# US 2003/0207150 A1 · Methods of controlling oxygen partial pressure during annealing of a perovskite dielectric layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0207150 A1
- Document ID: US20030207150A1
- Status: Published application
- Kind: A1
- Application number: 10/139,454
- Filed: 2002-05-06
- Published: 2003-11-06
- Earliest claimed: 2002-05-06
- Assignees: North Carolina State University
- Inventors: Jon-Paul Maria; Angus Ian Kingon
- Web page: https://patentgrep.com/patent/US20030207150A1

## CPC

- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 35/491: based on lead zirconates and lead titanates {, e.g. PZT}
- H01G 4/1245: {containing also titanates}
- C04B 2235/6584: at an oxygen percentage below that of air
- C04B 2235/664: Reductive annealing
- C04B 2235/768: Perovskite structure ABO3
- Y10T 428/1291: Next to Co-, Cu-, or Ni-base component
- Y10T 428/264: Up to 3 mils
- Y10T 428/265: 1 mil or less
- Y10T 428/31678: Of metal
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Oxygen partial pressure may be controlled during annealing of a perovskite dielectric layer by providing an oxygen-absorbing layer adjacent the perovskite dielectric layer, and annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure, such that the oxygen-absorbing layer locally reduces the oxygen partial pressure adjacent the perovskite dielectric layer to below the ambient oxygen partial pressure. Thus, a perovskite dielectric layer can be annealed without the need to provide ultra-high vacuum and/or ultra-high purity ambient environments.

## Claims

### Claim 1

A method of controlling oxygen partial pressure during annealing of a perovskite dielectric layer comprising:
providing an oxygen-absorbing layer adjacent the perovskite dielectric layer; and
annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure such that the oxygen-absorbing layer locally reduces the oxygen partial pressure adjacent the perovskite dielectric layer to below the ambient oxygen partial pressure.

### Claim 2 (depends on 1)

A method according to claim 1 wherein the oxygen-absorbing layer comprises at least one base metal.

### Claim 3 (depends on 1)

A method according to claim 1 wherein the perovskite dielectric layer comprises acceptor-doped lead zirconate titanate.

### Claim 4 (depends on 1)

A method according to claim 1 wherein the annealing comprises annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−5 Torr at temperature of at least about 500° C.

### Claim 5 (depends on 1)

A method according to claim 1 wherein the annealing comprises annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−3 Torr at temperature of at least about 500° C.

### Claim 6 (depends on 1)

A method according to claim 1 wherein the annealing comprises annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of between about 10−3 Torr and about 10−2 Torr at temperature of about 750° C.

### Claim 7 (depends on 1)

A method according to claim 1 wherein the annealing comprises annealing the perovskite dielectric layer at atmospheric pressure in a nitrogen ambient that contains about 5 parts per million of oxygen.

### Claim 8 (depends on 1)

A method according to claim 1 wherein the annealing comprises annealing the perovskite dielectric layer at atmospheric pressure in a nitrogen ambient that is obtained from a bottled nitrogen gas cylinder.

### Claim 9 (depends on 1)

A method according to claim 1 wherein the annealing is followed by forming an electrode on the perovskite dielectric layer opposite the oxygen-absorbing layer to produce a capacitor.

### Claim 10 (depends on 1)

A method according to claim 1 wherein the annealing comprises annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure such that the oxygen-absorbing layer locally reduces the oxygen partial pressure adjacent the perovskite dielectric layer to below the ambient oxygen partial pressure and does not form an oxide of the oxygen-absorbing layer between the oxygen-absorbing layer and the perovskite dielectric layer.

### Claim 11

A method of fabricating an electronic structure comprising:
forming an acceptor-doped perovskite dielectric layer on a conductive layer that comprises a base metal; and
annealing the acceptor-doped perovskite layer in an ambient that includes an ambient oxygen partial pressure such that the conductive layer that comprises a base metal absorbs oxygen adjacent the acceptor-doped perovskite dielectric layer to locally reduce the oxygen partial pressure in the acceptor-doped perovskite dielectric layer below the ambient oxygen partial pressure.

### Claim 12 (depends on 11)

A method according to claim 11 wherein the acceptor-doped perovskite dielectric layer comprises calcium doped lead zirconate titanate.

### Claim 13 (depends on 11)

A method according to claim 11 wherein the annealing comprises annealing the acceptor-doped perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−5 Torr at temperature of at least about 500° C.

### Claim 14 (depends on 11)

A method according to claim 11 wherein the annealing comprises annealing the acceptor-doped perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−3 Torr at temperature of at least about 500° C.

### Claim 15 (depends on 11)

A method according to claim 11 wherein the annealing comprises annealing the acceptor-doped perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of between about 10−3 Torr and about 10−2 Torr at temperature of about 750° C.

### Claim 16 (depends on 11)

A method according to claim 11 wherein the annealing comprises annealing the acceptor-doped perovskite dielectric layer at atmospheric pressure in a nitrogen ambient that contains about 5 parts per million of oxygen.

### Claim 17 (depends on 11)

A method according to claim 11 wherein the annealing comprises annealing the acceptor-doped perovskite dielectric layer at atmospheric pressure in a nitrogen ambient that is obtained from a bottled nitrogen gas cylinder.

### Claim 18 (depends on 11)

A method according to claim 11 wherein the annealing is followed by forming an electrode on the acceptor-doped perovskite dielectric layer opposite the conductive layer that comprises a base metal to produce a capacitor.

### Claim 19 (depends on 11)

A method according to claim 11 wherein the conductive layer that comprises a base metal comprises a core layer comprising a base metal having opposing faces and a cladding layer comprising a base metal on one of the opposing faces, and wherein the forming comprises forming the acceptor-doped perovskite dielectric layer on the cladding layer.

### Claim 20 (depends on 11)

A method according to claim 11 wherein the annealing comprises annealing the acceptor-doped perovskite layer in an ambient that includes an ambient oxygen partial pressure such that the conductive layer that comprises a base metal absorbs oxygen adjacent the acceptor-doped perovskite dielectric layer to locally reduce the oxygen partial pressure in the acceptor-doped perovskite dielectric layer below the ambient oxygen partial pressure and does not form an oxide of the base metal between the conductive layer and the perovskite dielectric layer.

### Claim 21

A method of fabricating an electronic structure comprising:
providing a metal foil comprising a cladding layer comprising a base metal and a core layer comprising a base metal thereon;
forming a perovskite dielectric layer on the cladding layer; and
annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−5 Torr at temperature of at least about 500° C.

### Claim 22 (depends on 21)

A method according to claim 21 wherein the annealing comprises annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−3 Torr at temperature of at least about 500° C.

### Claim 23 (depends on 21)

A method according to claim 21 wherein the annealing comprises annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of between about 10−3 Torr and about 10−2 Torr at temperature of at least about 500° C.

### Claim 24 (depends on 21)

A method according to claim 21 wherein the annealing comprises annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of between about 10−3 Torr and about 10−2 Torr at temperature of about 750° C.

### Claim 25 (depends on 21)

A method according to claim 21 wherein the annealing comprises annealing the perovskite dielectric layer at atmospheric pressure in a nitrogen ambient that contains about 5 parts per million of oxygen.

### Claim 26 (depends on 21)

A method according to claim 21 wherein the annealing comprises annealing the perovskite dielectric layer at atmospheric pressure in a nitrogen ambient that is obtained from a bottled nitrogen gas cylinder.

### Claim 27 (depends on 21)

A method according to claim 21 wherein the forming a perovskite dielectric layer on the first cladding layer comprises forming a perovskite dielectric layer directly on the cladding layer.

### Claim 28 (depends on 21)

A method according to claim 21 wherein the annealing is followed by forming an electrode on the perovskite dielectric layer opposite the metal foil to produce a capacitor.

### Claim 29 (depends on 21)

A method according to claim 21 wherein the perovskite dielectric layer comprises calcium doped lead zirconate titanate, wherein the core layer comprises copper and wherein the cladding layer comprises nickel.

### Claim 30 (depends on 21)

A method according to claim 21 wherein the annealing comprises annealing the perovskite dielectric layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−5 Torr at temperature of at least about 500° C. without forming an oxide of the first cladding layer between the cladding layer and the perovskite dielectric layer.

### Claim 31

A method of controlling oxygen partial pressure during annealing of a layer comprising:
providing an oxygen-absorbing layer adjacent the layer; and
annealing the layer in an ambient that includes an ambient oxygen partial pressure such that the oxygen-absorbing layer locally reduces the oxygen partial pressure adjacent the layer to below the ambient oxygen partial pressure.

### Claim 32 (depends on 31)

A method according to claim 31 wherein the oxygen-absorbing layer comprises at least one base metal.

### Claim 33 (depends on 31)

A method according to claim 31 wherein the annealing comprises annealing the layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−5 Torr at temperature of at least about 500° C.

### Claim 34 (depends on 31)

A method according to claim 31 wherein the annealing comprises annealing the layer in an ambient that includes an ambient oxygen partial pressure of at least about 10−3 Torr at temperature of at least about 500° C.

### Claim 35 (depends on 31)

A method according to claim 31 wherein the annealing comprises annealing the layer in an ambient that includes an ambient oxygen partial pressure of between about 10−3 Torr and about 10−2 Torr at temperature of about 750° C.

### Claim 36 (depends on 31)

A method according to claim 31 wherein the annealing comprises annealing the layer at atmospheric pressure in a nitrogen ambient that contains about 5 parts per million of oxygen.

### Claim 37 (depends on 31)

A method according to claim 31 wherein the annealing comprises annealing the layer at atmospheric pressure in a nitrogen ambient that is obtained from a bottled nitrogen gas cylinder.

### Claim 38

An electronic structure comprising:
a perovskite dielectric layer; and
an oxygen-containing layer having a first face adjacent the perovskite dielectric layer, a second face opposite the perovskite dielectric layer and a center region therebetween, the oxygen-containing layer having lower oxygen concentration at the center region than adjacent at least one of the first and second faces thereof.

### Claim 39 (depends on 38)

A structure according to claim 38 wherein the oxygen-containing layer has lower oxygen concentration at the center region than adjacent both of the first and second faces thereof.

### Claim 40 (depends on 38)

A structure according to claim 38 wherein the oxygen concentration in the oxygen-containing layer decreases from adjacent the second face to adjacent the first face.

### Claim 41 (depends on 38)

A structure according to claim 38 wherein the oxygen concentration in the oxygen-containing layer decreases from adjacent the second face to the center region and from adjacent the first face to the center region.

### Claim 42 (depends on 38)

A structure according to claim 38 wherein the oxygen-containing layer comprises:
a first cladding layer comprising nickel on the perovskite dielectric layer;
a core layer comprising copper on the first cladding layer opposite the perovskite dielectric layer; and
a second cladding layer comprising nickel on the core layer opposite the first cladding layer.

### Claim 43 (depends on 42)

A structure according to claim 42 wherein the core layer includes an average oxygen concentration that is less than that of the second cladding layer and the first cladding layer includes an average oxygen concentration that is less than that of the core layer.

### Claim 44 (depends on 43)

A structure according to claim 43 wherein the oxygen concentration decreases exponentially across the core layer from adjacent the second cladding layer to adjacent the first cladding layer.

### Claim 45 (depends on 42)

A structure according to claim 42 wherein the core layer includes an average oxygen concentration that is less than that of the first and second cladding layers.

### Claim 46 (depends on 45)

A structure according to claim 45 wherein the core layer includes a center region and wherein the oxygen concentration decreases exponentially across the core layer from adjacent the second cladding layer to the center region and from adjacent the first cladding layer to the center region.

### Claim 47 (depends on 38)

A structure according to claim 38 further comprising a layer comprising metal on the perovskite dielectric layer opposite the oxygen-containing layer to produce a capacitor.

### Claim 48 (depends on 42)

A structure according to claim 42 wherein the perovskite dielectric layer is directly on the first cladding layer.

### Claim 49 (depends on 48)

A structure according to claim 48 further comprising a nickel oxide layer on the second cladding layer opposite the core layer.

### Claim 50 (depends on 42)

A structure according to claim 42 wherein the core layer is substantially thicker than the first and second cladding layers.

### Claim 51 (depends on 42)

A structure according to claim 42 wherein the core layer is substantially thicker than the perovskite dielectric layer.

### Claim 52 (depends on 42)

A structure according to claim 42 wherein the first and second cladding layers are about 4 μm thick and wherein the core layer is about 17 μm thick.

### Claim 53 (depends on 38)

A structure according to claim 38 wherein the perovskite dielectric layer comprises lead zirconate titanate.

### Claim 54 (depends on 53)

A structure according to claim 53 wherein the lead zirconate titanate comprises calcium doped lead zirconate titanate.

### Claim 55 (depends on 52)

A structure according to claim 52 wherein the perovskite dielectric layer is less than about 1 μm thick.