# US 2003/0207111 A1 · Dimensionally stable polyester yarn for high tenacity treated cords

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0207111 A1
- Document ID: US20030207111A1
- Status: Published application
- Kind: A1
- Application number: 10/440,642
- Filed: 2003-05-19
- Published: 2003-11-06
- Earliest claimed: 1988-07-05
- Assignees: AlliedSignal Inc.
- Inventors: Charles Jay Nelson; Jayendra Hiralal Bheda; Peter Bryan Rim; James Michael Turner
- Web page: https://patentgrep.com/patent/US20030207111A1

## CPC

- D01F 6/62: from polyesters
- D01D 5/12: Stretch-spinning methods ({D01D5/098 takes precedence} finishing by stretching D02J1/22)
- Y10T 428/2913: Rod, strand, filament or fiber
- Y10T 428/2969: Polyamide, polyimide or polyester
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Polyethylene terephthalate yarn is prepared by spinning under high stress conditions in the transition region between oriented-amorphous and oriented-crystalline undrawn yarns by selection of process parameters to form an undrawn yarn that is a crystalline, partially oriented yarn with a crystallinity of 3 to 15 percent and a melting point elevation of 2 to 10° C. The spun yarn is then hot drawn to a total draw ratio between 1.5/1 and 2.5/1 with the resulting properties: (A) a terminal modulus of at least 20 g/d, (B) a dimensional stability defined by E4.5+FS<13.5 percent, (C) a tenacity of at least 7 grams per denier, (D) a melting point elevation of 9 to 14° C., and (E) an amorphous orientation function of less than 0.75. The resulting treated tire cord provides high tenacity in combination with improved dimensional stability.

## Claims

### Claim 1

A process for production of a drawn polyethylene terephthalate yarn which translates to a high tenacity dimensionally stable tire cord, comprising:
(A) extruding a molten melt-spinnable polyethylene terephthalate having an intrinsic viscosity of 0.8 of greater through a shaped extrusion orifice having a plurality of openings to form a molten spun yarn,
(B) solidifying the spun yarn gradually by passing the yarn through a solidification zone which comprises (a) a retarded cooling zone and (b) a cooling zone adjacent said retarded cooling zone wherein said yarn is rapidly cooled and solidified in a blown air atmosphere,
(C) withdrawing the solidified yarn at sufficient speed to form a crystalline, partially oriented yarn with a crystallinity of 3 to 15% and a melting point elevation of 2 to 10° C., and
(D) hot drawing the yarn to a total draw ratio between 1.5/1 and 2.5/1.

### Claim 2 (depends on 1)

The process of claim 1 wherein the melting point elevation is 2 to 5° C.

### Claim 3 (depends on 1)

The process of claim 1 wherein φ1/2 is at least 26°.

### Claim 4 (depends on 1)

The process of claim 1 wherein the steps A, B, C, and D are performed in a continuous integrated spin-draw process.

### Claim 5 (depends on 4)

The process of claim 4 wherein the melting point elevation is 2 to 5° C.

### Claim 6 (depends on 4)

The process of claim 4 wherein φ1/2 is at least 26°.

### Claim 7

A drawn polyethylene terephthalate multifilament yarn having the following combination of properties:
(A) a terminal modulus of at least 20 g/d,
(B) a dimensional stability defined by E4.5+FS<13.5%,
(C) a tenacity of at least 7 grams/denier,
(D) a melting point elevation of 9 to 14° C., and
(E) a amorphous orientation function of less than 0.75.

### Claim 8 (depends on 7)

The drawn yarn of claim 7 wherein the melting point elevation is 9-11° C.

### Claim 9 (depends on 7)

The drawn yarn of claim 7 which has the melting point characteristic defined by Z* greater than or equal to 1.3.

### Claim 10 (depends on 7)

Dimensionally stable yarns of claim 7 which have the melting characteristic defined by Z greater than or equal to 1.7.

### Claim 11 (depends on 7)

The drawn yarn of claim 7 which has an effective crosslink density (N) between 10×1021 and 20×1021 crosslinks per cubic centimeter.

### Claim 12 (depends on 7)

A high tenacity, dimensionally stable treated tire cord prepared from the yarn of claim 7.

### Claim 13 (depends on 12)

A rubber article incorporating as reinforcing material the high tenacity, dimensionally stable cord of claim 12.

### Claim 14 (depends on 7)

A composite incorporating as reinforcing material the drawn yarn of claim 7.

### Claim 15

A drawn polyethylene terephthalate yarn which, when twisted into an 8×8 twists per inch 1000 denier 3-end greige cord and tensilized by the sequence of dipping into a first blocked diisocyanate dipping solution, stretching at 440° F. (227° C.) for 40 seconds, dipping into a second resourcinol-formaldehyde-latex dipping solution, and relaxing at 440° F. (227° C.) for 60 seconds, provides the following treated cord property combinations:
(a) a dimensional stability defined by LASE-5 of at least 2.3 grams per denier at 4 percent free shrinkage, and
(b) a tenacity of at least 7.0 grams per denier at 4 percent free shrinkage, said dimensional stability and said tenacity being determined by interpolation of LASE-5 versus free shrinkage data to 4 percent free shrinkage.

### Claim 16 (depends on 15)

The yarn of claim 15 which provides a at 4 percent free sllr tnkace, saidl cdiineiisiona il stability a saied tLe c ity K)linicj (Jeteriii ined by interpolat of 1LJL 5 versus free slr i tyKagc data to hi perLce(r free sho inkae .