# US 2003/0209818 A1 · Pretreatment of contact lens moulds

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0209818 A1
- Document ID: US20030209818A1
- Status: Published application
- Kind: A1
- Application number: 10/431,151
- Filed: 2003-05-07
- Published: 2003-11-13
- Earliest claimed: 2002-05-13
- Inventors: Harald Bothe; Bernhard Seiferling; Axel Heinrich; Achim Muller
- Web page: https://patentgrep.com/patent/US20030209818A1

## CPC

- B29D 11/00125: {Auxiliary operations, e.g. removing oxygen from the mould, conveying moulds from a storage to the production line in an inert atmosphere}
- B29C 33/62: based on polymers or oligomers
- B29C 35/0888: {using transparant moulds}
- B29C 37/0032: {the coating being applied upon the mould surface before introducing the moulding compound, e.g. applying a gelcoat (B29C44/14 and B29C44/32 take precedence)}
- B08B 9/00: Cleaning hollow articles by methods or apparatus specially adapted thereto
- B29C 2035/0827: {using UV radiation}
- B29L 2011/0041: {Contact lenses}
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B08B: CLEANING IN GENERAL; PREVENTION OF FOULING IN GENERAL
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

The invention relates to a process for the manufacture of a moulding, comprising the steps: (a) applying to at least one surface of a multi-part UV-transmissible quartz or glass mould a solution of a poly(oxyethylene)-poly(oxypropylene) block copolymer, (b) optionally, drying the solution on the mould, (c) introducing an aqueous solution comprising a water-soluble prepolymer having crosslinkable groups into the mould, (d) initiating of crosslinking by irradiation with UV-light, (e) removing the mouldings from the mould, and (f) optionally, washing and drying the mould.

## Claims

### Claim 1

A process for the manufacture of a moulding, comprising the steps:
(a) applying to at least one surface of a multi-part UV-transmissible quartz or glass mould a solution of a poly(oxyethylene)-poly(oxypropylene) block copolymer,
(b) optionally, drying the solution on the mould,
(c) introducing an aqueous solution comprising a water-soluble prepolymer having crosslinkable groups into the mould,
(d) initiating of crosslinking by irradiation with UV-light,
(e) removing the mouldings from the mould, and
(f) optionally, washing and drying the mould.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the steps (a) to (f) are repeated in a cycle.

### Claim 3 (depends on 1, 2)

The process according to claim 1 or 2, wherein the moulding is an ophthalmic lens, in particular a contact lens or an intraocular lens.

### Claim 4 (depends on 1, 2, 3)

The process according to any one of the claims 1 to 3, wherein the poly(oxyethylene)-poly(oxypropylene) block copolymer is of formula
HO—(CH2CH2—O)y—(CH(CH3)CH2O)x—(CH2CH2O)y—H (I), HO—(CH(CH3)CH2O)x—(CH2CH2O)y—(CH2CH(CH3)O)x—H (II), 3
wherein i, j, x and y each have values from 2 to 400.

### Claim 5 (depends on 4)

The process according to claim 4, wherein the block copolymer is of formula (I) having a number average molecular weight of from 3,000 to 15,000.

### Claim 6 (depends on 4)

The process according to claim 4, wherein the block copolymer is of formula (III) having a number average molecular weight of from 10,000 to 30,000.

### Claim 7

The process according to any one of claims i to 6, wherein the solution comprises, based on the total weight of the solution, of from 0.01 to 3% (w/w), preferably of from 0.1 to 0.25% (w/w) of the block copolymer.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

The process according to any one of claims 1 to 7, wherein the solution comprises a C1-C4-alkanol, C2-C6-dialkylether, or C3-C5-ketone.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

The process according to any one of claims 1 to 8 wherein, in step (a), the solution of the tenside is applied by spraying or stamping.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

The process according to any one of claims 1 to 9, wherein the processing of each of steps (a) and (b) is less than 10 seconds.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

The process according to any one of claims 1 to 10, wherein the water-soluble prepolymer having crosslinkable groups is a derivative of a polyvinyl alcohol having a molecular weight of at least about 2000 that, based on the number of hydroxy groups of the polyvinyl alcohol, comprises from approximately 0.5 to approximately 80% of units of formula
4
wherein R is C1-C8-alkylene, R1 is hydrogen or C1-C7-alkyl and R2 is an olefinically unsaturated, electron-attracting, copolymerizable radical preferably having up to 25 carbon atoms.

### Claim 12 (depends on 11)

The process according to claim 11, wherein, in the units of formula (V), R is methylene, R1 is hydrogen and R2 is acryloyl.

### Claim 13

A process for the pretreatment of contact lens moulds comprising the following steps:
(a) providing a two-part UV-curable reusable quartz or glass lens mould;
(b) applying to at least one part of the mould a layer of at least one non-ionic tenside which is a poly(oxyethylene)-poly(oxypropylene) block copolymer; and
(c) drying said layer.