# US 2003/0211730 A1 · Method for forming contact hole in semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0211730 A1
- Document ID: US20030211730A1
- Status: Published application
- Kind: A1
- Application number: 10/330,913
- Filed: 2002-12-27
- Published: 2003-11-13
- Earliest claimed: 2002-05-07
- Assignees: Hynix Semiconductor Inc.
- Inventors: Kun Joo Park
- Web page: https://patentgrep.com/patent/US20030211730A1

## CPC

- H10W 20/069: {by forming self-aligned vias or self-aligned contact plugs}
- H10D 84/0149: {Manufacturing their interconnections or electrodes, e.g. source or drain electrodes}
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Disclosed is a method for forming a contact hole in the process of manufacturing a logic device employing a shallow trench isolation (STI) method. The method prevents an isolation region from being damaged because there is little overlap margin for a contact hole in the active region, when a contact hole is formed in an isolation region beyond the border of an active region, that is, when a borderless contact hole is formed. According to the method, a silicon nitride layer used as an etch-stop layer is formed in the process of providing the STI, thereby avoiding deterioration of the characteristics of a resulting semiconductor device.

## Claims

### Claim 1

A method for forming a contact hole in a semiconductor device comprising the steps of:
forming a pad oxide layer and a first silicon nitride layer on a silicon substrate;
forming a trench on a part of the entire structure formed in the above step and forming an oxide layer on the entire structure including the trench;
selectively etching the oxide layer so that the oxide layer remains only within the trench;
forming a second silicon nitride layer over the entire structure including the oxide layer remaining in the trench
planarizing the second silicon nitride layer and a part of the first silicon nitride layer, so that the top surface of the first silicon nitride layer is exposed, and then selectively etching a part of the first silicon nitride layer and the pad oxide layer to define a gate region;
forming a gate within the etched part for defining a gate region in the first silicon nitride layer and the pad oxide layer, and then forming a source/drain in the silicon substrate under each side of the gate; and
forming an interlayer oxide film over the above structure and selectively etching the interlayer oxide film to form a contact hole in the interlayer oxide film which exposes the source/drain.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a gas formed by mixing CxFy, CoHpFq and Ar in a predetermined ratio is used for etching the first silicon nitride layer and the pad oxide layer.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a gas formed by mixing Cl2, HBr, Ns and Ar is used for forming the trench.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the etching of the oxide layer within the trench is performed by means of plasma etching using a ‘CxFy+O2’ gas,
wherein the selective etching of the first silicon nitride layer and the pad oxide layer is also performed by means of plasma etching using a ‘CxFy+O2’ gas, and
wherein the etching of the interlayer oxide film is performed by means of plasma etching using a ‘CxFy+O2’ gas as a main component.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the oxide layer within the trench is etched at a relatively high speed and the remaining first silicon nitride is etched at a very low speed by using the ‘CxFy+O2’ gas and controlling the added amount of the oxygen (O2).

### Claim 6 (depends on 1)

The method according to claim 1, wherein the pad oxide layer laid under the first silicon nitride layer is remained without being damaged even if the oxide layer within the trench is fully etched at the time of plasma etching of the oxide layer within the trench.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the interlayer oxide film is plasma etched using a gas which has a high ratio of C to F, e.g., C4F8 or C5H8 gas with a minimum amount of O2 being added.