# US 2003/0209745 A1 · Tailored insulator properties for devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0209745 A1
- Document ID: US20030209745A1
- Status: Published application
- Kind: A1
- Application number: 10/408,069
- Filed: 2003-04-04
- Published: 2003-11-13
- Earliest claimed: 2001-04-20
- Assignees: International Business Machines Corporation
- Inventors: Robert Benjamin Laibowitz; John David Baniecki; Johannes Georg Bednorz; Jean-Pierre A. Locquet
- Web page: https://patentgrep.com/patent/US20030209745A1

## CPC

- H10P 14/6544: {to change the morphology of the insulating materials, e.g. transformation of an amorphous layer into a crystalline layer}
- H10B 12/03: {Making the capacitor or connections thereto}
- H10D 64/01338: {with a treatment, e.g. annealing, after the formation of the conductor}
- H10D 64/01342: {by deposition, e.g. evaporation, ALD or laser deposition (H10D64/01344 takes precedence)}
- H10P 14/6539: {by exposure to corpuscular radiation, e.g. exposure to electrons, alpha-particles, protons or ions}
- H10P 30/20: into semiconductor materials, e.g. for doping
- H10P 30/221: {characterised by the angle between the ion beam and the mask}
- H10P 30/222: {characterised by the angle between the ion beam and the crystal planes or the main crystal surface (characterised by the angle between the ion beam and the mask H10P30/221)}
- H10P 30/40: into insulating materials
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10P 14/69398: {the material having a perovskite structure, e.g. BaTiO3}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for tailoring properties of high k thin layer perovskite materials, and devices comprising such insulators are herein presented. The method comprise the steps of, first, substantially completing the manufacture of a device, which device contains the high k insulator in a polycrystalline form. The device, such as a capacitor, or an FET, went through the typically high temperature manufacturing process of a fabrication line. In the next step, the device is in situ ion implanted with such a dose and energy to convert a fraction of the polycrystalline material into an amorphous material state, hereby tailoring the properties of the insulator. The fraction of polycrystalline material converted to amorphous material might be 1. This process can be applied to many electronic devices and some optical devices. The process results in novel perovskite thin layer materials and novel devices fabricated with such materials.

## Claims

### Claim 1

A method for tailoring properties of an insulator, comprising the steps of:
substantially completing the manufacture of a device, wherein the device comprise the insulator, and wherein the insulator is formed of a crystalline material; and
converting a fraction of the crystalline material of the insulator into an amorphous material by ion implanting the device.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of converting by ion implanting includes a choice of parameters for the ion implanting in a manner that the tailored properties of the insulator match operational requirements of the device.

### Claim 3 (depends on 1)

The method of claim 1, wherein the tailored properties of the insulator comprise a dielectric constant.

### Claim 4 (depends on 1)

The method of claim 1, wherein the tailored properties of the insulator comprise a leakage current.

### Claim 5 (depends on 1)

The method of claim 1, wherein the tailored properties of the insulator comprise a strain.

### Claim 6 (depends on 1)

The method of claim 1, wherein the fraction of the crystalline material converted into the amorphous material is in the range of about 0.01 to 1.

### Claim 7 (depends on 6)

The method of claim 6, wherein the fraction of the crystalline material converted into the amorphous material is in the range of about 0.5 to 0.99.

### Claim 8 (depends on 3)

The method of claim 3, wherein the dielectric constant ranges between the dielectric constant of the crystalline material and the dielectric constant of the amorphous material, exhibiting a substantially linear relationship with the fraction of the amorphous material present in the insulator.

### Claim 9 (depends on 1)

The method of claim 1, wherein the step of ion implanting includes the step of using a mask.

### Claim 10 (depends on 1)

The method of claim 1 further comprising the step of annealing the device.

### Claim 11 (depends on 1)

The method of claim 1, further including the step of selecting the insulator to be a perovskite material.

### Claim 12 (depends on 2)

The method of claim 2, wherein the step of substantially completing the manufacture of the device includes the step of forming an electrical device.

### Claim 13 (depends on 12)

The method of claim 12, wherein the electrical device is embedded in an integrated circuit.

### Claim 14 (depends on 2)

The method of claim 2, wherein the step of substantially completing the manufacture of the device includes the step of forming an optical device.

### Claim 15 (depends on 12)

The method of claim 12, wherein the electrical device is a capacitor, and wherein a dielectric layer between capacitor electrodes comprise the fractionally amorphous insulator.

### Claim 16 (depends on 15)

The method of claim 15, wherein the step of ion implanting is executed through the top electrode of the capacitor.

### Claim 17 (depends on 15)

The method of claim 15, further including the step of selecting the fractionally amorphous insulator to be a perovskite material.

### Claim 18 (depends on 17)

The method of claim 17, wherein the step of ion implanting includes the step of using a mask.

### Claim 19 (depends on 17)

The method of claim 17, wherein the fraction of amorphous matter in the perovskite is essentially 1.

### Claim 20 (depends on 17)

The method of claim 17, wherein the implanted ion species are chosen from the group consisting of Mn, Cr, Cl, Nb, Ti, F, H or D.

### Claim 21 (depends on 20)

The method of claim 20, further comprising the step of annealing the capacitor in an oxygen atmosphere up to a temperature of 600° C.

### Claim 22 (depends on 17)

The method of claim 17, wherein the capacitor is embedded in an integrated circuit.

### Claim 23 (depends on 12)

The method of claim 12, wherein the electrical device is a stacked-capacitor, and wherein a dielectric layer between stacked-capacitor electrodes comprise the fractionally amorphous insulator.

### Claim 24 (depends on 23)

The method of claim 23, further including the step of selecting the fractionally amorphous insulator to be a perovskite material.

### Claim 25 (depends on 24)

The method of claim 24, wherein the step of ion implanting includes the step of using a mask.

### Claim 26 (depends on 24)

The method of claim 24, wherein the fraction of amorphous matter in the perovskite is essentially 1.

### Claim 27 (depends on 23)

The method of claim 23, wherein the ion implantation provides a strain relief between the stacked-capacitor electrodes and the insulator.

### Claim 28 (depends on 24)

The method of claim 24, wherein the stacked-capacitor is embedded in an integrated circuit.

### Claim 29 (depends on 12)

The method of claim 12, wherein the electrical device is a field effect transistor, and wherein a gate dielectric comprise the fractionally amorphous insulator.

### Claim 30 (depends on 29)

The method of claim 29, wherein the step of ion implanting is executed through a gate electrode of the transistor.

### Claim 31 (depends on 29)

The method of claim 29, further including the step of selecting the fractionally amorphous insulator to be a perovskite material.

### Claim 32 (depends on 31)

The method of claim 31, wherein the step of ion implanting includes the step of using a mask.

### Claim 33 (depends on 31)

The method of claim 31, wherein the fraction of amorphous matter in the perovskite is essentially 1.

### Claim 34 (depends on 29)

The method of claim 29, further comprising the step of annealing the transistor in an oxygen atmosphere up to a temperature of 600° C.

### Claim 35 (depends on 31)

The method of claim 31, wherein the field effect transistor is embedded in an integrated circuit.

### Claim 36 (depends on 14)

The method of claim 14, wherein the optical device is a dielectric mirror, and wherein dielectric layers of the dielectric mirror comprise a plurality of layers of the fractionally amorphous insulator.

### Claim 37 (depends on 36)

The method of claim 36, further including the step of selecting the fractionally amorphous insulator to be a perovskite material.

### Claim 38 (depends on 14)

The method of claim 14, wherein the optical device is a dielectric filter, and wherein dielectric layers of the dielectric filter comprise a plurality of layers of the fractionally amorphous insulator.

### Claim 39 (depends on 38)

The method of claim 38, further including the step of selecting the fractionally amorphous insulator to be a perovskite material.

### Claim 40 (depends on 14)

The method of claim 14, wherein the optical device is a dielectric grating, and wherein a dielectric layer of the dielectric grating comprise a layer of the fractionally amorphous insulator.

### Claim 41 (depends on 40)

The method of claim 40, further including the step of selecting the fractionally amorphous insulator to be a perovskite material.

### Claim 42 (depends on 40)

The method of claim 40, wherein the step of ion implanting includes the step of using a mask.

### Claim 43

A less than 1000 nm thick layer of perovskite material, consisting of a polycrystalline and an amorphous material state, wherein the fraction of the amorphous material state is in the range of 50% to 99%.

### Claim 44

A device, comprising:
a less than 1000 nm thick layer of perovskite material, consisting of a polycrystalline and an amorphous material state, wherein the fraction of the amorphous material state is in the range of 50% to 99%.

### Claim 45 (depends on 44)

The device of claim 44, wherein the device is an electronic device.

### Claim 46 (depends on 45)

The method of claim 45, wherein the electrical device is embedded in an integrated circuit.

### Claim 47 (depends on 44)

The device of claim 44, wherein the step of substantially completing the manufacture of the device includes the step of forming an optical device.

### Claim 48 (depends on 45)

The device of claim 45, wherein the device is a capacitor, and wherein a dielectric layer between capacitor electrodes comprise the fractionally amorphous perovskite material.

### Claim 49 (depends on 45)

The device of claim 45, wherein the electronic device is a stacked capacitor, and wherein a dielectric layer between stacked-capacitor electrodes comprise the fractionally amorphous perovskite material.

### Claim 50 (depends on 45)

The device of claim 45, wherein the electronic device is a field effect transistor, and wherein a gate dielectric comprise the fractionally amorphous perovskite material.

### Claim 51 (depends on 47)

The device of claim 47, wherein the optical device is a dielectric mirror, and wherein dielectric layers of the dielectric mirror comprise a plurality of layers of the fractionally amorphous perovskite material.

### Claim 52 (depends on 47)

The device of claim 47, wherein the optical device is a dielectric filter, and wherein dielectric layers of the dielectric filter comprise a plurality of layers of the fractionally amorphous perovskite material.

### Claim 53 (depends on 47)

The device of claim 47, wherein the optical device is a dielectric grating, and wherein a dielectric layer of the dielectric grating comprise a layer of the fractionally amorphous perovskite material.