# US 2003/0207591 A1 · A method for high temperature oxide layer anneal to prevent oxide edge peeling

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0207591 A1
- Document ID: US20030207591A1
- Status: Published application
- Kind: A1
- Application number: 10/140,396
- Filed: 2002-05-06
- Published: 2003-11-06
- Earliest claimed: 2002-05-06
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Ching-Shan Lu; Kuo-Bin Huang; Jih-Churng Twu
- Web page: https://patentgrep.com/patent/US20030207591A1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for preventing oxide layer peeling in a high temperature annealing process including providing a plurality of spaced apart stacked semiconductor wafers for carrying out a high temperature annealing process including ambient nitrogen gas the plurality of spaced apart stacked semiconductor wafers stacked such that a process surface including an oxide layer of at least one semiconductor wafer is adjacent to a backside surface of another semiconductor wafer said backside surface having a layer of silicon nitride formed thereon prior to carrying out the high temperature annealing process; and, carrying out the high temperature annealing process.

## Claims

### Claim 1

A method for preventing oxide layer peeling in a high temperature annealing process comprising the steps of:
providing a plurality of spaced apart stacked semiconductor wafers for carrying out a high temperature annealing process including ambient nitrogen gas the plurality of spaced apart stacked semiconductor wafers stacked such that a process surface including an oxide layer of at least one semiconductor wafer is adjacent to a backside surface of another semiconductor wafer said backside surface having a layer of silicon nitride formed thereon prior to carrying out the high temperature annealing process; and,
carrying out the high temperature annealing process.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silicon nitride layer is formed at a thickness of from about 300 Angstroms to about 2000 Angstroms.

### Claim 3 (depends on 1)

The method of claim 1, wherein the backside surface of the another semiconductor comprises a control wafer for monitoring the high temperature annealing process conditions.

### Claim 4 (depends on 3)

The method of claim 3, wherein the control wafer is provided for monitoring at least one of annealing temperature, oxide layer thickness, and semiconductor wafer electrical resistance.

### Claim 5 (depends on 3)

The method of claim 3, wherein the control wafer is disposed in a gas flow pathway for supplying the ambient nitrogen gas to the plurality of spaced apart stacked semiconductor wafers.

### Claim 6 (depends on 1)

The method of claim 1, wherein the high temperature annealing process is carried out in one of a vertically and horizontally oriented furnace.

### Claim 7 (depends on 1)

The method of claim 1, wherein the oxide layer is a silicon oxide layer formed on a silicon substrate.

### Claim 8 (depends on 7)

The method of claim 7, wherein the silicon oxide layer is conformally formed over a shallow trench isolation trench opening.

### Claim 9 (depends on 8)

The method of claim 8, wherein the silicon oxide layer is formed at a thickness of from about 50 Angstroms to about 300 Angstroms.

### Claim 10 (depends on 1)

The method of claim 1, wherein the oxide layer is a silicon oxide layer forming at least one of a pad oxide, a shallow trench isolation liner, and a gate oxide.

### Claim 11 (depends on 1)

The method of claim 1, wherein the high temperature annealing process is carried out at a temperature of from about 1000 degrees Centigrade to about 1150 degrees Centigrade.

### Claim 12

A method for preventing silicon oxide layer peeling in a high temperature annealing process comprising the steps of:
providing a plurality of spaced apart stacked semiconductor wafers for carrying out a high temperature annealing process including ambient nitrogen gas the plurality of spaced apart stacked semiconductor wafers stacked such that at least one semiconductor wafer having a process surface including a silicon oxide layer formed thereon is adjacently disposed to a backside surface of an adjacently disposed semiconductor wafer said backside surface having a layer of silicon nitride formed thereon prior to carrying out the high temperature annealing process; and,
carrying out the high temperature annealing process at a temperature above about 900 degrees Centigrade.

### Claim 13 (depends on 12)

The method of claim 12, wherein the silicon nitride layer is formed at a thickness of from about 300 Angstroms to about 2000 Angstroms.

### Claim 14 (depends on 1)

The method of claim 1, wherein the adjacently disposed semiconductor is a control wafer for monitoring the high temperature annealing process conditions.

### Claim 15 (depends on 14)

The method of claim 14, wherein the control wafer is provided for monitoring at least one of annealing temperature, oxide layer thickness, and semiconductor wafer electrical resistance.

### Claim 16 (depends on 14)

The method of claim 14, wherein the control wafer is disposed in a gas flow pathway for supplying the ambient nitrogen gas to the plurality of spaced apart stacked semiconductor wafers.

### Claim 17 (depends on 12)

The method of claim 12, wherein the high temperature annealing process is carried out in one of a vertically and horizontally oriented furnace.

### Claim 18 (depends on 12)

The method of claim 12, wherein the silicon oxide layer is formed on a silicon substrate.

### Claim 19 (depends on 18)

The method of claim 18, wherein the silicon oxide layer is conformally formed over a shallow trench isolation trench opening.

### Claim 20 (depends on 19)