# US 2003/0203607 A1 · Method of manufacturing a portion of a memory

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0203607 A1
- Document ID: US20030203607A1
- Status: Published application
- Kind: A1
- Application number: 10/405,351
- Filed: 2003-04-01
- Published: 2003-10-30
- Earliest claimed: 1999-08-30
- Assignees: Micron Technology, Inc.
- Inventors: Gary Chen; Li Li; Yongjun Jeff Hu
- Web page: https://patentgrep.com/patent/US20030203607A1

## CPC

- H10D 64/664: {the additional layers comprising a barrier layer between the layer of silicon and an upper metal or metal silicide layer}
- H10D 64/01312: {the additional layer comprising a metal or metal silicide formed by deposition, i.e. without a silicidation reaction, e.g. sputter deposition}
- H10D 64/01354: {passivation or protection of the electrode, e.g. using re-oxidation}
- H10P 50/667: {by liquid etching only}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Metal nitride and metal oxynitride extrusions often form on metal silicides. These extrusions can cause short circuits and degrade processing yields. The present invention discloses a method of selectively removing such extrusions. In one embodiment, a novel wet etch comprising an oxidizing agent and a chelating agent selectively removes the extrusions from a wordline in a memory array. In another embodiment, the wet etch includes a base that adjusts the pH of the etch to selectively remove certain extrusions relative to other substances in the wordline. Accordingly, new metal silicide structures can be used to form novel wordlines and other types of integrated circuits.

## Claims

### Claim 1

A method of fabricating at least a portion of a memory, the method comprising the acts of:
depositing a tungsten silicide barrier layer on a portion of a memory;
processing the portion of the memory such that tungsten oxynitride extrusions extend from an exposed surface of the barrier layer; and
selectively etching the tungsten oxynitride extrusions with a solution comprising water, hydrogen peroxide and EDTA.

### Claim 2 (depends on 1)

The method of claim 1 wherein the amount of hydrogen peroxide in the solution ranges from approximately 2% to 50% of the solution.

### Claim 3 (depends on 1)

The method of claim 1 wherein the amount of hydrogen peroxide in the solution is approximately 10% of the solution.

### Claim 4 (depends on 1)

The method of claim 1 wherein the amount of EDTA in the solution ranges from approximately 0.001% to 5% of the solution.

### Claim 5 (depends on 1)

The method of claim 1 wherein the amount of EDTA in the solution is approximately 0.03% of the solution.

### Claim 6 (depends on 1)

The method of claim 1 wherein the solution further comprises ammonium hydroxide.

### Claim 7 (depends on 6)

The method of claim 6 wherein the amount of ammonium hydroxide ranges from approximately 0.5% to 30% of the solution.

### Claim 8 (depends on 6)

The method of claim 6 wherein the amount of ammonium hydroxide in the solution is approximately 0.02% of the solution.

### Claim 9 (depends on 6)

The method of claim 6 wherein the solution further comprises potassium sulfate.

### Claim 10 (depends on 9)

The method of claim 9 wherein the amount of potassium sulfate in the solution is approximately b 2% of the solution.

### Claim 11 (depends on 1)

The method of claim 1 wherein the memory is a SDRAM.

### Claim 12 (depends on 1)

The method of claim 1 wherein the memory is a static memory.

### Claim 13 (depends on 1)

The method of claim 1 wherein the memory is a dynamic memory.

### Claim 14 (depends on 1)

The method of claim 1 wherein the memory is an extended data out memory.

### Claim 15

A method of fabricating at least a portion of a memory, the method comprising the acts of:
depositing a titanium silicide conductive layer on a portion of a memory;
processing the portion of the memory such that titanium nitride extrusions extend from an exposed surface of the conductive layer; and
selectively etching the titanium nitride extrusions with a solution comprising water, hydrogen peroxide and EDTA.

### Claim 16 (depends on 15)

The method of claim 15 wherein the amount of hydrogen peroxide in the solution ranges from approximately 2% to 50% of the solution.

### Claim 17 (depends on 15)

The method of claim 15 wherein the amount of hydrogen peroxide in the solution is approximately 10% of the solution.

### Claim 18 (depends on 15)

The method of claim 15 wherein the amount of EDTA in the solution ranges from approximately 0.001% to 5% of the solution.

### Claim 19 (depends on 15)

The method of claim 15 wherein the amount of EDTA in the solution is approximately 0.03% of the solution.

### Claim 20 (depends on 15)

The method of claim 15 wherein the solution further comprises ammonium hydroxide.

### Claim 21 (depends on 20)

The method of claim 20 wherein the amount of ammonium hydroxide ranges from approximately 0.5% to 30% of the solution.

### Claim 22 (depends on 20)

The method of claim 20 wherein the amount of ammonium hydroxide in the solution is approximately 0.02% of the solution.

### Claim 23 (depends on 20)

The method of claim 20 wherein the solution further comprises potassium sulfate.

### Claim 24 (depends on 23)

The method of claim 23 wherein the amount of potassium sulfate in the solution is approximately 2% of the solution.

### Claim 25 (depends on 15)

The method of claim 15 wherein the memory is a SDRAM.

### Claim 26 (depends on 15)

The method of claim 15 wherein the memory is a static memory.

### Claim 27 (depends on 15)

The method of claim 15 wherein the memory is a dynamic memory.

### Claim 28 (depends on 15)

The method of claim 15 wherein the memory is an extended data out memory.

### Claim 29

A method of fabricating at least a portion of a memory, the method comprising the acts of:
depositing a titanium silicide conductive layer on a portion of a memory;
processing the portion of the memory such that titanium oxynitride extrusions extend from an exposed surface of the conductive layer; and
selectively etching the titanium oxynitride extrusions with a solution comprising water, hydrogen peroxide and EDTA.

### Claim 30 (depends on 29)

The method of claim 29 wherein the amount of hydrogen peroxide in the solution ranges from approximately 2% to 50% of the solution.

### Claim 31 (depends on 29)

The method of claim 29 wherein the amount of hydrogen peroxide in the solution is approximately 10% of the solution.

### Claim 32 (depends on 29)

The method of claim 29 wherein the amount of EDTA in the solution ranges from approximately 0.001% to 5% of the solution.

### Claim 33 (depends on 29)

The method of claim 29 wherein the amount of EDTA in the solution is approximately 0.03% of the solution.

### Claim 34 (depends on 29)

The method of claim 29 wherein the solution further comprises ammonium hydroxide.

### Claim 35 (depends on 34)

The method of claim 34 wherein the amount of ammonium hydroxide ranges from approximately 0.5% to 30% of the solution.

### Claim 36 (depends on 34)

The method of claim 34 wherein the amount of ammonium hydroxide in the solution is approximately 0.02% of the solution.

### Claim 37 (depends on 34)

The method of claim 34 wherein the solution further comprises potassium sulfate.

### Claim 38 (depends on 37)

The method of claim 37 wherein the amount of potassium sulfate in the solution is approximately 2% of the solution.

### Claim 39 (depends on 29)

The method of claim 29 wherein the memory is a SDRAM.

### Claim 40 (depends on 29)

The method of claim 29 wherein the memory is a static memory.

### Claim 41 (depends on 29)

The method of claim 29 wherein the memory is a dynamic memory.

### Claim 42 (depends on 29)

The method of claim 29 wherein the memory is an extended data out memory.

### Claim 43

A method of fabricating a wordline in a memory array, the method comprising the acts of:
depositing a low-resistance metal silicide layer on a wordline stack;
processing the wordline stack such that metal oxynitride extrusions extend from the metal silicide layer; and
selectively etching the metal oxynitride extrusions with a solution comprising at least an oxidizing agent and a chelating agent.

### Claim 44 (depends on 43)

The method of claim 43 wherein the oxidizing agent is a substance selected from the group consisting of hydrogen peroxide, ozonated water, ozone, nitric acid, hypochlorous acid, chloric acid, ammonium persulphate and sulfuric acid.

### Claim 45 (depends on 43)

The method of claim 43 wherein the chelating agent is a substance selected from the group consisting of ETDA, ligands, amines, carboxylic acid compounds, oxalate, acetate, disodium ethylenediamine acid, glycine, iminodiacetic acid, nitrolotriacetic acid, tetraammonium ethylenediaminetetraacetate, and tetramethylammonium ethylenediaminetetraacetate.

### Claim 46 (depends on 43)

The method of claim 43 wherein the solution further comprises a base that adjusts the pH of the solution to about seven to eight.

### Claim 47 (depends on 46)

The method of claim 46 wherein the base is a substance selected from the group consisting of ammonium hydroxide, tetramethyl ammonium hydroxide, trimethoxyamphetamine, choline hydroxide, sodium hydroxide, and potassium hydroxide.

### Claim 48 (depends on 46)

The method of claim 46 wherein the solution further comprises a buffer salt.

### Claim 49 (depends on 48)

The method of claim 48 wherein the buffer salt is a substance selected from the group consisting of potassium sulfate, potassium phosphate, and diammonium phosphate.

### Claim 50

A method of fabricating at least a portion of a memory array, the method comprising the acts of:
depositing a low-resistance metal silicide layer on a portion of a memory array;
processing the portion of the memory array such that metal nitride extrusions extend from the metal silicide layer; and
selectively etching the metal nitride extrusions with a solution comprising at least an oxidizing agent and a chelating agent.

### Claim 51 (depends on 50)

The method of claim 50 wherein the oxidizing agent is a substance selected from the group consisting of hydrogen peroxide, ozonated water, ozone, nitric acid, hypochlorous acid, chloric acid, ammonium persulphate and sulfuric acid.

### Claim 52 (depends on 50)

The method of claim 50 wherein the chelating agent is a substance selected from the group consisting of ETDA, ligands, amines, carboxylic acid compounds, oxalate, acetate, disodium ethylenediamine acid, glycine, iminodiacetic acid, nitrolotriacetic acid, tetraammonium ethylenediaminetetraacetate, and tetramethylammonium ethylenediaminetetraacetate.

### Claim 53 (depends on 50)

The method of claim 50 wherein the solution further comprises a base that adjusts the pH of the solution to about seven to eight.

### Claim 54 (depends on 53)

The method of claim 53 wherein the base is a substance selected from the group consisting of ammonium hydroxide, tetramethyl ammonium hydroxide, trimethoxyamphetamine, choline hydroxide, sodium hydroxide, and potassium hydroxide.

### Claim 55 (depends on 53)

The method of claim 53 wherein the solution further comprises a buffer salt.

### Claim 56 (depends on 55)

The method of claim 55 wherein the buffer salt is a substance selected from the group consisting of potassium sulfate, potassium phosphate, and diammonium phosphate.