# US 2003/0207579 A1 · Method of etching a deep trench having a tapered profile in silicon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0207579 A1
- Document ID: US20030207579A1
- Status: Published application
- Kind: A1
- Application number: 10/137,176
- Filed: 2002-05-01
- Published: 2003-11-06
- Earliest claimed: 2002-05-01
- Assignees: Applied Materials, Inc.
- Inventors: Michael Rattner; Jeffrey D. Chinn
- Web page: https://patentgrep.com/patent/US20030207579A1

## CPC

- H10P 50/242: {of Group IV materials}
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Disclosed herein is a method of etching deep trenches in a substrate which utilizes the overlying mask structure to achieve a trench having a positive tapered sidewall angle of less than about 88°. The method employs the successive etching of a lateral undercut in the substrate beneath a masking material, while at the same time etching vertically downward beneath the mask. The coordinated widening of the lateral undercut at the top of the trench, while vertically extending the depth of the trench, is designed to provide the desired trench sidewall taper angle.

## Claims

### Claim 1

A method of etching trenches in a substrate which have a trench depth of at least 20 μm and a positive tapered sidewall angle of less than about 88°, wherein the method employs a masking layer overlying said substrate, and the successive etching of a lateral undercut in said substrate beneath said masking layer, while at the same time etching vertically downward beneath said masking layer, and wherein a coordinated widening of said lateral undercut at the top of said trench with said vertical downward etching provides said positive tapered sidewall angle.

### Claim 2 (depends on 1)

A method in accordance with claim 1, including the following steps:
a) an etching step which comprises exposing said substrate to a plasma through a pattern in said masking layer;
b) a polymer deposition step which comprises exposing said substrate to a polymer forming plasma; and
c) alternatingly repeating step a) and step b) until a predetermined specific trench depth and tapered sidewall angle are achieved.

### Claim 3 (depends on 2)

A method in accordance with claim 2, wherein said substrate is selected from the group consisting of silicon, a metal, and an oxide.

### Claim 4 (depends on 3)

A method in accordance with claim 3, wherein said etching step is accomplished using a plasma generated from a plasma source gas comprising fluorine species, or chlorine species, or a combination of fluorine species and chlorine species.

### Claim 5 (depends on 3)

A method in accordance with claim 3, wherein said polymer deposition step is accomplished using a plasma generated from a plasma source gas selected from the group consisting of C4F8, CH2F2, CHF3, and combinations thereof.

### Claim 6 (depends on 3)

A method in accordance with claim 3, wherein a process chamber in which steps a) and b) are carried out is at a pressure ranging from about 30 mTorr to about 150 mTorr.

### Claim 7 (depends on 3)

A method in accordance with claim 3, wherein a bias power of about 35 W or less is applied to said substrate during said etching step.

### Claim 8 (depends on 7)

A method in accordance with claim 7, wherein said bias power is about 15 W or less.

### Claim 9 (depends on 8)

A method in accordance with claim 8, wherein said bias power is within the range of about 5 W to about 10 W.

### Claim 10 (depends on 3)

A method in accordance with claim 3, wherein said substrate temperature during steps a) and b) ranges from about 40° C. to about 120° C.

### Claim 11 (depends on 3)

A method in accordance with claim 3, wherein said method provides an etched trench having an etch profile angle within the range of about 40° to about 85°.

### Claim 12 (depends on 11)

A method in accordance with claim 11, wherein said method provides an etched trench having an etch profile angle within the range of about 60° to about 85°.

### Claim 13 (depends on 3)

A method in accordance with claim 3, wherein, subsequent to the last step b), a clean-up step is carried out in which said substrate is exposed to an oxygen plasma.

### Claim 14

A method of etching a trench in a silicon substrate, wherein the method includes:
a) an etching step comprising exposing said silicon substrate, through a patterned masking layer, to a plasma generated from a fluorine-containing gas;
b) a polymer deposition step comprising exposing said silicon substrate to a plasma generated from a gas which is capable of forming a polymer on etched silicon surfaces; and
c) alternatingly repeating said etching step and said polymer deposition step, wherein said etching step and said polymer deposition step are performed at a process chamber pressure within the range of about 30 mTorr to about 150 mTorr, and wherein a bias power of about 35 W or less is applied to said substrate during said etching step.

### Claim 15 (depends on 14)

The method of claim 14, wherein said method provides an etched trench having an etch profile angle within the range of about 40° to about 85°.

### Claim 16 (depends on 15)

The method of claim 15, wherein said method provides an etched trench having an etch profile angle within the range of about 60° to about 85°.

### Claim 17 (depends on 14)

The method of claim 14, wherein said method provides a trench having a depth of at least 20 microns.

### Claim 18 (depends on 14)

The method of claim 14, wherein said method provides a trench having an aspect ratio within the range of about 2:1 to about 1:2.

### Claim 19 (depends on 14)

The method of claim 14, wherein said bias power is about 15 W or less.

### Claim 20 (depends on 19)

The method of claim 19, wherein said bias power is within the range of about 5 W to about 10 W.

### Claim 21 (depends on 14)

The method of claim 14, wherein said silicon substrate is etched at an etch rate of at least 2 microns per minute.

### Claim 22 (depends on 21)

The method of claim 21, wherein said silicon substrate is etched at an etch rate within the range of about 7 microns per minute to about 10 microns per minute.

### Claim 23 (depends on 14)

The method of claim 14, wherein said substrate is biased using an RF source operating at a frequency within the range of 100 kHz to 13.56 MHz.

### Claim 24 (depends on 23)

The method of claim 23, wherein said frequency is within the range of 100 kHz to 2 MHz.

### Claim 25 (depends on 14)

The method of claim 14, wherein said method is performed at a substrate temperature within the range of about 40° C. to about 120° C.

### Claim 26 (depends on 14)

The method of claim 14, wherein said fluorine-containing gas is selected from the group consisting of SF6, CF4, NF3, and combinations thereof.

### Claim 27 (depends on 26)

The method of claim 26, wherein said fluorine-containing gas is SF6.

### Claim 28 (depends on 14)

The method of claim 14, wherein said polymer-forming gas is selected from the group consisting of C4F8, CH2F2, CHF3, and combinations thereof.

### Claim 29 (depends on 28)

The method of claim 28, wherein said polymer-forming gas is C4F8.

### Claim 30 (depends on 14)

The method of claim 14, wherein said polymer-forming gas contains carbon and fluorine in a carbon: fluorine ratio of at least 1:3.

### Claim 31 (depends on 30)

The method of claim 30, wherein said carbon: fluorine ratio is at least 1:2.

### Claim 32 (depends on 14)

The method of claim 14, wherein a ratio of a flow rate of said fluorine-containing gas during said etching step and a flow rate of said polymer-forming gas during said polymer deposition step is within the range of about 6:1 to about 1:1.

### Claim 33 (depends on 14)

The method of claim 14, wherein said masking layer comprises a photoresist.

### Claim 34 (depends on 14)

The method of claim 14, wherein said masking layer comprises a material selected from the group consisting of silicon oxide, silicon nitride, and silicon oxynitride.

### Claim 35 (depends on 14)

The method of claim 14, wherein said method further comprises the following step:
a-1) a clean-up step, comprising exposing said silicon substrate to an oxygen plasma, and wherein said clean-up step is performed following at least one of said etching steps.

### Claim 36 (depends on 14)

The method of claim 14, wherein step a) and step b) are performed in succession for at least 3 cycles.