# US 2003/0207952 A1 · Crosslinked olefin elastomer foam

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0207952 A1
- Document ID: US20030207952A1
- Status: Published application
- Kind: A1
- Application number: 10/454,512
- Filed: 2003-06-05
- Published: 2003-11-06
- Earliest claimed: 1998-10-30
- Assignees: Mitsui Chemicals, Inc.
- Inventors: Takanori Sueda; Naoto Yasaka; Chong-Sun Yoo; Jeong-Sik Yoon; Kyung-Man Choi; Kwon-Ik Lee
- Web page: https://patentgrep.com/patent/US20030207952A1

## CPC

- C08J 9/0061: {characterized by the use of several polymeric components}
- C08J 9/0023: {containing oxygen}
- C08J 9/08: developing carbon dioxide
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08J 2323/02: not modified by chemical after treatment
- C08J 2323/06: Polyethene
- C08J 2323/16: Ethene-propene or ethene-propene-diene copolymers
- C08J 2423/00: Characterised by the use of homopolymers or copolymers of unsaturated aliphatic hydrocarbons having only one carbon-to-carbon double bond; Derivatives of such polymers
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 2203/14: used for foams
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2312/00: Crosslinking
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A crosslinked olefin elastomer foam has a specific gravity of 0.05 to 0.2, an expansion ratio of 8 to 15, a compression set of 30 to 60% and a tear strength of 1.5 to 2.5 kg/cm. The crosslinked foam is obtained by heating an elastomer composition comprising a specific ethylene/α-olefin copolymer, an organic peroxide, a crosslinking auxiliary and a foaming agent. The crosslinked foam has a high expansion ratio, is free from surface roughening attributed to defoaming, realizes a soft touch, exhibits a low compression set and is excellent in mechanical strength (particularly tear strength) and heat resistance.

## Claims

### Claim 1

A crosslinked olefin elastomer foam having a specific gravity of 0.05 to 0.2, an expansion ratio of 8 to 15, a compression set of 30 to 60% and a tear strength of 1.5 to 2.5 kg/cm.

### Claim 2

A crosslinked olefin elastomer foam having a specific gravity of 0.1 to 0.2, a compression set of 20 to 60% and a tear strength of 2.0 to 4.0 kg/cm.

### Claim 3 (depends on 1, 2)

The crosslinked olefin elastomer foam as claimed in claim 1 or 2, which is a crosslinked foam obtained by heating an olefin elastomer composition, the olefin elastomer composition comprising:
an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F).

### Claim 4 (depends on 3)

The crosslinked olefin elastomer foam as claimed in claim 3, wherein the ethylene/α-olefin copolymer (A) has a molecular weight distribution (Mw/Mn), as measured by gel permeation chromatography (GPC), of 2.3 to 4.0.

### Claim 5 (depends on 3)

The crosslinked olefin elastomer foam as claimed in claim 3, wherein the ethylene/α-olefin copolymer (A) comprises a mixture of:
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A1) having a density of greater than 0.88 g/cm3 but not greater than 0.90 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min; and
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A2) having a density of 0.90 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A1) and ethylene/α-olefin copolymer (A2) is 100 parts by weight,
the mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 6 (depends on 3)

The crosslinked olefin elastomer foam as claimed in claim 3, wherein the ethylene/α-olefin copolymer (A) comprises a mixture of:
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A3) having a density of 0.88 to less than 0.91 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min; and
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A4) having a density of 0.91 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A3) and ethylene/α-olefin copolymer (A4) is 100 parts by weight,
the mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 7 (depends on 3)

The crosslinked olefin elastomer foam as claimed in claim 3, wherein the crosslinking auxiliary (E) and the organic peroxide (D) are used in a weight ratio ((E)/(D)) of 1/8 to 3/1.

### Claim 8

An elastomer composition for crosslinked olefin elastomer foam, comprising:
an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F).

### Claim 9 (depends on 8)

The elastomer composition for crosslinked olefin elastomer foam as claimed in claim 8, wherein the ethylene/α-olefin copolymer (A) has a molecular weight distribution (Mw/Mn), as measured by gel permeation chromatography (GPC), of 2.3 to 4.0.

### Claim 10

An elastomer composition for crosslinked olefin elastomer foam, comprising:
an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F),
wherein the ethylene/α-olefin copolymer (A) comprises a mixture of:
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A1) having a density of greater than 0.88 g/cm3 but not greater than 0.90 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min; and
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A2) having a density of 0.90 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A1) and ethylene/α-olefin copolymer (A2) is 100 parts by weight,
the mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 11

An elastomer composition for crosslinked olefin elastomer foam, comprising:
an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F), wherein the ethylene/α-olefin copolymer (A) comprises a mixture of:
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A3) having a density of 0.88 to less than 0.91 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min; and
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A4) having a density of 0.91 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A3) and ethylene/α-olefin copolymer (A4) is 100 parts by weight,
the mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 12 (depends on 8, 10, 11)

The elastomer composition for crosslinked olefin elastomer foam as claimed in any of claims 8, 10 and 11, wherein the crosslinking auxiliary (E) and the organic peroxide (D) are used in a weight ratio ((E)/(D)) of 1/8 to 3/1.

### Claim 13

A crosslinked olefin elastomer foam, which is a crosslinked foam obtained by heating an olefin elastomer composition, the olefin elastomer composition comprising:
70 to 95 parts by weight of an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min, and
5 to 30 parts by weight of a modified polyolefin (B) obtained by grafting a polyolefin with an unsaturated carboxylic acid or a derivative thereof, provided that the sum of ethylene/α-olefin copolymer (A) and modified polyolefin (B) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F).

### Claim 14 (depends on 13)

The crosslinked olefin elastomer foam as claimed in claim 13, wherein the ethylene/α-olefin copolymer (A) has a molecular weight distribution (Mw/Mn), as measured by gel permeation chromatography (GPC), of 2.3 to 4.0.

### Claim 15 (depends on 13)

The crosslinked olefin elastomer foam as claimed in claim 13, wherein the ethylene/α-olefin copolymer (A) comprises a mixture of:
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A1) having a density of greater than 0.88 g/cm3 but not greater than 0.90 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, and
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A2) having a density of 0.90 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A1) and ethylene/α-olefin copolymer (A2) is 100 parts by weight,
the mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 16

A crosslinked olefin elastomer foam, which is a crosslinked foam obtained by heating an olefin elastomer composition, the olefin elastomer composition comprising:
50 to 95 parts by weight of an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min, and
5 to 50 parts by weight of a high-pressure processed low-density polyethylene (C) having a density of 0.91 to less than 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A) and high-pressure processed low-density polyethylene (C) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F).

### Claim 17

A crosslinked olefin elastomer foam, which is a crosslinked foam obtained by heating an olefin elastomer composition, the olefin elastomer composition comprising:
5 to 90 parts by weight of an ethylene/α-olefin copolymer (A1) having a density of greater than 0.88 g/cm3 but not greater than 0.90 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min,
5 to 90 parts by weight of an ethylene/α-olefin copolymer (A2) having a density of 0.90 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, and
5 to 50 parts by weight of a high-pressure processed low-density polyethylene (C) having a density of 0.91 to less than 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A1), ethylene/α-olefin copolymer (A2) and high-pressure processed low-density polyethylene (C) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F),
wherein the ethylene/α-olefin copolymer (A1) and the ethylene/α-olefin copolymer (A2) constitute a mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 18

A crosslinked olefin elastomer foam, which is a crosslinked foam obtained by heating an olefin elastomer composition, the olefin elastomer composition comprising:
20 to 90 parts by weight of an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min,
5 to 30 parts by weight of a modified polyolefin (B) obtained by grafting a polyolefin with an unsaturated carboxylic acid or a derivative thereof, and
5 to 50 parts by weight of a high-pressure processed low-density polyethylene (C) having a density of 0.91 to less than 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A), modified polyolefin (B) and high-pressure processed low-density polyethylene (C) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F).

### Claim 19

A crosslinked olefin elastomer foam, which is a crosslinked foam obtained by heating an olefin elastomer composition, the olefin elastomer composition comprising:
5 to 85 parts by weight of an ethylene/α-olefin copolymer (A1) having a density of greater than 0.88 g/cm3 but not greater than 0.90 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min,
5 to 85 parts by weight of an ethylene/α-olefin copolymer (A2) having a density of 0.90 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min,
5 to 30 parts by weight of a modified polyolefin (B) obtained by grafting a polyolefin with an unsaturated carboxylic acid or a derivative thereof, and
5 to 50 parts by weight of a high-pressure processed low-density polyethylene (C) having a density of 0.91 to less than 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A1), ethylene/α-olefin copolymer (A2), modified polyolefin (B) and high-pressure processed low-density polyethylene (C) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F),
wherein the ethylene/α-olefin copolymer (A1) and the ethylene/α-olefin copolymer (A2) constitute a mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 20 (depends on 13, 16, 17, 18, 19)

The crosslinked olefin elastomer foam as claimed in any of claims 13, 16, 17, 18 and 19, wherein the crosslinking auxiliary (E) and the organic peroxide (D) are used in a weight ratio ((E)/(D)) of 1/8 to 3/1.

### Claim 21

An elastomer composition for crosslinked olefin elastomer foam, comprising:
70 to 95 parts by weight of an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min, and
5 to 30 parts by weight of a modified polyolefin (B) obtained by grafting a polyolefin with an unsaturated carboxylic acid or a derivative thereof, provided that the sum of ethylene/α-olefin copolymer (A) and modified polyolefin (B) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F).

### Claim 22 (depends on 21)

The elastomer composition for crosslinked olefin elastomer foam as claimed in claim 21, wherein the ethylene/α-olefin copolymer (A) has a molecular weight distribution (Mw/Mn), as measured by gel permeation chromatography (GPC), of 2.3 to 4.0.

### Claim 23 (depends on 21)

The elastomer composition for crosslinked olefin elastomer foam as claimed in claim 21, wherein the ethylene/α-olefin copolymer (A) comprises a mixture of:
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A1) having a density of greater than 0.88 g/cm3 but not greater than 0.90 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, and
5 to 95 parts by weight of an ethylene/α-olefin copolymer (A2) having a density of 0.90 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A1) and ethylene/α-olefin copolymer (A2) is 100 parts by weight,
the mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 24

An elastomer composition for crosslinked olefin elastomer foam, comprising:
50 to 95 parts by weight of an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min, and
5 to 50 parts by weight of a high-pressure processed low-density polyethylene (C) having a density of 0.91 to less than 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A) and high-pressure processed low-density polyethylene (C) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F).

### Claim 25

An elastomer composition for crosslinked olefin elastomer foam, comprising:
5 to 90 parts by weight of an ethylene/α-olefin copolymer (A1) having a density of greater than 0.88 g/cm3 but not greater than 0.90 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min,
5 to 90 parts by weight of an ethylene/α-olefin copolymer (A2) having a density of 0.90 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, and
5 to 50 parts by weight of a high-pressure processed low-density polyethylene (C) having a density of 0.91 to less than 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A1), ethylene/α-olefin copolymer (A2) and high-pressure processed low-density polyethylene (C) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F),
wherein the ethylene/α-olefin copolymer (A1) and the ethylene/α-olefin copolymer (A2) constitute a mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 26

An elastomer composition for crosslinked olefin elastomer foam, comprising:
20 to 90 parts by weight of an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min,
5 to 30 parts by weight of a modified polyolefin (B) obtained by grafting a polyolefin with an unsaturated carboxylic acid or a derivative thereof, and
5 to 50 parts by weight of a high-pressure processed low-density polyethylene (C) having a density of 0.91 to less than 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A), modified polyolefin (B) and high-pressure processed low-density polyethylene (C) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F).

### Claim 27

An elastomer composition for crosslinked olefin elastomer foam, comprising:
5 to 85 parts by weight of an ethylene/α-olefin copolymer (A1) having a density of greater than 0.88 g/cm3 but not greater than 0.90 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min,
5 to 85 parts by weight of an ethylene/α-olefin copolymer (A2) having a density of 0.90 to 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min,
5 to 30 parts by weight of a modified polyolefin (B) obtained by grafting a polyolefin with an unsaturated carboxylic acid or a derivative thereof, and
5 to 50 parts by weight of a high-pressure processed low-density polyethylene (C) having a density of 0.91 to less than 0.93 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (A1), ethylene/α-olefin copolymer (A2), modified polyolefin (B) and high-pressure processed low-density polyethylene (C) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F),
wherein the ethylene/α-olefin copolymer (A1) and the ethylene/α-olefin copolymer (A2) constitute a mixture having a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 10 g/10 min.

### Claim 28 (depends on 21, 24, 25, 26, 27)

The elastomer composition for crosslinked olefin elastomer foam as claimed in any of claims 21, 24, 25, 26 and 27, wherein the crosslinking auxiliary (E) and the organic peroxide (D) are used in a weight ratio ((E)/(D)) of 1/8 to 3/1.

### Claim 29

A crosslinked olefin elastomer foam, which is a crosslinked foam obtained by heating an olefin elastomer composition, the olefin elastomer composition comprising:
70 to 98 parts by weight of an ethylene/α-olefin copolymer (G) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, and
2 to 30 parts by weight of a polypropylene (H) having a melt flow rate (measured at 230° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (G) and polypropylene (H) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F),
wherein the ethylene/α-olefin copolymer (G) and the polypropylene (H) constitute a mixture having a melt flow rate (measured at 230° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min.

### Claim 30 (depends on 29)

The crosslinked olefin elastomer foam as claimed in claim 29, wherein the polypropylene (H) is at least one member selected from the group consisting of propylene homopolymer, propylene block copolymers and propylene/α-olefin random copolymers.

### Claim 31 (depends on 29)

The crosslinked olefin elastomer foam as claimed in claim 29, wherein the crosslinking auxiliary (E) and the organic peroxide (D) are used in a weight ratio ((E)/(D)) of 1/8 to 3/1.

### Claim 32

An elastomer composition for crosslinked olefin elastomer foam, comprising:
70 to 98 parts by weight of an ethylene/α-olefin copolymer (G) having a density of 0.88 to 0.92 g/cm3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 50 g/10 min, and
2 to 30 parts by weight of a polypropylene (H) having a melt flow rate (measured at 230° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.5 to 50 g/10 min, provided that the sum of ethylene/α-olefin copolymer (G) and polypropylene (H) is 100 parts by weight;
an organic peroxide (D);
a crosslinking auxiliary (E); and
a foaming agent (F),
wherein the ethylene/α-olefin copolymer (G) and the polypropylene (H) constitute a mixture having a melt flow rate (measured at 230°C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 min.

### Claim 33 (depends on 32)

The elastomer composition for crosslinked olefin elastomer foam as claimed in claim 32, wherein the polypropylene (H) is at least one member selected from the group consisting of propylene homopolymer, propylene block copolymers and propylene/α-olefin random copolymers.

### Claim 34 (depends on 32)

The elastomer composition for crosslinked olefin elastomer foam as claimed in claim 32, wherein the crosslinking auxiliary (E) and the organic peroxide (D) are used in a weight ratio ((E)/(D)) of 1/8 to 3/1.