# US 2003/0209167 A1 · Dental retrograde-filling material containing cobalt and process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0209167 A1
- Document ID: US20030209167A1
- Status: Published application
- Kind: A1
- Application number: 10/198,535
- Filed: 2002-07-18
- Published: 2003-11-13
- Earliest claimed: 2002-05-07
- Inventors: Feng-Huei Lin; Chun-Pin Lin; Wen-Hsi Wang
- Web page: https://patentgrep.com/patent/US20030209167A1

## CPC

- A61K 6/831: comprising non-metallic elements or compounds thereof, e.g. carbon
- A61K 6/54: Filling; Sealing
- A61K 6/84: comprising metals or alloys
- A61K 6/853: Silicates
- A61K 6/876: Calcium oxide
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)

## Abstract

A dental retrograde-filling material process, comprising the steps of: taking 3:1 mole ratio of a calcium oxide and a silicon dioxide mixes a 1˜5 w.t. % cobalt oxide at 1200˜1800 degree Celsius temperature to get a A-product including a tricalcium silicate, a dicalcium silicate and a containing cobalt composition; taking 3:1 mole ratio of a calcium oxide and an aluminum oxide at 1200˜1800 degree Celsius temperature reacts a B-product including a tricalcium aluminate; taking 4:1:1 mole ratio of a calcium oxide, an aluminum oxide and a ferric oxide at 1200˜1800 degree Celsius temperature reacts a C-product including a calcium alminoferrite; and mixing the A-product, B-product and C-product are the retrograde-filling material. The dental retrograde-filling material mixes of taking 8:1:1 mole ratio of said tricalcium silicate, dicalcium silicate and containing cobalt composition, tricalcium aluminate and calcium alminoferrite.

## Claims

### Claim 1

A dental retrograde-filling material process, comprising the steps of:
taking 3:1 mole ratio of a calcium oxide and a silicon dioxide mixes a 1˜5 w.t. % cobalt oxide at 1200˜1800 degree Celsius temperature to get a A-product including a tricalcium silicate, a dicalcium silicate and containing a cobalt composition;
taking 3:1 mole ratio of a calcium oxide and an aluminum oxide at 1200˜1800 degree Celsius temperature reacts a B-product including a tricalcium aluminate;
taking 4:1:1 mole ratio of a calcium oxide, an aluminum oxide and a ferric oxide at 1200˜1800 degree Celsius temperature reacts a C-product including a calcium alminoferrite; and
mixing said A-product, B-product and C-product being said retrograde-filling material.

### Claim 2 (depends on 1)

The process of claim 1, wherein the best heating temperature of A-product is 1400 degree Celsius temperature.

### Claim 3 (depends on 1)

The process of claim 1, wherein the heating time of A-product is 2 to 4 hours.

### Claim 4 (depends on 3)

The process of claim 3, wherein the best heating time of A-product is 3 hours.

### Claim 5 (depends on 1)

The process of claim 1, wherein further comprises a step: said A-product after heating being rapid cooling by a nitrogen solution.

### Claim 6 (depends on 1)

The process of claim 1, wherein the best heating temperature of B-product is 1400 degree Celsius temperature.

### Claim 7 (depends on 1)

The process of claim 1, wherein the heating time of B-product is 2 to 4 hours.

### Claim 8 (depends on 7)

The process of claim 7, wherein the best heating time of B-product is 2 hours.

### Claim 9 (depends on 1)

The process of claim 1, wherein further comprises a step: said B-product after heating being rapid cooling by a nitrogen solution.

### Claim 10 (depends on 1)

The process of claim 1, wherein the best heating temperature of C-product is 1350 degree Celsius temperature.

### Claim 11 (depends on 1)

The process of claim 1, wherein the heating time of C-product is 2 to 4 hours.

### Claim 12 (depends on 11)

The process of claim 11, wherein the best heating time of C-product is 2 hours.

### Claim 13 (depends on 1)

The process of claim 1, wherein further comprises a step: said C-product after heating being rapid cooling by a nitrogen solution.

### Claim 14

A dental retrograde-filling material comprising:
a tricalcium silicate, dicalcium silicate and containing cobalt composition;
a tricalcium aluminate;
a calcium alminoferrite;
wherein said dental retrograde-filling material mixes of taking 8:1:1 mole ratio of said tricalcium silicate, dicalcium silicate and containing cobalt composition, tricalcium aluminate and calcium alminoferrite.