# US 2003/0211670 A1 · Methods for forming low resistivity, ultrashallow junctions with low damage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0211670 A1
- Document ID: US20030211670A1
- Status: Published application
- Kind: A1
- Application number: 10/142,313
- Filed: 2002-05-09
- Published: 2003-11-13
- Earliest claimed: 2002-05-09
- Assignees: Varian Semiconductor Equipment Associates, Inc.
- Inventors: Daniel F. Downey
- Web page: https://patentgrep.com/patent/US20030211670A1

## CPC

- H10P 30/21: {of electrically active species}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/225: {of a molecular ion, e.g. decaborane}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods for forming ultrashallow junctions in semiconductor wafers include introducing into a shallow surface layer of a semiconductor wafer a dopant material that is selected to form charge carrier complexes which produce at least two charge carriers per complex, and short-time thermal processing of the doped surface layer to form the charge carrier complexes. The short-time thermal processing step may be implemented as flash rapid thermal processing of the doped surface layer, sub-melt laser processing of the doped surface layer, or RF or microwave annealing of the doped surface layer.

## Claims

### Claim 1

A method for forming an ultrashallow junction in a semiconductor wafer, comprising:
introducing into a shallow surface layer of a semiconductor wafer a dopant material that is selected to form charge carrier complexes which produce at least two charge carriers per complex; and
short-time thermal processing of the doped surface layer to form said charge carrier complexes.

### Claim 2 (depends on 1)

A method as defined in claim 1, wherein the step of short-time thermal processing comprises flash rapid thermal processing of the doped surface layer.

### Claim 3 (depends on 1)

A method as defined in claim 1, wherein the step of short-time thermal processing comprises rapid heating of the substrate to an intermediate temperature and flash heating of the doped surface layer to a final temperature that is higher than the intermediate temperature.

### Claim 4 (depends on 1)

A method as defined in claim 1, wherein the step of short-time thermal processing comprises sub-melt laser processing of the doped surface layer.

### Claim 5 (depends on 1)

A method as defined in claim 1, wherein the step of short-time thermal processing of the doped surface layer comprises heating the doped surface layer to a desired temperature for a time of about 100 milliseconds or less.

### Claim 6 (depends on 1)

A method as defined in claim 1, wherein the step of short-time thermal processing of the doped surface layer comprises heating the doped surface layer to a desired temperature for a time of about 10 milliseconds or less.

### Claim 7 (depends on 1)

A method as defined in claim 1, wherein the step of short-time thermal processing of the doped surface layer comprises thermal processing at a temperature in a range of about 1000° C. to 1410° C.

### Claim 8 (depends on 1)

A method as defined in claim 1, wherein the step of short-time thermal processing of the doped surface layer comprises thermal processing at a temperature in a range of about 1050° C. to 1350° C.

### Claim 9 (depends on 1)

A method as defined in claim 1, wherein the dopant material comprises two species selected to form said charge carrier complexes.

### Claim 10 (depends on 1)

A method as defined in claim 1, wherein the dopant material comprises a compound containing two species selected to form said charge carrier complexes.

### Claim 11 (depends on 1)

A method as defined in claim 1, wherein the dopant material is selected to chemically bond with atoms of the semiconductor wafer to form the charge carrier complexes.

### Claim 12 (depends on 1)

A method as defined in claim 1, wherein the dopant material is selected to form bound exciton complexes.

### Claim 13 (depends on 1)

A method as defined in claim 1, wherein the dopant material is selected from the group consisting of B—F, B—Ge, B—Si, P—F, P—Ge, P—Si, As—F, As—Ge and As—Si.

### Claim 14 (depends on 1)

A method as defined in claim 1, wherein the step of introducing a dopant material into a shallow surface layer comprises ion implantation of the dopant material.

### Claim 15 (depends on 1)

A method as defined in claim 1, wherein the step of introducing a dopant material into a shallow surface layer comprises plasma doping of the dopant material.

### Claim 16 (depends on 1)

A method as defined in claim 1, wherein said dopant material is selected from the group consisting of boron, boron and germanium, BF2 and BF3.

### Claim 17 (depends on 1)

A method as defined in claim 1, wherein the step of short-time thermal processing comprises RF or microwave annealing of the doped surface layer.

### Claim 18

A method for forming an ultrashallow junction in a semiconductor wafer, comprising:
introducing into a shallow surface layer of a semiconductor wafer a dopant material selected from the group consisting of boron, boron and germanium, BF2 and BF3; and
flash rapid thermal processing of the doped surface layer to form charge carrier complexes which produce at least two charge carriers per complex.

### Claim 19 (depends on 18)

A method as defined in claim 18, wherein the step of flash rapid thermal processing of the doped surface layer comprises rapid heating of the substrate to an intermediate temperature and flash heating of the doped surface layer to a final temperature that is higher than the intermediate temperature.

### Claim 20 (depends on 18)

A method as defined in claim 18, wherein the step of flash rapid thermal processing of the doped surface layer comprises heating the doped surface layer to a desired temperature for a time of about 100 milliseconds or less.

### Claim 21 (depends on 18)

A method as defined in claim 18, wherein the step of flash rapid thermal processing of the doped surface layer comprises heating the doped surface layer to a desired temperature for a time of about 10 milliseconds of less.

### Claim 22 (depends on 18)

A method as defined in claim 18, wherein the step of flash rapid thermal processing of the doped surface layer comprises thermal processing at a temperature in a range of about 1000° C. to 1410° C.

### Claim 23 (depends on 18)

A method as defined in claim 18, wherein the step of flash rapid thermal processing of the doped surface layer comprises thermal processing at a temperature in a range of about 1050° C. to 1350° C.

### Claim 24 (depends on 18)

A method as defined in claim 18, wherein the step of introducing a dopant material comprises ion implantation of the dopant material.

### Claim 25 (depends on 18)

A method as defined in claim 18, wherein the step of introducing a dopant material comprises plasma doping of the dopant material.