# US 2003/0208091 A1 · Process for producing pyromellitic acid

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0208091 A1
- Document ID: US20030208091A1
- Status: Published application
- Kind: A1
- Application number: 10/440,255
- Filed: 2003-05-19
- Published: 2003-11-06
- Earliest claimed: 1999-05-10
- Assignees: Mitsubishi Gas Chemical Company, Inc.
- Inventors: Kazuo Tanaka; Hiroshi Ogawa; Ikutraro Maruki; Atsushi Okoshi
- Web page: https://patentgrep.com/patent/US20030208091A1

## CPC

- C07C 51/265: having alkyl side chains which are oxidised to carboxyl groups
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

A process for producing pyromellitic acid which comprises oxidizing 2,4,5-trimethylbenzealdehyde and/or its oxidized derivative in the presence of a catalyst containing iron, manganese and bromine, or additionally containing zirconium or cerium continuously or semi-continuously using aqueous acetic acid solvent and 0.05-2% by weight of bromide ion. The catalyst used in the present invention has high activity, and the catalyst solution has low corrosive because the reaction is performed at low bromide concentration by using a solvent of aqueous acetic acid. So pyromellitic acid is produced industrially advantageously in high yield continuously or semi-continuously which has been a major difficulty up to now.

## Claims

### Claim 1

A process for producing pyromellitic acid which comprises oxidizing 2,4,5-trimethylbenzaldehyde and/or its oxidized derivative in the presence of a catalyst containing iron, manganese and bromine, and which may additionally contain zirconium or cerium continuously or semi-continuously by using aqueous acetic acid solvent.

### Claim 2 (depends on 1)

A process for producing pyromellitic acid according to claim 1, wherein 2,4,5-trimethylbenzealdehyde and/or its oxidized derivative is oxidized continuously at 180-240° C. using an acetic acid solvent containing 10-90% by weight of water.

### Claim 3 (depends on 2)

A process for producing pyromellitic acid according to claim 2, wherein total concentration of metal atom of iron, manganese, zirconium and cerium is 0.03-2% by weight in solvent, and atomic ratio of bromide ion to total of the metal is 0.5-15.

### Claim 4 (depends on 2)

A process for producing pyromellitic acid according to claim 2, wherein the catalyst has on the base of total metals, a manganese content of 55-99.9% by weight, an iron content of 0.1-15% by weight, zirconium content of 0-15% by weight and cerium content of 0-15% by weight.

### Claim 5 (depends on 2)

A process for producing pyromellitic acid according to claim 2, wherein iron content is 1-200 ppm, zirconium content is 0-500 ppm and cerium content is 0-500 ppm in solvent.

### Claim 6 (depends on 1)

A process for producing pyromellitic acid according to claim 1, wherein 2,4,5-trimethylbenzaldehyde and/or its oxidized derivative is oxidized semi-continuously at through-put of 0.6-1.3 mol/hr-kg.

### Claim 7 (depends on 6)

A process for producing pyromellitic acid according to claim 6, wherein the catalyst has on the base of basis of total metals, a manganese content of 50-99.9% by weight, an iron content of 0.1-15% by weight, a zirconium content of 0-15% by weight and cerium content of 0-15% by weight.

### Claim 8 (depends on 7)

A process for producing pyromellitic acid according to claim 7, wherein iron content is 1-200 ppm, zirconium content is 0-500 ppm and cerium content is 0-500 ppm in solvent.