# US 2003/0211422 A1 · Process for modifying resist structures and resist films from the aqueous phase

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0211422 A1
- Document ID: US20030211422A1
- Status: Published application
- Kind: A1
- Application number: 10/376,883
- Filed: 2003-02-28
- Published: 2003-11-13
- Earliest claimed: 2002-02-28
- Assignees: Infineon Technologies AG
- Inventors: Siew Siew Yip; Jorg Rottstegge; Ernst-Christian Richter; Gertrud Falk; Michael Sebald; Kerstin Seibold; Marion Kern
- Web page: https://patentgrep.com/patent/US20030211422A1

## CPC

- G03F 7/40: Treatment after imagewise removal, e.g. baking
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A process for chemically amplifying structured resists includes applying a chemically amplified resist to a substrate and structuring it in a customary manner. Preferably, the amplification agent is applied in the aqueous phase to the structured resist and, after chemical amplification is complete, excess agent is removed by an aqueous wash medium. By using water as a solvent for the amplification agent and as a wash medium, it is possible to avoid organic solvents that constitute an explosion hazard. Furthermore, removal of partially exposed resist sections is suppressed.

## Claims

### Claim 1

A method for amplifying structured resists, which comprises:
(a) applying a chemically amplified photoresist to a substrate, the photoresist having:
a film-forming polymer having:
acid-labile groups that are cleaved under action of acid and liberate groups that result in an increase in a solubility of the film-forming polymer in aqueous alkaline developers; and
anchor groups for linkage of amplification agents;
a photo acid generator;
a solvent in which the film-forming polymer is soluble, the solvent having a solvent polarity;
(b) drying the photoresist to produce a resist film;
(c) exposing the resist film section-by-section to obtain an exposed resist, an acid being liberated by the photo acid generator in exposed parts of the resist film;
(d) heating the exposed resist, the acid-labile groups being cleaved in the exposed parts and polar groups being liberated on the film-forming polymer, and, as a result, obtaining a contrasted resist having polar resist sections and non-polar resist sections;
(e) developing the contrasted resist with an alkaline developer having a polarity higher than the solvent polarity, the film-forming polymer being insoluble in the alkaline developer, the polar resist sections being removed from the substrate to obtain a structured resist;
(f) applying an amplification agent to the structured resist in a liquid phase, the amplification agent having at least one reactive group that can react with an anchor group of the film-forming polymer, the liquid phase containing a solvent or a solvent mixture in which the film-forming polymer is insoluble, and leaving the solution of the amplification agent on the structured resist to cause linkage of the amplification agent to the film-forming polymer to take place and obtain an amplified resist; and
(g) washing the amplified resist with a wash medium containing water as a solvent to remove excess amplification agent.

### Claim 2 (depends on 1)

The method according to claim 1, which further comprises providing the wash medium with more than 95% by weight of water.

### Claim 3 (depends on 1)

The method according to claim 1, which further comprises selecting the liquid phase of the amplification agent to be an aqueous solution or an aqueous emulsion.

### Claim 4 (depends on 1)

The method according to claim 1, which further comprises providing the liquid phase of the amplification agent with between 50% and 99% by weight of water.

### Claim 5 (depends on 1)

The method according to claim 1, which further comprises carrying out development and amplification of the contrasted resist in a common step.

### Claim 6 (depends on 1)

The method according to claim 1, which further comprises carrying out the developing step and the amplification agent applying step in a common step.

### Claim 7 (depends on 1)

The method according to claim 1, which further comprises providing a swelling promoter in the solution of the amplification agent.

### Claim 8 (depends on 7)

The method according to claim 7, which further comprises selecting the swelling promoter from a group consisting of an alcohol, a carboxylic acid, and a surfactant.

### Claim 9 (depends on 1)

The method according to claim 1, which further comprises providing a sterically hindered base or tertiary amine in the solution of the amplification agent.

### Claim 10 (depends on 1)

The method according to claim 1, which further comprises selecting the reactive group of the amplification agent as an amino group.

### Claim 11 (depends on 1)

The method according to claim 1, which further comprises providing the amplification agent with at least two reactive groups that can react with the anchor group of the film-forming polymer.

### Claim 12 (depends on 1)

The method according to claim 1, which further comprises providing the wash medium with more than 95% by weight of water.

### Claim 13 (depends on 12)

The method according to claim 12, which further comprises selecting the liquid phase of the amplification agent to be an aqueous solution or an aqueous emulsion.

### Claim 14 (depends on 13)

The method according to claim 13, which further comprises providing the liquid phase of the amplification agent with between 50% and 99% by weight of water.

### Claim 15 (depends on 14)

The method according to claim 14, which further comprises carrying out development and amplification of the contrasted resist in a common step.

### Claim 16 (depends on 15)

The method according to claim 15, which further comprises providing a swelling promoter in the solution of the amplification agent.

### Claim 17 (depends on 16)

The method according to claim 16, which further comprises selecting the swelling promoter from a group consisting of an alcohol, a carboxylic acid, and a surfactant.

### Claim 18 (depends on 15)

The method according to claim 15, which further comprises providing a sterically hindered base or tertiary amine in the solution of the amplification agent.

### Claim 19 (depends on 17)

The method according to claim 17, which further comprises selecting the reactive group of the amplification agent as an amino group.

### Claim 20 (depends on 18)

The method according to claim 18, which further comprises selecting the reactive group of the amplification agent as an amino group.

### Claim 21 (depends on 19)

The method according to claim 19, which further comprises providing the amplification agent with at least two reactive groups that can react with the anchor group of the film-forming polymer.

### Claim 22 (depends on 20)

The method according to claim 20, which further comprises providing the amplification agent with at least two reactive groups that can react with the anchor group of the film-forming polymer.

### Claim 23 (depends on 1)

The method according to claim 1, which further comprises providing the anchor groups with at least one group in the form of a protected anchor group.