# US 2003/0203803 A1 · Low melting high lithia glass compositions and methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0203803 A1
- Document ID: US20030203803A1
- Status: Published application
- Kind: A1
- Application number: 10/441,415
- Filed: 2003-05-19
- Published: 2003-10-30
- Earliest claimed: 1998-05-02
- Assignees: Westinghouse Savannah River Company
- Inventors: Carol M. Jantzen; John B. Pickett; Connie A. Cicero-Herman; James C. Marra
- Web page: https://patentgrep.com/patent/US20030203803A1

## CPC

- C03C 1/002: {Use of waste materials, e.g. slags}
- C03C 3/064: containing boron
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- C03C 3/105: containing aluminium
- Y10S 588/901: Compositions
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The invention relates to methods of vitrifying waste and for lowering the melting point of glass forming systems by including lithia formers in the glass forming composition in significant amounts, typically from about 0.16 wt % to about 11 wt %, based on the total glass forming oxides. The lithia is typically included as a replacement for alkali oxide glass formers that would normally be present in a particular glass forming system. Replacement can occur on a mole percent or weight percent basis, and typically results in a composition wherein lithia forms about 10 wt % to about 100 wt % of the alkali oxide glass formers present in the composition. The present invention also relates to the high lithia glass compositions formed by these methods. The invention is useful for stabilization of numerous types of waste materials, including aqueous waste streams, sludge solids, mixtures of aqueous supernate and sludge solids, combinations of spent filter aids from waste water treatment and waste sludges, supernate alone, incinerator ash, incinerator offgas blowdown, or combinations thereof, geological mine tailings and sludges, asbestos, inorganic filter media, cement waste forms in need of remediation, spent or partially spent ion exchange resins or zeolites, contaminated soils, lead paint, etc. The decrease in melting point achieved by the present invention desirably prevents volatilization of hazardous or radioactive species during vitrification.

## Claims

### Claim 1

A method of vitrifying radioactive, hazardous, or mixed waste comprising:
(1) mixing said waste with glass formers such that the resulting mixture comprises SiO2 and alkali oxide glass formers, wherein said alkali oxide glass formers comprise lithia formers and other alkali oxide glass formers in amounts such that the lithia formers, calculated as Li2O, are from 10.0 wt % to about 100 wt % of the total alkali oxide glass formers, calculated as M2O, where M is an alkali metal; and
(2) melting the resulting mixture at a temperature of between about 1050° C. and about 1250° C. and cooling to form a glass composition.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said lithia formers are from about 11.0 wt % to about 76 wt % of the total alkali oxide glass formers.

### Claim 3 (depends on 1)

The method according to claim 1, wherein
said mixture further comprise B2O3 formers in an amount sufficient to provide 5 wt % B2O3 or more in the glass composition;
said other alkali oxide glass formers comprise Na2O;
said lithia formers are between about 30 wt % and about 50 wt % of said alkali oxide glass formers; and
said melting is at a temperature between about 1150° C. and about 1200° C.

### Claim 4 (depends on 3)

The method according to claim 3, wherein said lithia formers are between about 35 wt % and about 50 wt % of said alkali oxide glass formers.

### Claim 5 (depends on 4)

The method according to claim 4, wherein said lithia formers are between about 40 wt % and about 48 wt % of said alkali oxide glass formers.

### Claim 6 (depends on 3)

The method according to claim 3, wherein said waste comprises a refractory mixture of waste water sludge and spent filter aids containing Al2O3 and SiO2, and wherein said glass composition has a waste loading of about 90 wt %.

### Claim 7 (depends on 1)

The method according to claim 1, wherein:
said mixture further comprises CaO formers in an amount sufficient to provide between about 0.25 wt % and about 0.5 wt % CaO in the glass composition;
said mixture either does not comprise B2O3 formers, or comprises B2O3 formers in amounts that provide less than 5 wt % B2O3 in the final glass composition;
said other alkali glass formers comprise Na2O;
said lithia formers are between about 25 wt % and about 35 wt % of said alkali oxide glass formers; and
said melting is at a temperature between about 1150° C. and about 1250° C.

### Claim 8 (depends on 7)

The method according to claim 7, wherein said lithia formers are about 30 wt % of said alkali oxide glass formers.

### Claim 9 (depends on 7)

The method according to claim 7, wherein said waste comprises a refractory mixture of waste water sludge and spent filter aids containing Al2O3 and SiO2, and wherein said glass composition has a waste loading of about 90 wt %.

### Claim 10 (depends on 7)

The method according to claim 7, wherein said melting is at a temperature of about 1200° C.

### Claim 11 (depends on 1)

The method according to claim 1, wherein:
said mixture further comprises CaO formers in an amount sufficient to provide between about 12 wt % and about 30 wt % CaO in the glass composition;
said mixture either does not comprise B2O3 formers, or comprises B2O3 formers in amounts that provide less than 5 wt % B2O3 in the final glass composition;
said other alkali glass formers comprise Na2O;
said lithia formers are between about 40 wt % and about 80 wt % of said alkali oxide glass formers; and
said melting is at a temperature between about 1175° C. and about 1200° C.

### Claim 12 (depends on 11)

The method according to claim 11, wherein said lithia formers are between about 42 wt % and about 75 wt % of said alkali oxide glass formers.

### Claim 13 (depends on 12)

The method according to claim 12, wherein said lithia formers are between about 42 wt % and about 47 wt % of said alkali oxide glass formers.

### Claim 14 (depends on 11)

The method according to claim 11, wherein said waste comprises CaCO3 containing sludge resulting from treatment of nitrate containing wastes by biodenitrification, followed by neutralization with lime.

### Claim 15 (depends on 1)

The method according to claim 1, wherein:
said mixture further comprises CaO formers in an amount sufficient to provide between about 15 wt % and about 22 wt % CaO in the glass composition;
said mixture either does not comprise B2O3 formers, or comprises B2O3 formers in amounts that provide less than 5 wt % B2O3 in the final glass composition;
said other alkali glass formers comprise Na2O;
said lithia formers are between about 37 wt % and about 46 wt % of said alkali oxide glass formers; and
said melting is at a temperature between about 1100° C. and about 1200° C.

### Claim 16 (depends on 15)

The method according to claim 15, wherein said temperature is about 1150° C.

### Claim 17 (depends on 15)

The method according to claim 15, wherein said waste comprises Ca(OH)2 and SiO2, Ag, Ni, depleted uranium, or Tc99.

### Claim 18 (depends on 15)

The method according to claim 15, wherein said mixture further comprises iron compounds sufficient to provide about 9.0 wt % to about 13 wt % Fe2O3, based on the final glass composition.

### Claim 19 (depends on 1)

The method according to claim 1, wherein:
said mixture further comprises CaO formers in an amount sufficient to provide between about 5 wt % and about 15 wt % CaO in the glass composition;
said mixture either does not comprise B2O3 formers, or comprises B2O3 formers in amounts that provide less than 5 wt % B2O3 in the final glass composition;
said other alkali glass formers comprise Na2O;
said lithia formers are between about 11 wt % and about 50 wt % of said alkali oxide glass formers; and
said melting is at a temperature between about 1125° C. and about 1275° C.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the CaO content in the glass composition is from about 10 wt % to about 13 wt %.

### Claim 21 (depends on 19)

The method according to claim 19, wherein said lithia formers are between about 28 wt % and about 50 wt % of said alkali oxide glass formers.

### Claim 22 (depends on 19)

The method according to claim 19, wherein said melting temperature is about 1150° C.

### Claim 23 (depends on 19)

The method according to claim 19, wherein said waste comprises concentrated acidic or caustic wastes or oily mopwater waste containing beryllium, thorium, uranium, emulsified oils, soaps, cleansers, or HF scrubber solutions.

### Claim 24 (depends on 19)

The method according to claim 19, wherein said mixture further comprises iron compounds sufficient to provide about 8 wt % to about 10 wt % Fe2O3, based on the final glass composition.

### Claim 25 (depends on 19)

The method according to claim 19, wherein said mixture further comprises phosphorus compounds sufficient to provide about 3 wt % to about 5 wt % P2O5, based on the final glass composition.

### Claim 26 (depends on 1)

The method according to claim 1, wherein:
said mixture further comprises BaO formers in an amount sufficient to provide between about 4 wt % and about 7 wt % BaO in the glass composition;
said mixture either does not comprise B2O3 formers, or comprises B2O3 formers in amounts that provide less than 5 wt % B2O3 in the final glass composition;
said other alkali glass formers comprise Na2O;
said lithia formers are between about 40 wt % and about 45 wt % of said alkali oxide glass formers; and
said melting is at a temperature between about 1000° C. and about 1200° C.

### Claim 27 (depends on 26)

The method according to claim 26, wherein said melting temperature is about 1050° C.

### Claim 28 (depends on 26)

The method according to claim 26, wherein said mixture further comprises lead compounds sufficient to provide about 8 wt % to about 12 wt % PbO, based on the final glass composition.

### Claim 29 (depends on 26)

The method according to claim 26, wherein said mixture further comprises iron compounds sufficient to provide about 3 wt % to about 6 wt % Fe2O3, based on the final glass composition.

### Claim 30 (depends on 26)

The method according to claim 26, wherein said waste comprises geologic mill tailings residues comprising radium, uranium, uranium daughter products, or heavy metals.

### Claim 31 (depends on 1)

The method according to claim 1, wherein:
said mixture further comprises CaO formers in an amount sufficient to provide between about 8 wt % and about 10 wt % CaO in the glass composition;
said mixture either does not comprise B2O3 formers, or comprises B2O3 formers in amounts that provide less than 5 wt % B2O3 in the final glass composition;
said other alkali glass formers comprise Na2O;
said lithia formers are between about 40 wt % and about 60 wt % of said alkali oxide glass formers; and
said melting is at a temperature between about 1000° C. and about 1200° C.

### Claim 32 (depends on 31)

The method according to claim 31, wherein said lithia formers are 50 wt % of said alkali oxide glass formers.

### Claim 33 (depends on 31)

The method according to claim 31, wherein said melting temperature is about 1150° C.

### Claim 34 (depends on 31)

The method according to claim 31, wherein said CaO formers are present in an amount sufficient to provide about 9 wt % CaO in the glass composition.

### Claim 35 (depends on 31)

The method according to claim 31, wherein said waste comprises contaminated soils or clays.

### Claim 36 (depends on 1)

The method according to claim 1, wherein:
said mixture further comprises MgO formers in an amount sufficient to provide between about 5 wt % and about 15 wt % MgO in the glass composition;
said mixture either does not comprise B2O3 formers, or comprises B2O3 formers in amounts that provide less than 5 wt % B2O3 in the final glass composition;
said other alkali glass formers comprise Na2O;
said lithia formers are between about 18 wt % and about 45 wt % of said alkali oxide glass formers; and
said melting is at a temperature between about 1000° C. and about 1200° C.

### Claim 37 (depends on 36)

The method according to claim 36, wherein said mixture further comprises iron compounds sufficient to provide about 8 wt % to about 25 wt % Fe2O3, based on the final glass composition.

### Claim 38 (depends on 36)

The method according to claim 36, wherein said melting temperature is about 1150° C.

### Claim 39 (depends on 36)

The method according to claim 36, wherein said waste is asbestos containing material.

### Claim 40

A method of decreasing the melting point of a waste glass that contains sodium oxide, potassium oxide, rubidium oxide, cesium oxide, or combinations thereof and that immobilizes radioactive, hazardous, or mixed waste, comprising:
preparing a mixture of waste and glass formers, comprising lithia or a lithia former, selected from the group consisting of Li0 and lithium compounds that convert to lithia during melting at elevated temperatures, in an amount sufficient to provide between about 0.16 wt % and about 9.30 wt % Li2O in the glass composition, based upon the total weight of oxide glass formers in the glass composition; and
heating the mixture to a temperature below the melting point of a corresponding mixture without said lithia or lithia formers.

### Claim 41 (depends on 40)

The method according to claim 40, wherein said mixture further comprises ferric oxide or a ferric oxide former selected from the group consisting of iron compounds that convert to ferric oxide during melting at elevated temperatures in an amount sufficient to provide between about 0.75 wt % and about 19.7 wt % in the glass composition, based upon the total weight of oxide glass formers in the glass composition.

### Claim 42 (depends on 40)

The method according to claim 40, wherein the melting point of the glass composition is about 177° C. to about 350° C. lower than the melting point of a corresponding glass composition formed without said lithia or lithia former.

### Claim 43 (depends on 40)

The method according to claim 40, wherein said lithia replaces at least a portion of the sodium oxide, potassium oxide, rubidium oxide, or cesium oxide normally present in said glass composition.

### Claim 44 (depends on 40)

The method according to claim 40, wherein the glass composition is an alkali borosilicate glass comprising Na2O, Li2O, B2O3, and SiO2 and having 5 wt % B2O3 or more based on the total oxide glass formers.

### Claim 45 (depends on 44)

The method according to claim 44, wherein the glass composition further comprises K2O or Al2O3, or both.

### Claim 46 (depends on 44)

The method according to claim 44, wherein said Li2O is present in an amount of about 4.8 wt % to about 5.0 wt %, based on the total oxide glass formers.

### Claim 47 (depends on 46)

The method according to claim 46, wherein the glass comprises less than about 2 wt % Fe2O3, based on the total oxide glass formers.

### Claim 48 (depends on 40)

The method according to claim 40, wherein the glass composition is a alkali lime silicate glass having less than 5 wt % B2O3, based on the total oxide glass formers.

### Claim 49 (depends on 40)

The method according to claim 40, wherein the amount of lithia or lithia former is sufficient to provide between about 4.77 wt % and about 9.3 wt % Li2O in the glass composition.

### Claim 50 (depends on 49)

The method according to claim 49, wherein the glass composition further comprises between about 1.49 wt % and about 1.86 wt % Fe2O3.

### Claim 51 (depends on 40)

The method according to claim 40, wherein the amount of lithia or lithia former is sufficient to provide between about 5.91 wt % and about 7.05 wt % Li2O in the glass composition.

### Claim 52 (depends on 51)

The method according to claim 51, wherein the waste glass further comprises between about 0.93 wt % and about 1.87 wt % Fe2O3.

### Claim 53 (depends on 40)

The method according to claim 40, wherein the amount of lithia or lithia former is sufficient to provide between about 3.0 wt % and about 6.0 wt % Li2O in the glass composition.

### Claim 54 (depends on 53)

The method according to claim 53, wherein the waste glass further comprises between about 9.38 wt % and about 12.51 wt % Fe2O3.

### Claim 55 (depends on 40)

The method according to claim 40, wherein the amount of lithia or lithia former is sufficient to provide between about 3.09 wt % and about 7.23 wt % Li2O in the glass composition.

### Claim 56 (depends on 55)

The method according to claim 55, wherein the waste glass further comprises between about 8.31 wt % and about 9.54 wt % Fe2O3.

### Claim 57 (depends on 40)

The method according to claim 40, wherein the amount of lithia or lithia former is sufficient to provide between about 7.36 wt % and about 8.50 wt % Li2O in the glass composition.

### Claim 58 (depends on 57)

The method according to claim 57, wherein the glass composition further comprises between about 4.08 wt % and about 4.43 wt % Fe2O3.

### Claim 59 (depends on 40)

The method according to claim 40, wherein the amount of lithia or lithia former is sufficient to provide about 11 wt % Li2O in the glass composition.

### Claim 60 (depends on 59)

The method according to claim 59, wherein the glass composition further comprises between about 0.75 wt % and about 1.21 wt % Fe2O3.

### Claim 61 (depends on 40)

The method according to claim 40, wherein the amount of lithia or lithia former is sufficient to provide between about 4.0 wt % and about 7.0 wt % Li2O in the glass composition.

### Claim 62 (depends on 61)

The method according to claim 61, wherein the glass composition further comprises between about 9.86 wt % and about 19.72 wt % Fe2O3.

### Claim 63 (depends on 40)

The method according to claim 40, wherein the amount of lithia or lithia former is sufficient to provide between about 2.0 wt % and about 5.0 wt % Li2O in the glass composition.

### Claim 64 (depends on 63)

The method according to claim 63, wherein the glass composition further comprises between about 11.3 wt % and about 12.3 wt % Fe2O3.

### Claim 65

An alkali oxide borosilicate glass composition suitable for immobilizing low level radioactive, hazardous, or mixed waste, comprising:
(a) SiO2 in an amount ranging from about 35 wt % to about 50 wt %;
(b) B2O3 in an amount ranging from about 5.0 wt % to about 15 wt %;
(c) Na2O in an amount ranging from about 9.0 wt % to about 20 wt %; and
(d) Li2O in an amount ranging from about 4.0 wt % to about 10 wt %.

### Claim 66 (depends on 65)

The alkali oxide borosilicate glass composition according to claim 65, further comprising:
(e) Al2O3 in an amount ranging from about 18 wt % to about 25 wt %.

### Claim 67 (depends on 65)

The alkali oxide borosilicate glass composition according to claim 65, further comprising:
(f) Fe2O3 in an amount ranging from about 1.5 wt % to about 1.9 wt %.

### Claim 68 (depends on 67)

The alkali oxide borosilicate glass composition according to claim 67, comprising in wt % based on the total oxide glass formers:
SiO2 about 39.9 to about 46.0;
B2O3 about 5.7 to about 9.3;
Na2O about 9.2 to about 9.7; and
Li2O about 4.8 to about 9.3.

### Claim 69 (depends on 68)

The alkali oxide borosilicate glass composition according to claim 68, further comprising:
Al2O3 about 19.0 to about 21.3.

### Claim 70 (depends on 68)

The alkali oxide borosilicate glass composition according to claim 68, further comprising:
Fe2O3 about 1.51 to about 1.86.

### Claim 71 (depends on 68)

The alkali oxide borosilicate glass composition according to claim 68, further comprising:
CaO about 0.32 to about 0.43;
K2O about 0.98 to about 1.53;
P2O5 about 1.12 to about 2.20; and
U3O8 about 4.94 to about 5.25.

### Claim 72

An alkali oxide-lime-silica glass composition suitable for immobilizing radioactive, hazardous, or mixed waste, comprising:
(a) SiO2 in an amount ranging from about 46 wt % to about 66 wt %;
(b) CaO in an amount ranging from about 5 wt % to about 28 wt %;
(c) Na2O in an amount ranging from about 1.9 wt % to about 25 wt %;
(d) Li2O in an amount ranging from about 3 wt % to about 11 wt %.

### Claim 73 (depends on 72)

The alkali oxide-lime-silica glass composition according to claim 72, further comprising:
(e) Al2O3 in an amount ranging from about 2.5 wt % to about 18 wt %.

### Claim 74 (depends on 72)

The alkali oxide-lime-silica glass composition according to claim 72, further comprising:
(f) Fe2O3 in an amount ranging from about 0.9 wt % to about 13 wt %.

### Claim 75 (depends on 72)

The alkali oxide-lime-silica glass composition according to claim 72, further comprising:
(g) K2O in an amount ranging form about 0 wt % to about 1.8 wt %; and
(h) P2O5 in an amount ranging from about 0 wt % to about 4.5 wt %.

### Claim 76 (depends on 72)

The alkali oxide-lime-silica glass composition according to claim 72, further comprising:
(i) U3O8 in an amount ranging from about 0.5 wt % to about 12 wt %.

### Claim 77 (depends on 72)

The alkali oxide-lime-silica glass composition according to claim 72, further comprising:
(j) UO2 in an amount ranging from about 0.4 wt % to about 12 wt %.

### Claim 78

An alkali oxide-baria-silica glass composition suitable for immobilizing radioactive, hazardous, or mixed waste, comprising:
(a) SiO2 in an amount ranging from about 48 wt % to about 56 wt %;
(b) BaO in an amount ranging from about 3.5 wt % to about 7.0 wt %;
(c) Na2O in an amount ranging from about 8.0 wt % to about 15 wt %; and
(d) Li2O in an amount ranging from about 6.0 wt % to about 10.0 wt %.

### Claim 79 (depends on 78)

The alkali oxide-baria-silica glass composition according to claim 78, further comprising:
(e) Al2O3 in an amount ranging from about 3.0 wt % to about 5.0 wt %.

### Claim 80 (depends on 78)

The alkali oxide-baria-silica glass composition according to claim 78, further comprising:
(f) PbO in an amount ranging from about 8 wt % to about 12 wt %.

### Claim 81 (depends on 78)

The alkali oxide-baria-silica glass composition according to claim 78, further comprising:
(g) Fe2O3 in an amount ranging from about 3.0 wt % to about 5.5 wt %.

### Claim 82 (depends on 78)

The alkali oxide-baria-silica glass composition according to claim 78, further comprising:
(h) CaO in an amount ranging from about 1.0 wt % to about 3.0 wt %; and
(i) K2O in an amount ranging from about 0.5 wt % to about 1.0 wt %.

### Claim 83

An alkali oxide-magnesia-silica glass composition suitable for immobilizing radioactive, hazardous, or mixed waste, comprising:
(a) SiO2 in an amount ranging from about 40 wt % to about 68 wt %;
(b) MgO in an amount ranging from about 5.0 wt % to about 15 wt %;
(c) Na2O in an amount ranging from about 7.0 wt % to about 20 wt %; and
(d) Li2O in an amount ranging from about 3.0 wt % to about 9.0 wt %.

### Claim 84 (depends on 83)

The alkali oxide-magnesia-silica glass composition according to claim 83, further comprising:
(e) K2O in an amount ranging from about 0.05 wt % to about 0.2 wt %.

### Claim 85 (depends on 83)

The alkali oxide-magnesia-silica glass composition according to claim 83, further comprising:
(f) Fe2O3 in an amount ranging from about 8.0 wt % to about 22 wt %.

### Claim 86 (depends on 83)

The alkali oxide-magnesia-silica glass composition according to claim 83, further comprising:
(g) Al2O3 in an amount ranging from about 0.1 wt % to about 0.7 wt %.

### Claim 87 (depends on 83)

The alkali oxide-magnesia-silica glass composition according to claim 83, further comprising:
(h) CaO in an amount ranging from about 0.15 wt % to about 0.75 wt %.