemispherical grained polysilicon is an annealed hemispherical grained polysilicon.

### Claim 25 (depends on 1)

The MIS capacitor of claim 1 further comprising a silicon-doped layer at the interface between said lower electrode and said dielectric layer comprising aluminum oxide.

### Claim 26 (depends on 25)

The MIS capacitor of claim 25, wherein said silicon-doped layer has a thickness of about 5 Angstroms to about 50 Angstroms.

### Claim 27 (depends on 25)

The MIS capacitor of claim 25, wherein said silicon-doped layer is an aluminum-oxygen-silicon layer.

### Claim 28 (depends on 1)

The MIS capacitor of claim 1 further comprising a metal-doped layer at the interface between said dielectric layer comprising aluminum oxide and said metal nitride upper electrode.

### Claim 29 (depends on 28)

The MIS capacitor of claim 28, wherein said metal-doped layer has a thickness of about 5 Angstroms to about 100 Angstroms.

### Claim 30 (depends on 28)

The MIS capacitor of claim 28, wherein said metal-doped layer is an aluminum-titanium-oxygen-nitrogen layer.

### Claim 31 (depends on 28)

The MIS capacitor of claim 28, wherein said metal-doped layer comprises a metal similar to the metal of said metal nitride upper electrode.

### Claim 32

A memory device comprising:
a substrate;
a memory cell formed over said substrate, said memory cell comprising a transistor including a gate fabricated on said substrate, and source and drain regions in said substrate disposed adjacent to said gate; and
a charge storage capacitor electrically connected to one of said source and drain regions, said capacitor comprising a semiconductive layer, an aluminum oxide dielectric layer formed over said semiconductive layer, and a metal nitride layer formed over said aluminum oxide dielectric layer.

### Claim 33 (depends on 32)

The memory device of claim 32, wherein said aluminum oxide dielectric layer further comprises a material incorporated with said aluminum oxide.

### Claim 34 (depends on 33)

The memory device of claim 33, wherein said material is selected from the group consisting of tantalum oxide, zirconium oxide, hafnium oxide, hafnium-aluminum-oxygen alloys and lanthanum-aluminum-oxygen alloys.

### Claim 35 (depends on 33)

The memory device of claim 33, wherein said aluminum oxide dielectric layer further comprises tantalum oxide.

### Claim 36 (depends on 33)

The memory device of claim 33, wherein said aluminum oxide dielectric layer is formed of interleaved layers of aluminum oxide and tantalum oxide.

### Claim 37 (depends on 33)

The memory device of claim 33, wherein said aluminum oxide dielectric layer is an ALD aluminum oxide layer.

### Claim 38 (depends on 37)

The memory device of claim 37, wherein said aluminum oxide dielectric layer is an annealed ALD aluminum oxide layer.

### Claim 39 (depends on 37)

The memory device of claim 37, wherein said ALD aluminum oxide layer has a thickness of about 10 Angstroms to about 100 Angstroms.

### Claim 40 (depends on 32)

The memory device of claim 32, wherein said metal nitride layer is a tungsten nitride layer.

### Claim 41 (depends on 40)

The memory device of claim 40, wherein said metal nitride layer is an ALD tungsten nitride layer.

### Claim 42 (depends on 41)

The memory device of claim 41, wherein said ALD tungsten nitride layer is a nitridized ALD tungsten nitride layer.

### Claim 43 (depends on 32)

The memory device of claim 32, wherein said metal nitride layer is a titanium nitride layer.

### Claim 44 (depends on 43)

The memory device of claim 43, wherein said metal nitride layer is an ALD titanium nitride layer.

### Claim 45 (depends on 44)

The memory device of claim 44, wherein said ALD titanium nitride layer is a nitridized ALD titanium nitride layer.

### Claim 46 (depends on 32)

The memory device of claim 32, wherein said metal nitride layer is a boron-doped titanium nitride layer.

### Claim 47 (depends on 46)

The memory device of claim 46, wherein said boron-doped titanium nitride layer is a nitridized boron-doped titanium nitride layer.

### Claim 48 (depends on 47)

The memory device of claim 47, wherein said boron-doped titanium nitride layer has a boron concentration of about 0.01% to about 30%.

### Claim 49 (depends on 32)

The memory device of claim 32, wherein said semiconductive layer is formed of a material selected from the group consisting of hemispherical grained polysilicon, silica, germanium and silicon.

### Claim 50 (depends on 49)

The memory device of claim 49, wherein said semiconductive layer is formed of hemispherical grained polysilicon.

### Claim 51 (depends on 50)

The memory device of claim 50, wherein said semiconductive layer is formed of etched hemispherical grained polysilicon with activated hemispherical grained polysilicon grains.

### Claim 52 (depends on 51)

The memory device of claim 51, wherein said etched hemispherical grained polysilicon is a nitridized etched hemispherical grained polysilicon.

### Claim 53 (depends on 51)

The memory device of claim 51, wherein said etched hemispherical grained polysilicon is an annealed hemispherical grained polysilicon.

### Claim 54 (depends on 32)

The memory device of claim 32, wherein said memory cell is a DRAM memory cell.

### Claim 55 (depends on 32)

The memory device of claim 32, wherein said memory cell is a SRAM memory cell.

### Claim 56

A processor-based system comprising:
a processor; and
an integrated circuit coupled to said processor, at least one of said integrated circuit and processor containing a capacitor, said capacitor comprising a hemispherical grained polysilicon lower capacitor electrode; an aluminum oxide dielectric layer formed over said lower capacitor electrode; and a metal nitride upper capacitor electrode formed over said aluminum oxide dielectric layer.

### Claim 57 (depends on 56)

The processor-based system of claim 56, wherein said hemispherical grained polysilicon lower electrode is a nitridized hemispherical grained polysilicon lower electrode.

### Claim 58 (depends on 56)

The processor-based system of claim 56, wherein said aluminum oxide dielectric layer is an ALD aluminum oxide dielectric layer.

### Claim 59 (depends on 58)

The processor-based system of claim 58, wherein said aluminum oxide dielectric layer is a nitridized ALD aluminum oxide dielectric layer.

### Claim 60 (depends on 56)

The processor-based system of claim 56, wherein said aluminum oxide dielectric layer further comprises a material incorporated with said aluminum oxide.

### Claim 61 (depends on 60)

The processor-based system of claim 60, wherein said material is selected from the group consisting of tantalum oxide, zirconium oxide, hafnium oxide, hafnium-aluminum-oxygen alloys and lanthanum-aluminum-oxygen alloys.

### Claim 62 (depends on 56)

The processor-based system of claim 56, wherein said integrated circuit is a memory device.

### Claim 63 (depends on 62)

The processor-based system of claim 62, wherein said memory device is a DRAM memory device.

### Claim 64 (depends on 62)

The processor-based system of claim 62, wherein said memory device is a SRAM memory device.

### Claim 65

A method of forming an MIS capacitor on a semiconductor substrate, comprising the acts of:
forming a semiconductive layer over a substrate;
forming a dielectric layer comprising aluminum oxide over said semiconductive layer by atomic layer deposition; and
forming a metal nitride layer over said dielectric layer.

### Claim 66 (depends on 65)

The method of claim 65, wherein said semiconductive layer is formed of hemispherical grained polysilicon.

### Claim 67 (depends on 66)

The method of claim 66 further comprising the act of opening the grains which form said layer of hemispherical grained polysilicon to activate said grains.

### Claim 68 (depends on 67)

The method of claim 67, wherein said act of opening said grains further comprising etching said layer of hemispherical grained polysilicon to form an etched layer of hemispherical grained polysilicon.

### Claim 69 (depends on 69)

The method of claim 69, wherein said act of etching said layer of hemispherical grained polysilicon further comprises contacting said layer of hemispherical grained polysilicon with a solution of HF.

### Claim 70 (depends on 69)

The method of claim 69 further comprising the act of subjecting said layer of hemispherical grained polysilicon to an RTN process.

### Claim 71 (depends on 69)

The method of claim 69 further comprising the act of subjecting said layer of hemispherical grained polysilicon to an anneal process.

### Claim 72 (depends on 69)

The method of claim 69 further comprising the act of subjecting said layer of hemispherical grained polysilicon to a PH3 anneal.

### Claim 73 (depends on 65)

The method of claim 65, wherein said metal nitride layer is a titanium nitride layer formed by CVD.

### Claim 74 (depends on 65)

The method of claim 65, wherein said metal nitride layer is a titanium nitride layer formed by ALD.

### Claim 75 (depends on 74)

The method of claim 74, wherein said titanium nitride layer is formed by ALD using a nitrogen source and a titanium source precursor.

### Claim 76 (depends on 65)

The method of claim 65, wherein said metal nitride layer is a boron-doped titanium nitride layer formed by CVD.

### Claim 77 (depends on 77)

The method of claim 77, wherein said act of providing said boron-doped titanium nitride layer further comprises the act of incorporating boron into a titanium nitride layer.

### Claim 78 (depends on 78)

The method of claim 78, wherein said act of incorporating boron into a titanium nitride layer further comprises the act of exposing said titanium nitride layer to B2H6.

### Claim 79 (depends on 79)

The method of claim 79, wherein said act of incorporating boron into a titanium nitride layer further comprises the act of exposing said titanium nitride layer to B2H6 at a temperature of about 200° C. to about 600° C.

### Claim 80 (depends on 65)

The method of claim 65, wherein said metal nitride layer is a tungsten nitride layer formed by CVD.

### Claim 81 (depends on 65)

The method of claim 65, wherein said metal nitride layer is a tungsten nitride layer formed by ALD.

### Claim 82 (depends on 65)

The method of claim 65, wherein said metal nitride layer is a boron-doped tungsten nitride layer formed by CVD.

### Claim 83 (depends on 82)

The method of claim 82, wherein said act of providing said boron-doped tungsten nitride layer further comprises the act of incorporating boron into a tungsten nitride layer.

### Claim 84 (depends on 65)

The method of claim 65, wherein said aluminum oxide dielectric layer is formed by ALD using an ozone source and an aluminum source precursor.

### Claim 85 (depends on 86)

The method of claim 86, wherein said aluminum source precursor is trimethyl-aluminum.

### Claim 86 (depends on 65)

The method of claim 65, wherein said aluminum oxide dielectric layer is formed to a thickness of about 10 Angstroms to about 500 Angstroms.

### Claim 87 (depends on 86)

The method of claim 86, wherein said aluminum oxide dielectric layer is formed to a thickness of about 25 Angstroms to about 100 Angstroms.

### Claim 88 (depends on 65)

The method of claim 65, wherein said aluminum oxide dielectric layer further comprises a material selected from the group consisting of tantalum oxide, zirconium oxide, hafnium oxide, hafnium-aluminum-oxygen alloys and lanthanum-aluminum-oxygen alloys.

### Claim 89 (depends on 88)

The method of claim 88, wherein said aluminum oxide dielectric layer is formed as a composite stack of at least one aluminum oxide layer and at least one tantalum oxide layer.

### Claim 90 (depends on 89)

The method of claim 89, wherein said aluminum oxide dielectric layer is formed of interleaved layers of aluminum oxide and tantalum oxide.

### Claim 91 (depends on 90)

The method of claim 90, wherein said aluminum oxide dielectric layer is an aluminum oxide/tantalum oxide/aluminum oxide stack.

### Claim 92

A method of forming an aluminum oxide MIS capacitor on a semiconductor substrate, comprising the acts of:
forming a lower capacitor electrode of hemispherical grained polysilicon over said semiconductor substrate;
forming a dielectric composite stack comprising aluminum oxide over said lower capacitor electrode; and
forming an upper capacitor electrode of tungsten nitride over said dielectric composite stack.

### Claim 93 (depends on 92)

The method of claim 92, wherein said dielectric composite stack is formed by ALD.

### Claim 94 (depends on 93)

The method of claim 93, wherein said dielectric composite stack is formed of interleaved layers of aluminum oxide and another metal oxide material.

### Claim 95 (depends on 94)

The method of claim 94, wherein said metal oxide material is selected from the group consisting of tantalum oxide, zirconium oxide, hafnium oxide, hafnium-aluminum-oxygen alloys and lanthanum-aluminum-oxygen alloys.

### Claim 96 (depends on 92)

The method of claim 92 further comprising the act of subjecting said dielectric composite stack to a nitridizing treatment.

### Claim 97 (depends on 96)

The method of claim 96 further comprising the act of subjecting said dielectric composite stack to a PH3 anneal treatment.

### Claim 98 (depends on 92)

The method of claim 92, wherein said tungsten nitride layer is formed by ALD using a tungsten source and a nitrogen source precursor.

### Claim 99 (depends on 92)

The method of claim 92 further comprising the act of etching said hemispherical grained polysilicon to form an etched hemispherical grained polysilicon.

### Claim 100 (depends on 99)

The method of claim 99, wherein said act of etching said hemispherical grained polysilicon further comprises contacting said hemispherical grained polysilicon with a solution of HF.

### Claim 101 (depends on 100)

The method of claim 100 further comprising the act of subjecting said hemispherical grained polysilicon to a PH3 anneal.

### Claim 102 (depends on 101)

The method of claim 101 further comprising the act of subjecting said hemispherical grained polysilicon to an RTN treatment.

### Claim 103 (depends on 102)

The method of claim 102 further comprising the act of subjecting said hemispherical grained polysilicon to a HF solution after said PH3 anneal and before said RTN treatment.