# US 2003/0206090 A1 · Dust Core

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0206090 A1
- Document ID: US20030206090A1
- Status: Published application
- Kind: A1
- Application number: 10/412,174
- Filed: 2003-04-11
- Published: 2003-11-06
- Earliest claimed: 2000-09-08
- Assignees: TDK Corporation
- Inventors: Hideharu Moro
- Web page: https://patentgrep.com/patent/US20030206090A1

## CPC

- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- H01F 3/08: made from powder (powder coatings on sheets H01F3/02; on strips or ribbons H01F3/04; on wires H01F3/06)
- H01F 27/255: made from particles (H01F27/26 takes precedence)
- Y10T 29/49032: Fabricating head structure or component thereof
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A dust core consists essentially of ferromagnetic powder; and an insulating binder, in which the ferromagnetic powder is dispersed; wherein the insulating binder is a silicone resin comprising a trifunctional alkyl-phenyl silicone resin and optionally containing an inorganic insulator such as an inorganic oxide, carbide or nitride. Preferably the alkyl-phenyl silicone resin is a methyl-phenyl silicone resin and comprises about 20 to 70 mol % of trifunctional groups. The dust core can be produced by pressure-molding a ferromagnetic powder, a lubricant and a trifunctional alkyl-phenyl silicone resin binder and heat treating the molded core at a temperature in the range of about 300 to about 800 ° C. for a time period in the range of about 20 minutes to about 2 hours in a non-oxidizing atmosphere. The dust core has high magnetic permeability representing the direct current superimposition characteristics, has reduced core loss and has increased mechanical strength.

## Claims

### Claim 1

A dust core consisting essentially of:
ferromagnetic powder; and
an insulating binder, in which the ferromagnetic powder is dispersed;
wherein the insulating binder is a trifunctional alkyl-phenyl silicone resin and optionally includes an inorganic insulator dispersed therein.

### Claim 2 (depends on 2)

A dust core according to claim 2, wherein the alkyl-phenyl silicone resin has a phenyl content in the range of about 15 mol % to about 60 mol %, based on all organic groups in the silicone resin.

### Claim 3 (depends on 1)

A dust core according to claim 1, wherein the amount of the trifunctional alkyl-phenyl silicone resin contained in the dust core is in the range of about 0.3 to about 5% by weight, based on the weight of ferromagnetic powder.

### Claim 4 (depends on 1)

A dust core according to claim 1 wherein the trifunctional alkyl-phenyl silicone resin is a trifunctional methyl-phenyl silicone resin.

### Claim 5 (depends on 4)

A dust core according to claim 4, wherein the methyl-phenyl silicone resin has a phenyl content in the range of about 15 mol % to about 60 mol %, based on all organic groups in the silicone resin.

### Claim 6 (depends on 4)

A dust core according to claim 4, wherein the amount of the trifunctional methyl-phenyl silicone resin contained in the dust core is in the range of about 0.3 to about 5% by weight, based on the weight of ferromagnetic powder.

### Claim 7 (depends on 1)

A dust core according to claim 1 wherein the inorganic insulator is selected from the group consisting of an inorganic oxide, an inorganic carbide, and an inorganic nitride.

### Claim 8

A dust core consisting essentially of:
ferromagnetic powder; and
an insulating binder in which the ferromagnetic powder is dispersed; wherein the insulating binder is a trifunctional methyl-phenyl silicone resin optionally including an inorganic insulator dispersed therein, the methyl-phenyl silicone resin having about 20 mol % to about 70 mol % of trifunctional silicone structural units, based on total moles of silicone resin.

### Claim 9 (depends on 8)

A dust core according to claim 8, wherein the amount of methyl-phenyl silicone resin contained in the dust core is in the range of about 0.5 to about 3 wt % based on the ferromagnetic powder.

### Claim 10 (depends on 8)

A dust core according to claim 8, wherein the methyl-phenyl silicone resin has a phenyl content in the range of about 15 mol % to about 60 mol %, based on all organic groups in the silicone resin.

### Claim 11 (depends on 8)

A dust core according to claim 8 wherein the inorganic insulator is selected from the group consisting of an inorganic oxide, an inorganic carbide, and an inorganic nitride.

### Claim 12

A method of producing a dust core comprising pressure molding a mixture of ferromagnetic powder and a lubricant dispersed in an insulating material to form a molded core; and
heat treating the molded core at a temperature in the range of about 300 to about 800° C. for a time period in the range of about 20 minutes to about 2 hours in a non-oxidizing atmosphere;
the insulating material comprising a trifunctional alkyl-phenyl silicone resin having a phenyl content in the range of about 15 mol % to about 60 mol %, based on all organic groups in the silicone resin.

### Claim 13 (depends on 12)

The method of claim 12 wherein the lubricant is a fatty acid metal salt.

### Claim 14 (depends on 12)

The method of claim 12 wherein the insulating material further comprises an inorganic insulator.

### Claim 15 (depends on 14)

The method of claim 14 wherein the inorganic insulator is selected from the group consisting of an inorganic oxide, an inorganic carbide, and an inorganic nitride.

### Claim 16 (depends on 12)

A method according to claim 12, wherein the alkyl-phenyl silicone resin comprises about 20 mol % to about 70 mol % of trifunctional silicone structural units, based on total moles of alkyl-phenyl silicone resin; and the amount of alkyl-phenyl silicone resin in the dust core being in the range of about 0.5 to about 3% by weight, based on the weight of ferromagnetic powder.

### Claim 17 (depends on 12)

A method according to claim 12, wherein molded core is heat treated at a temperature of not more than about 600° C.

### Claim 18 (depends on 12)

A method according to claim 12, wherein the alkyl-phenyl silicone resin is a methyl-phenyl silicone resin.

### Claim 19 (depends on 18)

A dust core produced by the process of claim 18.

### Claim 20 (depends on 12)

A dust core produced by the process of claim 12.